Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions
Gespeichert in:
Veröffentlicht in: | International journal of greenhouse gas control 2016-04, Vol.47, p.25-37 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 37 |
---|---|
container_issue | |
container_start_page | 25 |
container_title | International journal of greenhouse gas control |
container_volume | 47 |
creator | Brunet, Jean-Patrick Leopold Li, Li Karpyn, Zuleima T. Huerta, Nicolas J. |
description | |
doi_str_mv | 10.1016/j.ijggc.2016.01.024 |
format | Article |
fullrecord | <record><control><sourceid>hal_cross</sourceid><recordid>TN_cdi_hal_primary_oai_HAL_hal_02302507v1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>oai_HAL_hal_02302507v1</sourcerecordid><originalsourceid>FETCH-LOGICAL-c431t-cc5a87f9fcf9f0db21c8f25b18d531c61607d04fc6aed8d886d70c75bc6fbfdd3</originalsourceid><addsrcrecordid>eNo9ULtOAzEQdAESIfAFNG4p7ljfw2fooogQpEhpoLZ89jr4dI_IvoDS8Q_8IV-CjyCK3dXszsxKQ8gNg5QB43dN6prdTqdZBCmwFLLijMxYVUJSipxfkMsQGgDOWCFm5GPllR4PHumwx971Ozp4GrC1SUDVRvxAl96NTquWegzOYK-Rjq5DqgJV9NA7e5xke-VVhyN6aqODxg778fvza7nNYq-965G6Pp7jNzf04YqcW9UGvP6bc_K6enxZrpPN9ul5udgkusjZmGhdKlHZe6tjgakzpoXNypoJU-ZMc8ahMlBYzRUaYYTgpgJdlbXmtrbG5HNye_J9U63ce9cpf5SDcnK92MhpB1kOWQnVO4vc_MTVfgjBo_0XMJBTtrKRv9nKKVsJLIqL_AehwHUp</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Brunet, Jean-Patrick Leopold ; Li, Li ; Karpyn, Zuleima T. ; Huerta, Nicolas J.</creator><creatorcontrib>Brunet, Jean-Patrick Leopold ; Li, Li ; Karpyn, Zuleima T. ; Huerta, Nicolas J.</creatorcontrib><identifier>ISSN: 1750-5836</identifier><identifier>DOI: 10.1016/j.ijggc.2016.01.024</identifier><language>eng</language><publisher>Elsevier</publisher><subject>Engineering Sciences ; Fluids mechanics ; Mechanics ; Reactive fluid environment</subject><ispartof>International journal of greenhouse gas control, 2016-04, Vol.47, p.25-37</ispartof><rights>Distributed under a Creative Commons Attribution 4.0 International License</rights><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c431t-cc5a87f9fcf9f0db21c8f25b18d531c61607d04fc6aed8d886d70c75bc6fbfdd3</citedby><cites>FETCH-LOGICAL-c431t-cc5a87f9fcf9f0db21c8f25b18d531c61607d04fc6aed8d886d70c75bc6fbfdd3</cites><orcidid>0000-0001-8995-967X ; 0000-0002-7163-6263</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,315,781,785,886,27928,27929</link.rule.ids><backlink>$$Uhttps://hal.science/hal-02302507$$DView record in HAL$$Hfree_for_read</backlink></links><search><creatorcontrib>Brunet, Jean-Patrick Leopold</creatorcontrib><creatorcontrib>Li, Li</creatorcontrib><creatorcontrib>Karpyn, Zuleima T.</creatorcontrib><creatorcontrib>Huerta, Nicolas J.</creatorcontrib><title>Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions</title><title>International journal of greenhouse gas control</title><subject>Engineering Sciences</subject><subject>Fluids mechanics</subject><subject>Mechanics</subject><subject>Reactive fluid environment</subject><issn>1750-5836</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2016</creationdate><recordtype>article</recordtype><recordid>eNo9ULtOAzEQdAESIfAFNG4p7ljfw2fooogQpEhpoLZ89jr4dI_IvoDS8Q_8IV-CjyCK3dXszsxKQ8gNg5QB43dN6prdTqdZBCmwFLLijMxYVUJSipxfkMsQGgDOWCFm5GPllR4PHumwx971Ozp4GrC1SUDVRvxAl96NTquWegzOYK-Rjq5DqgJV9NA7e5xke-VVhyN6aqODxg778fvza7nNYq-965G6Pp7jNzf04YqcW9UGvP6bc_K6enxZrpPN9ul5udgkusjZmGhdKlHZe6tjgakzpoXNypoJU-ZMc8ahMlBYzRUaYYTgpgJdlbXmtrbG5HNye_J9U63ce9cpf5SDcnK92MhpB1kOWQnVO4vc_MTVfgjBo_0XMJBTtrKRv9nKKVsJLIqL_AehwHUp</recordid><startdate>20160401</startdate><enddate>20160401</enddate><creator>Brunet, Jean-Patrick Leopold</creator><creator>Li, Li</creator><creator>Karpyn, Zuleima T.