상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향

This study investigated that the effect of rewetting agent on dentinal microtensile bond strength(${\mu}TBS$). Human molars were sectioned to expose the superficial dentin surfaces. Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (0)], and again subdi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:大韓齒科保存學會誌 2004, Vol.29 (2), p.153-161
Hauptverfasser: 강희영, 조영곤, 김종욱, 박병철, 유상훈, 진철희, 최희영, 기영재, Kang, Hee-Young, Cho, Young-Gon, Kim, Jong-Uk, Park, Byung-Cheul, Yoo, Sang-Hoon, Jin, Cheul-Hee, Choi, Hee-Young, Ki, Young-Jae
Format: Artikel
Sprache:kor
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 161
container_issue 2
container_start_page 153
container_title 大韓齒科保存學會誌
container_volume 29
creator 강희영
조영곤
김종욱
박병철
유상훈
진철희
최희영
기영재
Kang, Hee-Young
Cho, Young-Gon
Kim, Jong-Uk
Park, Byung-Cheul
Yoo, Sang-Hoon
Jin, Cheul-Hee
Choi, Hee-Young
Ki, Young-Jae
description This study investigated that the effect of rewetting agent on dentinal microtensile bond strength(${\mu}TBS$). Human molars were sectioned to expose the superficial dentin surfaces. Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (0)], and again subdivided into five groups by different dentin surface treatment-dry for 15s (D), blot dry (BD) or dry for 15s, and rewet with different rewetting agents [distilled water (DW), Gluma Desensitizer (GD) and Aqua-Prep (AP)] for 30s. After application of adhesive, composite resin was built up on the bonding surface. Each tooth was sectioned to obtain stick with $1\textrm{mm}^2$ cross sectional area and the ${\mu}TBS$ was determined by EZ test. In the S group, the mean ${\mu}TBS$ of GD, AP, and BD group was significantly higher than that of DW and D group (p < 0.05), In the O group, the mean, ${\mu}TBS$ of AP, GD, BD and DW group was significantly higher than that of D group (p < 0.05). The data suggested that Gluma Desensitizer and Aqua-Prep could be successfully used as rewetting agents, and Distilled water could be acceptable in aceton based adhesive system only.
format Article
fullrecord <record><control><sourceid>kisti</sourceid><recordid>TN_cdi_kisti_ndsl_JAKO200411922113998</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JAKO200411922113998</sourcerecordid><originalsourceid>FETCH-LOGICAL-k520-6a2b74a71319296d9ba6330d36fa8c4fd6f8d386fee775919f69c91c31490be43</originalsourceid><addsrcrecordid>eNotjD9Lw0AcQG9QsNR-h1scA_cvl7uxFP8XutS5JLkchBaX-AEMZpAudjBaJJYOLVIQDIIQv1Ly63fQotMbHu_toRZlzHWIkuIAdZIkDghRnHhC8xa6grsU8gze7uF5hmGZwsummRUYFu8Ypl9QrGBZ1OUtbj4qyCp4rWCxxvVnuc03dZk3D9mu28nveTN9xDBPt0_rQ7Rv_UkSdf7ZRsOT42HvzOkPTs973b4zdhlxpM8CT_ge5VQzLY0OfMk5MVxaX4XCGmmV4UraKPI8V1NtpQ41DTkVmgSR4G109Lcdx8lNPLo2yWR00b0cMEIE_X0ySrnWiv8AD91kDQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향</title><source>KoreaMed Open Access</source><creator>강희영 ; 조영곤 ; 김종욱 ; 박병철 ; 유상훈 ; 진철희 ; 최희영 ; 기영재 ; Kang, Hee-Young ; Cho, Young-Gon ; Kim, Jong-Uk ; Park, Byung-Cheul ; Yoo, Sang-Hoon ; Jin, Cheul-Hee ; Choi, Hee-Young ; Ki, Young-Jae</creator><creatorcontrib>강희영 ; 조영곤 ; 김종욱 ; 박병철 ; 유상훈 ; 진철희 ; 최희영 ; 기영재 ; Kang, Hee-Young ; Cho, Young-Gon ; Kim, Jong-Uk ; Park, Byung-Cheul ; Yoo, Sang-Hoon ; Jin, Cheul-Hee ; Choi, Hee-Young ; Ki, Young-Jae</creatorcontrib><description>This study investigated that the effect of rewetting agent on dentinal microtensile bond strength(${\mu}TBS$). Human molars were sectioned to expose the superficial dentin surfaces. Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (0)], and again subdivided into five groups by different dentin surface treatment-dry for 15s (D), blot dry (BD) or dry for 15s, and rewet with different rewetting agents [distilled water (DW), Gluma Desensitizer (GD) and Aqua-Prep (AP)] for 30s. After application of adhesive, composite resin was built up on the bonding surface. Each tooth was sectioned to obtain stick with $1\textrm{mm}^2$ cross sectional area and the ${\mu}TBS$ was determined by EZ test. In the S group, the mean ${\mu}TBS$ of GD, AP, and BD group was significantly higher than that of DW and D group (p &lt; 0.05), In the O group, the mean, ${\mu}TBS$ of AP, GD, BD and DW group was significantly higher than that of D group (p &lt; 0.05). The data suggested that Gluma Desensitizer and Aqua-Prep could be successfully used as rewetting agents, and Distilled water could be acceptable in aceton based adhesive system only.</description><identifier>ISSN: 1225-0864</identifier><language>kor</language><ispartof>大韓齒科保存學會誌, 2004, Vol.29 (2), p.153-161</ispartof><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,314,776,780,881,4010</link.rule.ids></links><search><creatorcontrib>강희영</creatorcontrib><creatorcontrib>조영곤</creatorcontrib><creatorcontrib>김종욱</creatorcontrib><creatorcontrib>박병철</creatorcontrib><creatorcontrib>유상훈</creatorcontrib><creatorcontrib>진철희</creatorcontrib><creatorcontrib>최희영</creatorcontrib><creatorcontrib>기영재</creatorcontrib><creatorcontrib>Kang, Hee-Young</creatorcontrib><creatorcontrib>Cho, Young-Gon</creatorcontrib><creatorcontrib>Kim, Jong-Uk</creatorcontrib><creatorcontrib>Park, Byung-Cheul</creatorcontrib><creatorcontrib>Yoo, Sang-Hoon</creatorcontrib><creatorcontrib>Jin, Cheul-Hee</creatorcontrib><creatorcontrib>Choi, Hee-Young</creatorcontrib><creatorcontrib>Ki, Young-Jae</creatorcontrib><title>상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향</title><title>大韓齒科保存學會誌</title><addtitle>Journal of Korean Academy of Operative Dentistry</addtitle><description>This study investigated that the effect of rewetting agent on dentinal microtensile bond strength(${\mu}TBS$). Human molars were sectioned to expose the superficial dentin surfaces. Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (0)], and again subdivided into five groups by different dentin surface treatment-dry for 15s (D), blot dry (BD) or dry for 15s, and rewet with different rewetting agents [distilled water (DW), Gluma Desensitizer (GD) and Aqua-Prep (AP)] for 30s. After application of adhesive, composite resin was built up on the bonding surface. Each tooth was sectioned to obtain stick with $1\textrm{mm}^2$ cross sectional area and the ${\mu}TBS$ was determined by EZ test. In the S group, the mean ${\mu}TBS$ of GD, AP, and BD group was significantly higher than that of DW and D group (p &lt; 0.05), In the O group, the mean, ${\mu}TBS$ of AP, GD, BD and DW group was significantly higher than that of D group (p &lt; 0.05). The data suggested that Gluma Desensitizer and Aqua-Prep could be successfully used as rewetting agents, and Distilled water could be acceptable in aceton based adhesive system only.</description><issn>1225-0864</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2004</creationdate><recordtype>article</recordtype><sourceid>JDI</sourceid><recordid>eNotjD9Lw0AcQG9QsNR-h1scA_cvl7uxFP8XutS5JLkchBaX-AEMZpAudjBaJJYOLVIQDIIQv1Ly63fQotMbHu_toRZlzHWIkuIAdZIkDghRnHhC8xa6grsU8gze7uF5hmGZwsummRUYFu8Ypl9QrGBZ1OUtbj4qyCp4rWCxxvVnuc03dZk3D9mu28nveTN9xDBPt0_rQ7Rv_UkSdf7ZRsOT42HvzOkPTs973b4zdhlxpM8CT_ge5VQzLY0OfMk5MVxaX4XCGmmV4UraKPI8V1NtpQ41DTkVmgSR4G109Lcdx8lNPLo2yWR00b0cMEIE_X0ySrnWiv8AD91kDQ</recordid><startdate>2004</startdate><enddate>2004</enddate><creator>강희영</creator><creator>조영곤</creator><creator>김종욱</creator><creator>박병철</creator><creator>유상훈</creator><creator>진철희</creator><creator>최희영</creator><creator>기영재</creator><creator>Kang, Hee-Young</creator><creator>Cho, Young-Gon</creator><creator>Kim, Jong-Uk</creator><creator>Park, Byung-Cheul</creator><creator>Yoo, Sang-Hoon</creator><creator>Jin, Cheul-Hee</creator><creator>Choi, Hee-Young</creator><creator>Ki, Young-Jae</creator><scope>JDI</scope></search><sort><creationdate>2004</creationdate><title>상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향</title><author>강희영 ; 조영곤 ; 김종욱 ; 박병철 ; 유상훈 ; 진철희 ; 최희영 ; 기영재 ; Kang, Hee-Young ; Cho, Young-Gon ; Kim, Jong-Uk ; Park, Byung-Cheul ; Yoo, Sang-Hoon ; Jin, Cheul-Hee ; Choi, Hee-Young ; Ki, Young-Jae</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-k520-6a2b74a71319296d9ba6330d36fa8c4fd6f8d386fee775919f69c91c31490be43</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>kor</language><creationdate>2004</creationdate><toplevel>online_resources</toplevel><creatorcontrib>강희영</creatorcontrib><creatorcontrib>조영곤</creatorcontrib><creatorcontrib>김종욱</creatorcontrib><creatorcontrib>박병철</creatorcontrib><creatorcontrib>유상훈</creatorcontrib><creatorcontrib>진철희</creatorcontrib><creatorcontrib>최희영</creatorcontrib><creatorcontrib>기영재</creatorcontrib><creatorcontrib>Kang, Hee-Young</creatorcontrib><creatorcontrib>Cho, Young-Gon</creatorcontrib><creatorcontrib>Kim, Jong-Uk</creatorcontrib><creatorcontrib>Park, Byung-Cheul</creatorcontrib><creatorcontrib>Yoo, Sang-Hoon</creatorcontrib><creatorcontrib>Jin, Cheul-Hee</creatorcontrib><creatorcontrib>Choi, Hee-Young</creatorcontrib><creatorcontrib>Ki, Young-Jae</creatorcontrib><collection>KoreaScience</collection><jtitle>大韓齒科保存學會誌</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>강희영</au><au>조영곤</au><au>김종욱</au><au>박병철</au><au>유상훈</au><au>진철희</au><au>최희영</au><au>기영재</au><au>Kang, Hee-Young</au><au>Cho, Young-Gon</au><au>Kim, Jong-Uk</au><au>Park, Byung-Cheul</au><au>Yoo, Sang-Hoon</au><au>Jin, Cheul-Hee</au><au>Choi, Hee-Young</au><au>Ki, Young-Jae</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향</atitle><jtitle>大韓齒科保存學會誌</jtitle><addtitle>Journal of Korean Academy of Operative Dentistry</addtitle><date>2004</date><risdate>2004</risdate><volume>29</volume><issue>2</issue><spage>153</spage><epage>161</epage><pages>153-161</pages><issn>1225-0864</issn><abstract>This study investigated that the effect of rewetting agent on dentinal microtensile bond strength(${\mu}TBS$). Human molars were sectioned to expose the superficial dentin surfaces. Samples were divided into two groups according to type of adhesives-Single Bond (S) and One-Step (0)], and again subdivided into five groups by different dentin surface treatment-dry for 15s (D), blot dry (BD) or dry for 15s, and rewet with different rewetting agents [distilled water (DW), Gluma Desensitizer (GD) and Aqua-Prep (AP)] for 30s. After application of adhesive, composite resin was built up on the bonding surface. Each tooth was sectioned to obtain stick with $1\textrm{mm}^2$ cross sectional area and the ${\mu}TBS$ was determined by EZ test. In the S group, the mean ${\mu}TBS$ of GD, AP, and BD group was significantly higher than that of DW and D group (p &lt; 0.05), In the O group, the mean, ${\mu}TBS$ of AP, GD, BD and DW group was significantly higher than that of D group (p &lt; 0.05). The data suggested that Gluma Desensitizer and Aqua-Prep could be successfully used as rewetting agents, and Distilled water could be acceptable in aceton based adhesive system only.</abstract><tpages>9</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 1225-0864
ispartof 大韓齒科保存學會誌, 2004, Vol.29 (2), p.153-161
issn 1225-0864
language kor
recordid cdi_kisti_ndsl_JAKO200411922113998
source KoreaMed Open Access
title 상아질에 적용된 재 습윤제가 미세인장 결합강도에 미치는 영향
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-14T09%3A53%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-kisti&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=%EC%83%81%EC%95%84%EC%A7%88%EC%97%90%20%EC%A0%81%EC%9A%A9%EB%90%9C%20%EC%9E%AC%20%EC%8A%B5%EC%9C%A4%EC%A0%9C%EA%B0%80%20%EB%AF%B8%EC%84%B8%EC%9D%B8%EC%9E%A5%20%EA%B2%B0%ED%95%A9%EA%B0%95%EB%8F%84%EC%97%90%20%EB%AF%B8%EC%B9%98%EB%8A%94%20%EC%98%81%ED%96%A5&rft.jtitle=%E5%A4%A7%E9%9F%93%E9%BD%92%E7%A7%91%E4%BF%9D%E5%AD%98%E5%AD%B8%E6%9C%83%E8%AA%8C&rft.au=%EA%B0%95%ED%9D%AC%EC%98%81&rft.date=2004&rft.volume=29&rft.issue=2&rft.spage=153&rft.epage=161&rft.pages=153-161&rft.issn=1225-0864&rft_id=info:doi/&rft_dat=%3Ckisti%3EJAKO200411922113998%3C/kisti%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true