Dielectric Properties of Fine Grains Barium Titanate Ceramics Prepared by Mechanochemical Synthesis

Barium titanate was prepared by the advanced procedure of mechanochemical synthesis from barium and titanium oxides after 50 hours of milling. The X-ray examination of the milled powders showed the phase evolution during synthesis and the perovskite phase was initiated after 5 hours and was complete...