강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석
Ferroelectric ceramics are broadly used for various industrial applications. In this research, the lead-free ferroelectric ceramics of $(K_{0.5}Na_{0.5})NbO_3$ was fabricated by using the solid state synthesis. The $(K_{0.5}Na_{0.5})NbO_3$ pellets were sintered at 1200, 1150 and $1100^{\circ}C$ for...
Gespeichert in:
Veröffentlicht in: | 한국표면공학회지 2017, Vol.50 (4), p.277-281 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | kor |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 281 |
---|---|
container_issue | 4 |
container_start_page | 277 |
container_title | 한국표면공학회지 |
container_volume | 50 |
creator | 현준원 변재덕 Hyun, June Won Byun, Jaeduk |
description | Ferroelectric ceramics are broadly used for various industrial applications. In this research, the lead-free ferroelectric ceramics of $(K_{0.5}Na_{0.5})NbO_3$ was fabricated by using the solid state synthesis. The $(K_{0.5}Na_{0.5})NbO_3$ pellets were sintered at 1200, 1150 and $1100^{\circ}C$ for 4 hours in air atmosphere. Field-emission scanning electron microscopy (FE-SEM) characterization of the sintered KNN ceramics revealed surface morphology and grain size. And we used the X-ray diffraction (XRD) for measuring the sample crystal phase. Temperature dependence of the dielectric constant was measured by using an LCR meter. The sintered at $1150^{\circ}C$ for 4 hours sample has a highest dielectric constant 6011 at Curie temperature ($T_C$) and dense structure with $2.33{\mu}m$ grain size. |
format | Article |
fullrecord | <record><control><sourceid>kisti</sourceid><recordid>TN_cdi_kisti_ndsl_JAKO201726439088814</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JAKO201726439088814</sourcerecordid><originalsourceid>FETCH-kisti_ndsl_JAKO2017264390888143</originalsourceid><addsrcrecordid>eNpjYeA0NDIy1bUwMDLhYOAtLs5MMjA2MzK3NDQz52Rwf7Vh6ps5C94saHmzaYuGt4KBnqmCXyKY0vRL8lcwVngzd4bCmwVz3izcoPB6Qz-Q2fJqx4Y3CxoV3nbtfNOyUeH1tpY3LXN5GFjTEnOKU3mhNDeDqptriLOHbnZmcUlmfF5KcU68l6O3v5GBobmRmYmxpYGFhYWhiTGx6gDw70Tb</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석</title><source>Alma/SFX Local Collection</source><creator>현준원 ; 변재덕 ; Hyun, June Won ; Byun, Jaeduk</creator><creatorcontrib>현준원 ; 변재덕 ; Hyun, June Won ; Byun, Jaeduk</creatorcontrib><description>Ferroelectric ceramics are broadly used for various industrial applications. In this research, the lead-free ferroelectric ceramics of $(K_{0.5}Na_{0.5})NbO_3$ was fabricated by using the solid state synthesis. The $(K_{0.5}Na_{0.5})NbO_3$ pellets were sintered at 1200, 1150 and $1100^{\circ}C$ for 4 hours in air atmosphere. Field-emission scanning electron microscopy (FE-SEM) characterization of the sintered KNN ceramics revealed surface morphology and grain size. And we used the X-ray diffraction (XRD) for measuring the sample crystal phase. Temperature dependence of the dielectric constant was measured by using an LCR meter. The sintered at $1150^{\circ}C$ for 4 hours sample has a highest dielectric constant 6011 at Curie temperature ($T_C$) and dense structure with $2.33{\mu}m$ grain size.</description><identifier>ISSN: 1225-8024</identifier><language>kor</language><ispartof>한국표면공학회지, 2017, Vol.50 (4), p.277-281</ispartof><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,780,784,885,4024</link.rule.ids></links><search><creatorcontrib>현준원</creatorcontrib><creatorcontrib>변재덕</creatorcontrib><creatorcontrib>Hyun, June Won</creatorcontrib><creatorcontrib>Byun, Jaeduk</creatorcontrib><title>강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석</title><title>한국표면공학회지</title><addtitle>Journal of the Korean institute of surface engineering</addtitle><description>Ferroelectric ceramics are broadly used for various industrial applications. In this research, the lead-free ferroelectric ceramics of $(K_{0.5}Na_{0.5})NbO_3$ was fabricated by using the solid state synthesis. The $(K_{0.5}Na_{0.5})NbO_3$ pellets were sintered at 1200, 1150 and $1100^{\circ}C$ for 4 hours in air atmosphere. Field-emission scanning electron microscopy (FE-SEM) characterization of the sintered KNN ceramics revealed surface morphology and grain size. And we used the X-ray diffraction (XRD) for measuring the sample crystal phase. Temperature dependence of the dielectric constant was measured by using an LCR meter. The sintered at $1150^{\circ}C$ for 4 hours sample has a highest dielectric constant 6011 at Curie temperature ($T_C$) and dense structure with $2.33{\mu}m$ grain size.