</creator><creator>Huerta, Nicolas J.</creator><general>Elsevier</general><scope>AAYXX</scope><scope>CITATION</scope><scope>1XC</scope><orcidid>https://orcid.org/0000-0001-8995-967X</orcidid><orcidid>https://orcid.org/0000-0002-7163-6263</orcidid></search><sort><creationdate>20160401</creationdate><title>Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions</title><author>Brunet, Jean-Patrick Leopold ; Li, Li ; Karpyn, Zuleima T. ; Huerta, Nicolas J.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c431t-cc5a87f9fcf9f0db21c8f25b18d531c61607d04fc6aed8d886d70c75bc6fbfdd3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2016</creationdate><topic>Engineering Sciences</topic><topic>Fluids mechanics</topic><topic>Mechanics</topic><topic>Reactive fluid environment</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Brunet, Jean-Patrick Leopold</creatorcontrib><creatorcontrib>Li, Li</creatorcontrib><creatorcontrib>Karpyn, Zuleima T.</creatorcontrib><creatorcontrib>Huerta, Nicolas J.</creatorcontrib><collection>CrossRef</collection><collection>Hyper Article en Ligne (HAL)</collection><jtitle>International journal of greenhouse gas control</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Brunet, Jean-Patrick Leopold</au><au>Li, Li</au><au>Karpyn, Zuleima T.</au><au>Huerta, Nicolas J.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions</atitle><jtitle>International journal of greenhouse gas control</jtitle><date>2016-04-01</date><risdate>2016</risdate><volume>47</volume><spage>25</spage><epage>37</epage><pages>25-37</pages><issn>1750-5836</issn><pub>Elsevier</pub><doi>10.1016/j.ijggc.2016.01.024</doi><tpages>13</tpages><orcidid>https://orcid.org/0000-0001-8995-967X</orcidid><orcidid>https://orcid.org/0000-0002-7163-6263</orcidid><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1750-5836 |
ispartof | International journal of greenhouse gas control, 2016-04, Vol.47, p.25-37 |
issn | 1750-5836 |
language | eng |
recordid | cdi_hal_primary_oai_HAL_hal_02302507v1 |
source | Elsevier ScienceDirect Journals Complete |
subjects | Engineering Sciences Fluids mechanics Mechanics Reactive fluid environment |
title | Fracture opening or self-sealing: Critical residence time as a unifying parameter for cement–CO2–brine interactions |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T07%3A36%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-hal_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Fracture%20opening%20or%20self-sealing:%20Critical%20residence%20time%20as%20a%20unifying%20parameter%20for%20cement%E2%80%93CO2%E2%80%93brine%20interactions&rft.jtitle=International%20journal%20of%20greenhouse%20gas%20control&rft.au=Brunet,%20Jean-Patrick%20Leopold&rft.date=2016-04-01&rft.volume=47&rft.spage=25&rft.epage=37&rft.pages=25-37&rft.issn=1750-5836&rft_id=info:doi/10.1016/j.ijggc.2016.01.024&rft_dat=%3Chal_cross%3Eoai_HAL_hal_02302507v1%3C/hal_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |