SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구

The effect of loading waveform on elevated temperature low-cycle fatigue crack growth behavior in a SUS 304 stainless steel have been investigated under symmetrical trangular (fast-fast), trapezoidal and asymmetrical(fast-slow, slow-fast) waveforms at 650.deg. C. It was found that the crack growth r...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Han-guk haeyang gonghak hoeji (Online) 1992, Vol.6 (1), p.122-130
Hauptverfasser: 이상록(Sang-Rok Lee), 이학주(Hak-Joo Lee), 오세욱(Sae-Wook Oh), 허정원(Chung-Weon Hue), 임만배(Man-Bea Lim)
Format: Artikel
Sprache:kor
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 130
container_issue 1
container_start_page 122
container_title Han-guk haeyang gonghak hoeji (Online)
container_volume 6
creator 이상록(Sang-Rok Lee)
이학주(Hak-Joo Lee)
오세욱(Sae-Wook Oh)
허정원(Chung-Weon Hue)
임만배(Man-Bea Lim)
description The effect of loading waveform on elevated temperature low-cycle fatigue crack growth behavior in a SUS 304 stainless steel have been investigated under symmetrical trangular (fast-fast), trapezoidal and asymmetrical(fast-slow, slow-fast) waveforms at 650.deg. C. It was found that the crack growth rate in fast-slow loading waveform appeared to be higher a little and the crack growth rate in slow-fast loading waveform much higer than that in fast-fast loading waveform, and difference in crack growth rate between fast-show and slow-fast waveforms nearly didn't appear in the region of da/dN>10/sup -2/ The crack growth rate in the trapezoidal loading waveform with t/sub h/=500sec appeared to be faster than that in slow(500sec)-fast(1sec). In addition, parameter modified J-integral could be considered as useful parameter for fatigue crack growth rate in all waveforms. The result obtained are as follow. da/dN=4.91*10/sup -3/ (.DELTA. J/sub c/)/sup 0.565/.
format Article
fullrecord <record><control><sourceid>nurimedia_kisti</sourceid><recordid>TN_cdi_kisti_ndsl_JAKO199211920577694</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><nurid>NODE00706222</nurid><sourcerecordid>NODE00706222</sourcerecordid><originalsourceid>FETCH-LOGICAL-k822-e892ddb6a547911218809a3919b6973ec5b07a6f43d40afc207640bb1af5379f3</originalsourceid><addsrcrecordid>eNpVT8tKw0AAXETBUvsPuXgM7CO7mz2WWp_FHlrPYdMkEFqLNPXgzUMRhEortDQHhQoKCh5CrejBL8pu_sH4APE0D2YGZgUUMLa5yTiiq6CAMKYm5Iyvg1IUhS6khHBOGSyAfuOoYRBopclU38ZGNo31_XU2HGbxVM_Ghpok6uHdSF_mOn7MJh_q7iZ9m-vZUs8HeUpfXKnRwFDJyMgNvVj-63_tjS7T5FwlT2rxrfUsSV-fN8BaIDuRX_rFImhuV5uVXbNW39mrlGtm28bY9G2BPc9lklpcIISRbUMhiUDCZYITv0VdyCULLOJZUAYtnD-0oOsiGVDCRUCKYPNnth1G_dDpelHH2S8f1JEQGCGBIeWcCesv1z3thce-F0rnJCeyd-Yc1reqEHLIMMbkE2zPhN0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구</title><source>Alma/SFX Local Collection</source><creator>이상록(Sang-Rok Lee) ; 이학주(Hak-Joo Lee) ; 오세욱(Sae-Wook Oh) ; 허정원(Chung-Weon Hue) ; 임만배(Man-Bea Lim)</creator><creatorcontrib>이상록(Sang-Rok Lee) ; 이학주(Hak-Joo Lee) ; 오세욱(Sae-Wook Oh) ; 허정원(Chung-Weon Hue) ; 임만배(Man-Bea Lim)</creatorcontrib><description>The effect of loading waveform on elevated temperature low-cycle fatigue crack growth behavior in a SUS 304 stainless steel have been investigated under symmetrical trangular (fast-fast), trapezoidal and asymmetrical(fast-slow, slow-fast) waveforms at 650.deg. C. It was found that the crack growth rate in fast-slow loading waveform appeared to be higher a little and the crack growth rate in slow-fast loading waveform much