</description><issn>1225-8024</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2017</creationdate><recordtype>article</recordtype><sourceid>JDI</sourceid><recordid>eNpjYeA0NDIy1bUwMDLhYOAtLs5MMjA2MzK3NDQz52Rwf7Vh6ps5C94saHmzaYuGt4KBnqmCXyKY0vRL8lcwVngzd4bCmwVz3izcoPB6Qz-Q2fJqx4Y3CxoV3nbtfNOyUeH1tpY3LXN5GFjTEnOKU3mhNDeDqptriLOHbnZmcUlmfF5KcU68l6O3v5GBobmRmYmxpYGFhYWhiTGx6gDw70Tb</recordid><startdate>2017</startdate><enddate>2017</enddate><creator>현준원</creator><creator>변재덕</creator><creator>Hyun, June Won</creator><creator>Byun, Jaeduk</creator><scope>JDI</scope></search><sort><creationdate>2017</creationdate><title>강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석</title><author>현준원 ; 변재덕 ; Hyun, June Won ; Byun, Jaeduk</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-kisti_ndsl_JAKO2017264390888143</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>kor</language><creationdate>2017</creationdate><toplevel>online_resources</toplevel><creatorcontrib>현준원</creatorcontrib><creatorcontrib>변재덕</creatorcontrib><creatorcontrib>Hyun, June Won</creatorcontrib><creatorcontrib>Byun, Jaeduk</creatorcontrib><collection>KoreaScience</collection><jtitle>한국표면공학회지</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>현준원</au><au>변재덕</au><au>Hyun, June Won</au><au>Byun, Jaeduk</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석</atitle><jtitle>한국표면공학회지</jtitle><addtitle>Journal of the Korean institute of surface engineering</addtitle><date>2017</date><risdate>2017</risdate><volume>50</volume><issue>4</issue><spage>277</spage><epage>281</epage><pages>277-281</pages><issn>1225-8024</issn><abstract>Ferroelectric ceramics are broadly used for various industrial applications. In this research, the lead-free ferroelectric ceramics of $(K_{0.5}Na_{0.5})NbO_3$ was fabricated by using the solid state synthesis. The $(K_{0.5}Na_{0.5})NbO_3$ pellets were sintered at 1200, 1150 and $1100^{\circ}C$ for 4 hours in air atmosphere. Field-emission scanning electron microscopy (FE-SEM) characterization of the sintered KNN ceramics revealed surface morphology and grain size. And we used the X-ray diffraction (XRD) for measuring the sample crystal phase. Temperature dependence of the dielectric constant was measured by using an LCR meter. The sintered at $1150^{\circ}C$ for 4 hours sample has a highest dielectric constant 6011 at Curie temperature ($T_C$) and dense structure with $2.33{\mu}m$ grain size.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1225-8024 |
ispartof | 한국표면공학회지, 2017, Vol.50 (4), p.277-281 |
issn | 1225-8024 |
language | kor |
recordid | cdi_kisti_ndsl_JAKO201726439088814 |
source | Alma/SFX Local Collection |
title | 강유전체(K 0.5 Na 0.5 )NbO 3 의 제조 및 전기적 특성 분석 |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T21%3A33%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-kisti&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=%EA%B0%95%EC%9C%A0%EC%A0%84%EC%B2%B4(K%200.5%20Na%200.5%20)NbO%203%20%EC%9D%98%20%EC%A0%9C%EC%A1%B0%20%EB%B0%8F%20%EC%A0%84%EA%B8%B0%EC%A0%81%20%ED%8A%B9%EC%84%B1%20%EB%B6%84%EC%84%9D&rft.jtitle=%ED%95%9C%EA%B5%AD%ED%91%9C%EB%A9%B4%EA%B3%B5%ED%95%99%ED%9A%8C%EC%A7%80&rft.au=%ED%98%84%EC%A4%80%EC%9B%90&rft.date=2017&rft.volume=50&rft.issue=4&rft.spage=277&rft.epage=281&rft.pages=277-281&rft.issn=1225-8024&rft_id=info:doi/&rft_dat=%3Ckisti%3EJAKO201726439088814%3C/kisti%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |