도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향

Statement of problem: Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. Lithium disilicate glass-ceramic system has superior color reproducibility, because it uses the ceramic ingot which is similar to teeth s...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Taehan Chikwa Poch'ol Hakhoe chi 2005, Vol.43 (5), p.587-598
Hauptverfasser: 성동환, 이임기, 송진원, 복원미, 안승근, 박찬운, Seong Dong-Hwan, Lee Im-Gi, Sohng Jin-Won, Bok Won-Mi, Ahn Seung-Geun, Park Charn-Woon
Format: Artikel
Sprache:kor
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 598
container_issue 5
container_start_page 587
container_title Taehan Chikwa Poch'ol Hakhoe chi
container_volume 43
creator 성동환
이임기
송진원
복원미
안승근
박찬운
Seong Dong-Hwan
Lee Im-Gi
Sohng Jin-Won
Bok Won-Mi
Ahn Seung-Geun
Park Charn-Woon
description Statement of problem: Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. Lithium disilicate glass-ceramic system has superior color reproducibility, because it uses the ceramic ingot which is similar to teeth shade and uses the staining technique and layering technique. However, staining technique has a fault of discoloration. Also, porcelain is divided core and dentin layer, it is not enough to study about the influence of porcelain layer thickness and shade on the shade of ceramic restorations. Purpose: The purpose of this study was to evaluate the influence of porcelain layer thickness and color on the final shade of ceramic restorations. Materials and method: The CIE $L^*a^*b^*$(CIELAB) values of 72 assembled specimens, each consisting of 3 discs (enamel porcelain 0.2 mm/dentin porcelain -1.2, 0.9, 0.7, 0.5 or 0.3 mm/ceramic core -0.3, 0.5, 0.7, 0.9 or 1.2 mm, diameter is 1.0 mm) were evaluated with a spectrophotometer (Model Chromaview 300, Spectron Tech Co, Korea) for the shade A1, A2, A3 and A4. Distilled water (refractive index: 1.7) was used to attain optical contact between the layers. White, white gray, and white brown backgrounds were used to assess the influence of the background on the final shade. And the mean color difference value$({\Delta}E)$ was calculated. Results and conclusion: The results obtained from this study were as follows. 1. There was a significant correlation between the thickness ratio of the ceramic core/dentin porcelain system and $L^*,\;a^*\;and\;b^*$ values when the total thickness of specimen combination was smaller than 1.4 mm(P
format Article
fullrecord <record><control><sourceid>kisti</sourceid><recordid>TN_cdi_kisti_ndsl_JAKO200526813010297</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JAKO200526813010297</sourcerecordid><originalsourceid>FETCH-LOGICAL-k526-d35a2015b9f8e181f66d13392477b504bd8af1806d678411811d494d555b3fa83</originalsourceid><addsrcrecordid>eNotj7tKA0EYRqdQMMS8wzSWC3Of2TIE74GApA87TAaWBJvxARQV1MYIoiuYgIJdQCFZiOgTOb_v4KqpvuIcDnwrqEY4oQkzWq6hRgi5JVwxbSQ3NXQQr89gMoVFCeMCx5vR10cBD8cYTi9hPMdLelHEWRmnn78OlI_wfP4nPL3B_QjH1wW8F_HqFkNx8n33so5WfTYM_cZy66i7tdlt7STtzvZuq9lOBpKpxHGZMUKlTb3pU0O9Uo5ynjKhtZVEWGcyTw1RTmkjaGVQJ1LhpJSW-8zwOtr4zw7ycJT3Dl0Y9vaa-x1GSNU3tPpMWKr5Dw1XYR8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향</title><source>KoreaMed Open Access</source><creator>성동환 ; 이임기 ; 송진원 ; 복원미 ; 안승근 ; 박찬운 ; Seong Dong-Hwan ; Lee Im-Gi ; Sohng Jin-Won ; Bok Won-Mi ; Ahn Seung-Geun ; Park Charn-Woon</creator><creatorcontrib>성동환 ; 이임기 ; 송진원 ; 복원미 ; 안승근 ; 박찬운 ; Seong Dong-Hwan ; Lee Im-Gi ; Sohng Jin-Won ; Bok Won-Mi ; Ahn Seung-Geun ; Park Charn-Woon</creatorcontrib><description>Statement of problem: Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. Lithium disilicate glass-ceramic system has superior color reproducibility, because it uses the ceramic ingot which is similar to teeth shade and uses the staining technique and layering technique. However, staining technique has a fault of discoloration. Also, porcelain is divided core and dentin layer, it is not enough to study about the influence of porcelain layer thickness and shade on the shade of ceramic restorations. Purpose: The purpose of this study was to evaluate the influence of porcelain layer thickness and color on the final shade of ceramic restorations. Materials and method: The CIE $L^*a^*b^*$(CIELAB) values of 72 assembled specimens, each consisting of 3 discs (enamel porcelain 0.2 mm/dentin porcelain -1.2, 0.9, 0.7, 0.5 or 0.3 mm/ceramic core -0.3, 0.5, 0.7, 0.9 or 1.2 mm, diameter is 1.0 mm) were evaluated with a spectrophotometer (Model Chromaview 300, Spectron Tech Co, Korea) for the shade A1, A2, A3 and A4. Distilled water (refractive index: 1.7) was used to attain optical contact between the layers. White, white gray, and white brown backgrounds were used to assess the influence of the background on the final shade. And the mean color difference value$({\Delta}E)$ was calculated. Results and conclusion: The results obtained from this study were as follows. 1. There was a significant correlation between the thickness ratio of the ceramic core/dentin porcelain system and $L^*,\;a^*\;and\;b^*$ values when the total thickness of specimen combination was smaller than 1.4 mm(P&lt;0.05). 2. The specimen which the ceramic core thickness was more than 0.7 mm had the best masking effect against background colors. 3. The mean color difference value$({\Delta}E)$ is smaller than 2 $({\Delta}E&lt;2)$ when the ceramic core thickness was larger than 0.7 mm and the total thickness of specimen was more than 1.4 mm.</description><identifier>ISSN: 0301-2875</identifier><language>kor</language><ispartof>Taehan Chikwa Poch'ol Hakhoe chi, 2005, Vol.43 (5), p.587-598</ispartof><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,776,780,881,4009</link.rule.ids></links><search><creatorcontrib>성동환</creatorcontrib><creatorcontrib>이임기</creatorcontrib><creatorcontrib>송진원</creatorcontrib><creatorcontrib>복원미</creatorcontrib><creatorcontrib>안승근</creatorcontrib><creatorcontrib>박찬운</creatorcontrib><creatorcontrib>Seong Dong-Hwan</creatorcontrib><creatorcontrib>Lee Im-Gi</creatorcontrib><creatorcontrib>Sohng Jin-Won</creatorcontrib><creatorcontrib>Bok Won-Mi</creatorcontrib><creatorcontrib>Ahn Seung-Geun</creatorcontrib><creatorcontrib>Park Charn-Woon</creatorcontrib><title>도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향</title><title>Taehan Chikwa Poch'ol Hakhoe chi</title><addtitle>The journal of Korean academy of prosthodontics</addtitle><description>Statement of problem: Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. Lithium disilicate glass-ceramic system has superior color reproducibility, because it uses the ceramic ingot which is similar to teeth shade and uses the staining technique and layering technique. However, staining technique has a fault of discoloration. Also, porcelain is divided core and dentin layer, it is not enough to study about the influence of porcelain layer thickness and shade on the shade of ceramic restorations. Purpose: The purpose of this study was to evaluate the influence of porcelain layer thickness and color on the final shade of ceramic restorations. Materials and method: The CIE $L^*a^*b^*$(CIELAB) values of 72 assembled specimens, each consisting of 3 discs (enamel porcelain 0.2 mm/dentin porcelain -1.2, 0.9, 0.7, 0.5 or 0.3 mm/ceramic core -0.3, 0.5, 0.7, 0.9 or 1.2 mm, diameter is 1.0 mm) were evaluated with a spectrophotometer (Model Chromaview 300, Spectron Tech Co, Korea) for the shade A1, A2, A3 and A4. Distilled water (refractive index: 1.7) was used to attain optical contact between the layers. White, white gray, and white brown backgrounds were used to assess the influence of the background on the final shade. And the mean color difference value$({\Delta}E)$ was calculated. Results and conclusion: The results obtained from this study were as follows. 1. There was a significant correlation between the thickness ratio of the ceramic core/dentin porcelain system and $L^*,\;a^*\;and\;b^*$ values when the total thickness of specimen combination was smaller than 1.4 mm(P&lt;0.05). 2. The specimen which the ceramic core thickness was more than 0.7 mm had the best masking effect against background colors. 3. The mean color difference value$({\Delta}E)$ is smaller than 2 $({\Delta}E&lt;2)$ when the ceramic core thickness was larger than 0.7 mm and the total thickness of specimen was more than 1.4 mm.</description><issn>0301-2875</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2005</creationdate><recordtype>article</recordtype><sourceid>JDI</sourceid><recordid>eNotj7tKA0EYRqdQMMS8wzSWC3Of2TIE74GApA87TAaWBJvxARQV1MYIoiuYgIJdQCFZiOgTOb_v4KqpvuIcDnwrqEY4oQkzWq6hRgi5JVwxbSQ3NXQQr89gMoVFCeMCx5vR10cBD8cYTi9hPMdLelHEWRmnn78OlI_wfP4nPL3B_QjH1wW8F_HqFkNx8n33so5WfTYM_cZy66i7tdlt7STtzvZuq9lOBpKpxHGZMUKlTb3pU0O9Uo5ynjKhtZVEWGcyTw1RTmkjaGVQJ1LhpJSW-8zwOtr4zw7ycJT3Dl0Y9vaa-x1GSNU3tPpMWKr5Dw1XYR8</recordid><startdate>2005</startdate><enddate>2005</enddate><creator>성동환</creator><creator>이임기</creator><creator>송진원</creator><creator>복원미</creator><creator>안승근</creator><creator>박찬운</creator><creator>Seong Dong-Hwan</creator><creator>Lee Im-Gi</creator><creator>Sohng Jin-Won</creator><creator>Bok Won-Mi</creator><creator>Ahn Seung-Geun</creator><creator>Park Charn-Woon</creator><scope>JDI</scope></search><sort><creationdate>2005</creationdate><title>도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향</title><author>성동환 ; 이임기 ; 송진원 ; 복원미 ; 안승근 ; 박찬운 ; Seong Dong-Hwan ; Lee Im-Gi ; Sohng Jin-Won ; Bok Won-Mi ; Ahn Seung-Geun ; Park Charn-Woon</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-k526-d35a2015b9f8e181f66d13392477b504bd8af1806d678411811d494d555b3fa83</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>kor</language><creationdate>2005</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>성동환</creatorcontrib><creatorcontrib>이임기</creatorcontrib><creatorcontrib>송진원</creatorcontrib><creatorcontrib>복원미</creatorcontrib><creatorcontrib>안승근</creatorcontrib><creatorcontrib>박찬운</creatorcontrib><creatorcontrib>Seong Dong-Hwan</creatorcontrib><creatorcontrib>Lee Im-Gi</creatorcontrib><creatorcontrib>Sohng Jin-Won</creatorcontrib><creatorcontrib>Bok Won-Mi</creatorcontrib><creatorcontrib>Ahn Seung-Geun</creatorcontrib><creatorcontrib>Park Charn-Woon</creatorcontrib><collection>KoreaScience</collection><jtitle>Taehan Chikwa Poch'ol Hakhoe chi</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>성동환</au><au>이임기</au><au>송진원</au><au>복원미</au><au>안승근</au><au>박찬운</au><au>Seong Dong-Hwan</au><au>Lee Im-Gi</au><au>Sohng Jin-Won</au><au>Bok Won-Mi</au><au>Ahn Seung-Geun</au><au>Park Charn-Woon</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향</atitle><jtitle>Taehan Chikwa Poch'ol Hakhoe chi</jtitle><addtitle>The journal of Korean academy of prosthodontics</addtitle><date>2005</date><risdate>2005</risdate><volume>43</volume><issue>5</issue><spage>587</spage><epage>598</epage><pages>587-598</pages><issn>0301-2875</issn><abstract>Statement of problem: Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. Lithium disilicate glass-ceramic system has superior color reproducibility, because it uses the ceramic ingot which is similar to teeth shade and uses the staining technique and layering technique. However, staining technique has a fault of discoloration. Also, porcelain is divided core and dentin layer, it is not enough to study about the influence of porcelain layer thickness and shade on the shade of ceramic restorations. Purpose: The purpose of this study was to evaluate the influence of porcelain layer thickness and color on the final shade of ceramic restorations. Materials and method: The CIE $L^*a^*b^*$(CIELAB) values of 72 assembled specimens, each consisting of 3 discs (enamel porcelain 0.2 mm/dentin porcelain -1.2, 0.9, 0.7, 0.5 or 0.3 mm/ceramic core -0.3, 0.5, 0.7, 0.9 or 1.2 mm, diameter is 1.0 mm) were evaluated with a spectrophotometer (Model Chromaview 300, Spectron Tech Co, Korea) for the shade A1, A2, A3 and A4. Distilled water (refractive index: 1.7) was used to attain optical contact between the layers. White, white gray, and white brown backgrounds were used to assess the influence of the background on the final shade. And the mean color difference value$({\Delta}E)$ was calculated. Results and conclusion: The results obtained from this study were as follows. 1. There was a significant correlation between the thickness ratio of the ceramic core/dentin porcelain system and $L^*,\;a^*\;and\;b^*$ values when the total thickness of specimen combination was smaller than 1.4 mm(P&lt;0.05). 2. The specimen which the ceramic core thickness was more than 0.7 mm had the best masking effect against background colors. 3. The mean color difference value$({\Delta}E)$ is smaller than 2 $({\Delta}E&lt;2)$ when the ceramic core thickness was larger than 0.7 mm and the total thickness of specimen was more than 1.4 mm.</abstract><tpages>12</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 0301-2875
ispartof Taehan Chikwa Poch'ol Hakhoe chi, 2005, Vol.43 (5), p.587-598
issn 0301-2875
language kor
recordid cdi_kisti_ndsl_JAKO200526813010297
source KoreaMed Open Access
title 도재층의 두께와 색이 도재수복물의 최종 색조에 미치는 영향
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T07%3A18%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-kisti&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=%EB%8F%84%EC%9E%AC%EC%B8%B5%EC%9D%98%20%EB%91%90%EA%BB%98%EC%99%80%20%EC%83%89%EC%9D%B4%20%EB%8F%84%EC%9E%AC%EC%88%98%EB%B3%B5%EB%AC%BC%EC%9D%98%20%EC%B5%9C%EC%A2%85%20%EC%83%89%EC%A1%B0%EC%97%90%20%EB%AF%B8%EC%B9%98%EB%8A%94%20%EC%98%81%ED%96%A5&rft.jtitle=Taehan%20Chikwa%20Poch'ol%20Hakhoe%20chi&rft.au=%EC%84%B1%EB%8F%99%ED%99%98&rft.date=2005&rft.volume=43&rft.issue=5&rft.spage=587&rft.epage=598&rft.pages=587-598&rft.issn=0301-2875&rft_id=info:doi/&rft_dat=%3Ckisti%3EJAKO200526813010297%3C/kisti%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true