higer than that in fast-fast loading waveform, and difference in crack growth rate between fast-show and slow-fast waveforms nearly didn't appear in the region of da/dN&gt;10/sup -2/ The crack growth rate in the trapezoidal loading waveform with t/sub h/=500sec appeared to be faster than that in slow(500sec)-fast(1sec). In addition, parameter modified J-integral could be considered as useful parameter for fatigue crack growth rate in all waveforms. The result obtained are as follow. da/dN=4.91*10/sup -3/ (.DELTA. J/sub c/)/sup 0.565/.</description><identifier>ISSN: 1225-0767</identifier><identifier>EISSN: 2287-6715</identifier><language>kor</language><publisher>한국해양공학회</publisher><ispartof>Han-guk haeyang gonghak hoeji (Online), 1992, Vol.6 (1), p.122-130</ispartof><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,315,781,785,886,4025</link.rule.ids></links><search><creatorcontrib>이상록(Sang-Rok Lee)</creatorcontrib><creatorcontrib>이학주(Hak-Joo Lee)</creatorcontrib><creatorcontrib>오세욱(Sae-Wook Oh)</creatorcontrib><creatorcontrib>허정원(Chung-Weon Hue)</creatorcontrib><creatorcontrib>임만배(Man-Bea Lim)</creatorcontrib><title>SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구</title><title>Han-guk haeyang gonghak hoeji (Online)</title><addtitle>Journal of ocean engineering and technology</addtitle><description>The effect of loading waveform on elevated temperature low-cycle fatigue crack growth behavior in a SUS 304 stainless steel have been investigated under symmetrical trangular (fast-fast), trapezoidal and asymmetrical(fast-slow, slow-fast) waveforms at 650.deg. C. It was found that the crack growth rate in fast-slow loading waveform appeared to be higher a little and the crack growth rate in slow-fast loading waveform much higer than that in fast-fast loading waveform, and difference in crack growth rate between fast-show and slow-fast waveforms nearly didn't appear in the region of da/dN&gt;10/sup -2/ The crack growth rate in the trapezoidal loading waveform with t/sub h/=500sec appeared to be faster than that in slow(500sec)-fast(1sec). In addition, parameter modified J-integral could be considered as useful parameter for fatigue crack growth rate in all waveforms. The result obtained are as follow. da/dN=4.91*10/sup -3/ (.DELTA. J/sub c/)/sup 0.565/.</description><issn>1225-0767</issn><issn>2287-6715</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1992</creationdate><recordtype>article</recordtype><sourceid>JDI</sourceid><recordid>eNpVT8tKw0AAXETBUvsPuXgM7CO7mz2WWp_FHlrPYdMkEFqLNPXgzUMRhEortDQHhQoKCh5CrejBL8pu_sH4APE0D2YGZgUUMLa5yTiiq6CAMKYm5Iyvg1IUhS6khHBOGSyAfuOoYRBopclU38ZGNo31_XU2HGbxVM_Ghpok6uHdSF_mOn7MJh_q7iZ9m-vZUs8HeUpfXKnRwFDJyMgNvVj-63_tjS7T5FwlT2rxrfUsSV-fN8BaIDuRX_rFImhuV5uVXbNW39mrlGtm28bY9G2BPc9lklpcIISRbUMhiUDCZYITv0VdyCULLOJZUAYtnD-0oOsiGVDCRUCKYPNnth1G_dDpelHH2S8f1JEQGCGBIeWcCesv1z3thce-F0rnJCeyd-Yc1reqEHLIMMbkE2zPhN0</recordid><startdate>1992</startdate><enddate>1992</enddate><creator>이상록(Sang-Rok Lee)</creator><creator>이학주(Hak-Joo Lee)</creator><creator>오세욱(Sae-Wook Oh)</creator><creator>허정원(Chung-Weon Hue)</creator><creator>임만배(Man-Bea Lim)</creator><general>한국해양공학회</general><scope>DBRKI</scope><scope>TDB</scope><scope>JDI</scope></search><sort><creationdate>1992</creationdate><title>SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구</title><author>이상록(Sang-Rok Lee) ; 이학주(Hak-Joo Lee) ; 오세욱(Sae-Wook Oh) ; 허정원(Chung-Weon Hue) ; 임만배(Man-Bea Lim)</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-k822-e892ddb6a547911218809a3919b6973ec5b07a6f43d40afc207640bb1af5379f3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>kor</language><creationdate>1992</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>이상록(Sang-Rok Lee)</creatorcontrib><creatorcontrib>이학주(Hak-Joo Lee)</creatorcontrib><creatorcontrib>오세욱(Sae-Wook Oh)</creatorcontrib><creatorcontrib>허정원(Chung-Weon Hue)</creatorcontrib><creatorcontrib>임만배(Man-Bea Lim)</creatorcontrib><collection>DBPIA - 디비피아</collection><collection>DBPIA</collection><collection>KoreaScience</collection><jtitle>Han-guk haeyang gonghak hoeji (Online)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>이상록(Sang-Rok Lee)</au><au>이학주(Hak-Joo Lee)</au><au>오세욱(Sae-Wook Oh)</au><au>허정원(Chung-Weon Hue)</au><au>임만배(Man-Bea Lim)</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구</atitle><jtitle>Han-guk haeyang gonghak hoeji (Online)</jtitle><addtitle>Journal of ocean engineering and technology</addtitle><date>1992</date><risdate>1992</risdate><volume>6</volume><issue>1</issue><spage>122</spage><epage>130</epage><pages>122-130</pages><issn>1225-0767</issn><eissn>2287-6715</eissn><abstract>The effect of loading waveform on elevated temperature low-cycle fatigue crack growth behavior in a SUS 304 stainless steel have been investigated under symmetrical trangular (fast-fast), trapezoidal and asymmetrical(fast-slow, slow-fast) waveforms at 650.deg. C. It was found that the crack growth rate in fast-slow loading waveform appeared to be higher a little and the crack growth rate in slow-fast loading waveform much higer than that in fast-fast loading waveform, and difference in crack growth rate between fast-show and slow-fast waveforms nearly didn't appear in the region of da/dN&gt;10/sup -2/ The crack growth rate in the trapezoidal loading waveform with t/sub h/=500sec appeared to be faster than that in slow(500sec)-fast(1sec). In addition, parameter modified J-integral could be considered as useful parameter for fatigue crack growth rate in all waveforms. The result obtained are as follow. da/dN=4.91*10/sup -3/ (.DELTA. J/sub c/)/sup 0.565/.</abstract><pub>한국해양공학회</pub><tpages>9</tpages><oa>free_for_read</oa></addata></record>
fulltext fulltext
identifier ISSN: 1225-0767
ispartof Han-guk haeyang gonghak hoeji (Online), 1992, Vol.6 (1), p.122-130
issn 1225-0767
2287-6715
language kor
recordid cdi_kisti_ndsl_JAKO199211920577694
source Alma/SFX Local Collection
title SUS 304강의 하중파형에 따른 고온피로균열전파속도 및 전체하중파형의 평가방법의 연구
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-16T09%3A09%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-nurimedia_kisti&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=SUS%20304%EA%B0%95%EC%9D%98%20%ED%95%98%EC%A4%91%ED%8C%8C%ED%98%95%EC%97%90%20%EB%94%B0%EB%A5%B8%20%EA%B3%A0%EC%98%A8%ED%94%BC%EB%A1%9C%EA%B7%A0%EC%97%B4%EC%A0%84%ED%8C%8C%EC%86%8D%EB%8F%84%20%EB%B0%8F%20%EC%A0%84%EC%B2%B4%ED%95%98%EC%A4%91%ED%8C%8C%ED%98%95%EC%9D%98%20%ED%8F%89%EA%B0%80%EB%B0%A9%EB%B2%95%EC%9D%98%20%EC%97%B0%EA%B5%AC&rft.jtitle=Han-guk%20haeyang%20gonghak%20hoeji%20(Online)&rft.au=%EC%9D%B4%EC%83%81%EB%A1%9D(Sang-Rok%20Lee)&rft.date=1992&rft.volume=6&rft.issue=1&rft.spage=122&rft.epage=130&rft.pages=122-130&rft.issn=1225-0767&rft.eissn=2287-6715&rft_id=info:doi/&rft_dat=%3Cnurimedia_kisti%3ENODE00706222%3C/nurimedia_kisti%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rft_nurid=NODE00706222&rfr_iscdi=true