Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials
The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-...
Gespeichert in:
Veröffentlicht in: | Journal of pressure vessel technology 2017-12, Vol.139 (6) |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | 6 |
container_start_page | |
container_title | Journal of pressure vessel technology |
container_volume | 139 |
creator | Chopra, O. K Stevens, G. L Tregoning, R Rao, A. S |
description | The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented. |
doi_str_mv | 10.1115/1.4035885 |
format | Article |
fullrecord | <record><control><sourceid>asme_osti_</sourceid><recordid>TN_cdi_osti_scitechconnect_1400395</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>379474</sourcerecordid><originalsourceid>FETCH-LOGICAL-a311t-21f8689a31e106daaed7ebb66ab21dc416ff77bcc0f49e5255e334ebcae23d633</originalsourceid><addsrcrecordid>eNo1kEFLAzEQRoMoWKsHz14Wbx62ZjbJbnKU0qpQEUQRTyGbnbRbbCJJKvTfu6X1NHzw3jDzEXINdAIA4h4mnDIhpTghIxCVLKVq5CkZUap4qRSj5-QipTWlwJiAEfmaOYc2F8EVi365ysWnyRiLNzQ2h3hMM__bx-A36HMqgi_yCou5yf1yi4PlcG__Gy97ozff6ZKcuWHg1XGOycd89j59Khevj8_Th0VpGEAuK3CylmoICLTujMGuwbata9NW0FkOtXNN01pLHVcoKiGQMY6tNVixrmZsTG4Pe0PKvU62z2hXNng_vKWBU8qUGKC7A2RjSCmi0z-x35i400D1vjgN-ljcwN4cWJM2qNdhG_1wv2aN4g1nf5wWaNM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials</title><source>ASME Transactions Journals</source><source>Alma/SFX Local Collection</source><creator>Chopra, O. K ; Stevens, G. L ; Tregoning, R ; Rao, A. S</creator><creatorcontrib>Chopra, O. K ; Stevens, G. L ; Tregoning, R ; Rao, A. S ; Argonne National Lab. (ANL), Argonne, IL (United States)</creatorcontrib><description>The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented.</description><identifier>ISSN: 0094-9930</identifier><identifier>EISSN: 1528-8978</identifier><identifier>DOI: 10.1115/1.4035885</identifier><language>eng</language><publisher>United States: ASME</publisher><subject>GENERAL STUDIES OF NUCLEAR REACTORS</subject><ispartof>Journal of pressure vessel technology, 2017-12, Vol.139 (6)</ispartof><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a311t-21f8689a31e106daaed7ebb66ab21dc416ff77bcc0f49e5255e334ebcae23d633</citedby><cites>FETCH-LOGICAL-a311t-21f8689a31e106daaed7ebb66ab21dc416ff77bcc0f49e5255e334ebcae23d633</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,780,784,885,27924,27925,38520</link.rule.ids><backlink>$$Uhttps://www.osti.gov/servlets/purl/1400395$$D View this record in Osti.gov$$Hfree_for_read</backlink></links><search><creatorcontrib>Chopra, O. K</creatorcontrib><creatorcontrib>Stevens, G. L</creatorcontrib><creatorcontrib>Tregoning, R</creatorcontrib><creatorcontrib>Rao, A. S</creatorcontrib><creatorcontrib>Argonne National Lab. (ANL), Argonne, IL (United States)</creatorcontrib><title>Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials</title><title>Journal of pressure vessel technology</title><addtitle>J. Pressure Vessel Technol</addtitle><description>The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented.</description><subject>GENERAL STUDIES OF NUCLEAR REACTORS</subject><issn>0094-9930</issn><issn>1528-8978</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2017</creationdate><recordtype>article</recordtype><recordid>eNo1kEFLAzEQRoMoWKsHz14Wbx62ZjbJbnKU0qpQEUQRTyGbnbRbbCJJKvTfu6X1NHzw3jDzEXINdAIA4h4mnDIhpTghIxCVLKVq5CkZUap4qRSj5-QipTWlwJiAEfmaOYc2F8EVi365ysWnyRiLNzQ2h3hMM__bx-A36HMqgi_yCou5yf1yi4PlcG__Gy97ozff6ZKcuWHg1XGOycd89j59Khevj8_Th0VpGEAuK3CylmoICLTujMGuwbata9NW0FkOtXNN01pLHVcoKiGQMY6tNVixrmZsTG4Pe0PKvU62z2hXNng_vKWBU8qUGKC7A2RjSCmi0z-x35i400D1vjgN-ljcwN4cWJM2qNdhG_1wv2aN4g1nf5wWaNM</recordid><startdate>20171201</startdate><enddate>20171201</enddate><creator>Chopra, O. K</creator><creator>Stevens, G. L</creator><creator>Tregoning, R</creator><creator>Rao, A. S</creator><general>ASME</general><scope>AAYXX</scope><scope>CITATION</scope><scope>OIOZB</scope><scope>OTOTI</scope></search><sort><creationdate>20171201</creationdate><title>Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials</title><author>Chopra, O. K ; Stevens, G. L ; Tregoning, R ; Rao, A. S</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a311t-21f8689a31e106daaed7ebb66ab21dc416ff77bcc0f49e5255e334ebcae23d633</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2017</creationdate><topic>GENERAL STUDIES OF NUCLEAR REACTORS</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Chopra, O. K</creatorcontrib><creatorcontrib>Stevens, G. L</creatorcontrib><creatorcontrib>Tregoning, R</creatorcontrib><creatorcontrib>Rao, A. S</creatorcontrib><creatorcontrib>Argonne National Lab. (ANL), Argonne, IL (United States)</creatorcontrib><collection>CrossRef</collection><collection>OSTI.GOV - Hybrid</collection><collection>OSTI.GOV</collection><jtitle>Journal of pressure vessel technology</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Chopra, O. K</au><au>Stevens, G. L</au><au>Tregoning, R</au><au>Rao, A. S</au><aucorp>Argonne National Lab. (ANL), Argonne, IL (United States)</aucorp><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials</atitle><jtitle>Journal of pressure vessel technology</jtitle><stitle>J. Pressure Vessel Technol</stitle><date>2017-12-01</date><risdate>2017</risdate><volume>139</volume><issue>6</issue><issn>0094-9930</issn><eissn>1528-8978</eissn><abstract>The American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (Code) provides rules for the design of Class 1 components of nuclear power plants. However, the Code design curves do not address the effects of light water reactor (LWR) water environments. Existing fatigue strain-versus-life (ε–N) data illustrate significant effects of LWR water environments on the fatigue resistance of pressure vessel and piping steels. Extensive studies have been conducted at Argonne National Laboratory (Argonne) and elsewhere to investigate the effects of LWR environments on the fatigue life. This article summarizes the results of these studies. The existing fatigue ε–N data were evaluated to identify the various material, environmental, and loading conditions that influence the fatigue crack initiation; a methodology for estimating fatigue lives as a function of these parameters was developed. The effects were incorporated into the ASME Code Section III fatigue evaluations in terms of an environmental correction factor, Fen, which is the ratio of fatigue life in air at room temperature to the life in the LWR water environment at reactor operating temperatures. Available fatigue data were used to develop fatigue design curves for carbon and low-alloy steels, austenitic stainless steels (SSs), and nickel–chromium–iron (Ni–Cr–Fe) alloys and their weld metals. A review of the Code Section III fatigue adjustment factors of 2 and 20 is also presented, and the possible conservatism inherent in the choice is evaluated. A brief description of potential effects of neutron irradiation on fatigue crack initiation is presented.</abstract><cop>United States</cop><pub>ASME</pub><doi>10.1115/1.4035885</doi><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0094-9930 |
ispartof | Journal of pressure vessel technology, 2017-12, Vol.139 (6) |
issn | 0094-9930 1528-8978 |
language | eng |
recordid | cdi_osti_scitechconnect_1400395 |
source | ASME Transactions Journals; Alma/SFX Local Collection |
subjects | GENERAL STUDIES OF NUCLEAR REACTORS |
title | Effect of Light Water Reactor Water Environments on the Fatigue Life of Reactor Materials |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T09%3A23%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-asme_osti_&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20Light%20Water%20Reactor%20Water%20Environments%20on%20the%20Fatigue%20Life%20of%20Reactor%20Materials&rft.jtitle=Journal%20of%20pressure%20vessel%20technology&rft.au=Chopra,%20O.%20K&rft.aucorp=Argonne%20National%20Lab.%20(ANL),%20Argonne,%20IL%20(United%20States)&rft.date=2017-12-01&rft.volume=139&rft.issue=6&rft.issn=0094-9930&rft.eissn=1528-8978&rft_id=info:doi/10.1115/1.4035885&rft_dat=%3Casme_osti_%3E379474%3C/asme_osti_%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |