Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation

•Response of the catalyst depends on type of noble metal used.•Pd/Al2O3 shows the highest resistance to crude glycerol impurities.•Selectivity of silver supported catalyst alters in crude glycerol.•Organic sulphur and fatty acid derivatives are the most problematic contaminants. The activity of four...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied catalysis. A, General General, 2015-06, Vol.499, p.89-100
Hauptverfasser: Skrzyńska, Elżbieta, Zaid, Soraya, Girardon, Jean-Sébastien, Capron, Mickaël, Dumeignil, Franck
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 100
container_issue
container_start_page 89
container_title Applied catalysis. A, General
container_volume 499
creator Skrzyńska, Elżbieta
Zaid, Soraya
Girardon, Jean-Sébastien
Capron, Mickaël
Dumeignil, Franck
description •Response of the catalyst depends on type of noble metal used.•Pd/Al2O3 shows the highest resistance to crude glycerol impurities.•Selectivity of silver supported catalyst alters in crude glycerol.•Organic sulphur and fatty acid derivatives are the most problematic contaminants. The activity of four different noble metals (Ag, Au, Pd and Pt) in the liquid phase oxidation of pure glycerol was confronted with the results obtained with a crude glycerol fraction, received from a large-scale biodiesel production plant. The catalysts were characterized by numerous techniques, giving insight into actual metal loading (elemental analysis by ICP and XRF), surface morphology (nitrogen absorption methods—BET and porosity), chemical state of both the support and the metal (XRD and XPS), and, finally, the metal particle size distribution (TEM microscopy). A good dispersion of totally reduced noble metal particles of a nanometric size (an average metal diameters were equal 3.5nm, 4.2nm, 4.7nm and 21.2nm for respectively Pd, Pt, Au and Ag) was accompanied with a comparable values of total metal loadings on the alumina support (from 0.95 and 0.96wt.% for Pt and Pd, up to 0.98 and 1.13wt.% for Au and Ag supported catalysts, respectively). In terms of initial reaction rate, the most active sample was the Au/Al2O3 catalyst, both using pure (12976molh−1molAu−1) or crude glycerol (1230molh−1molAu−1). However, comparison of the selectivities and conversions after 1–2h shows that the most robust and resistant catalyst – toward the impurities present in crude glycerol – is Pd/Al2O3, with a loss of conversion less than 50% (in respect to analogous reaction using pure glycerol) and almost unchanged high selectivity to glyceric acid (close to 80–90%). Ag/Al2O3 also showed a relatively high resistance to impurities in terms of glycerol conversion, but with a drastic modification of its selectivity. The activity of the two other catalysts was dramatically affected with a conversion divided by ca. 4 and even 10 for the Pt and the Au catalysts, respectively, when using crude glycerol instead of pure glycerol. Finally, the effect of each main impurity (MONG-NM, i.e., matter organic non-glycerol and non-methanol; ash; methanol; sulphur compounds) was independently studied. In any case, the sulphur compounds and MONG-NM were the impurities the most detrimental for the performances of catalysts. Thus, they should be removed in priority from crude glycerol fractions before reaction, while as
doi_str_mv 10.1016/j.apcata.2015.04.008
format Article
fullrecord <record><control><sourceid>proquest_hal_p</sourceid><recordid>TN_cdi_hal_primary_oai_HAL_hal_01772465v1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0926860X15002410</els_id><sourcerecordid>1730095895</sourcerecordid><originalsourceid>FETCH-LOGICAL-c410t-a5da8ac468ac7372bca8a0371a7216c7b0ef96f7a1021b069ea7c805bfee13853</originalsourceid><addsrcrecordid>eNp9kE9r3DAQxUVoINsk3yAHHduD3ZH_Sb4UwtImhYVcWsghIGR5lNXitVxJXrLfvjIuOeYyjxne-8E8Qu4Y5AxY8-2Qq0mrqPICWJ1DlQOIC7JhgpdZKXj9iWygLZpMNPB8RT6HcACAomrrDXnZptxwjlbTDvfqZN3sqTPULNpbY9DjGGmYp8n5iD0dXTcgPWJKBWpHGvdItZ97pK_DWaN3A3VvtlfRuvGGXJpkw9v_ek3-_Pzxe_uY7Z4efm3vd5muGMRM1b0SSldNGrzkRafTCiVnihes0bwDNG1juGJQsA6aFhXXAurOILJS1OU1-bpy92qQk7dH5c_SKSsf73dyuQHjvKia-sSS98vqnbz7O2OI8miDxmFQI7o5SMZLgLYW7YKtVqv2LgSP5p3NQC7Fy4Nci5dL8RIqmYpPse9rDNPLJ4teBm1x1NhbjzrK3tmPAf8AyXOOoA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1730095895</pqid></control><display><type>article</type><title>Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation</title><source>Elsevier ScienceDirect Journals Complete</source><creator>Skrzyńska, Elżbieta ; Zaid, Soraya ; Girardon, Jean-Sébastien ; Capron, Mickaël ; Dumeignil, Franck</creator><creatorcontrib>Skrzyńska, Elżbieta ; Zaid, Soraya ; Girardon, Jean-Sébastien ; Capron, Mickaël ; Dumeignil, Franck</creatorcontrib><description>•Response of the catalyst depends on type of noble metal used.•Pd/Al2O3 shows the highest resistance to crude glycerol impurities.•Selectivity of silver supported catalyst alters in crude glycerol.•Organic sulphur and fatty acid derivatives are the most problematic contaminants. The activity of four different noble metals (Ag, Au, Pd and Pt) in the liquid phase oxidation of pure glycerol was confronted with the results obtained with a crude glycerol fraction, received from a large-scale biodiesel production plant. The catalysts were characterized by numerous techniques, giving insight into actual metal loading (elemental analysis by ICP and XRF), surface morphology (nitrogen absorption methods—BET and porosity), chemical state of both the support and the metal (XRD and XPS), and, finally, the metal particle size distribution (TEM microscopy). A good dispersion of totally reduced noble metal particles of a nanometric size (an average metal diameters were equal 3.5nm, 4.2nm, 4.7nm and 21.2nm for respectively Pd, Pt, Au and Ag) was accompanied with a comparable values of total metal loadings on the alumina support (from 0.95 and 0.96wt.% for Pt and Pd, up to 0.98 and 1.13wt.% for Au and Ag supported catalysts, respectively). In terms of initial reaction rate, the most active sample was the Au/Al2O3 catalyst, both using pure (12976molh−1molAu−1) or crude glycerol (1230molh−1molAu−1). However, comparison of the selectivities and conversions after 1–2h shows that the most robust and resistant catalyst – toward the impurities present in crude glycerol – is Pd/Al2O3, with a loss of conversion less than 50% (in respect to analogous reaction using pure glycerol) and almost unchanged high selectivity to glyceric acid (close to 80–90%). Ag/Al2O3 also showed a relatively high resistance to impurities in terms of glycerol conversion, but with a drastic modification of its selectivity. The activity of the two other catalysts was dramatically affected with a conversion divided by ca. 4 and even 10 for the Pt and the Au catalysts, respectively, when using crude glycerol instead of pure glycerol. Finally, the effect of each main impurity (MONG-NM, i.e., matter organic non-glycerol and non-methanol; ash; methanol; sulphur compounds) was independently studied. In any case, the sulphur compounds and MONG-NM were the impurities the most detrimental for the performances of catalysts. Thus, they should be removed in priority from crude glycerol fractions before reaction, while ashes and methanol should not be considered as completely undesirable.</description><identifier>ISSN: 0926-860X</identifier><identifier>EISSN: 1873-3875</identifier><identifier>DOI: 10.1016/j.apcata.2015.04.008</identifier><language>eng</language><publisher>Elsevier B.V</publisher><subject>Ashes ; Catalysis ; Catalysts ; Chemical Sciences ; Crude glycerol oxidation ; Glycerols ; Gold ; Impurities ; Methyl alcohol ; Noble metals ; Palladium ; Platinum ; Silver ; Sulfur compounds ; Supported noble metal catalysts</subject><ispartof>Applied catalysis. A, General, 2015-06, Vol.499, p.89-100</ispartof><rights>2015 Elsevier B.V.</rights><rights>Distributed under a Creative Commons Attribution 4.0 International License</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c410t-a5da8ac468ac7372bca8a0371a7216c7b0ef96f7a1021b069ea7c805bfee13853</citedby><cites>FETCH-LOGICAL-c410t-a5da8ac468ac7372bca8a0371a7216c7b0ef96f7a1021b069ea7c805bfee13853</cites><orcidid>0000-0002-4941-4680 ; 0000-0001-9727-8196</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.apcata.2015.04.008$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>230,314,780,784,885,3550,27924,27925,45995</link.rule.ids><backlink>$$Uhttps://hal.science/hal-01772465$$DView record in HAL$$Hfree_for_read</backlink></links><search><creatorcontrib>Skrzyńska, Elżbieta</creatorcontrib><creatorcontrib>Zaid, Soraya</creatorcontrib><creatorcontrib>Girardon, Jean-Sébastien</creatorcontrib><creatorcontrib>Capron, Mickaël</creatorcontrib><creatorcontrib>Dumeignil, Franck</creatorcontrib><title>Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation</title><title>Applied catalysis. A, General</title><description>•Response of the catalyst depends on type of noble metal used.•Pd/Al2O3 shows the highest resistance to crude glycerol impurities.•Selectivity of silver supported catalyst alters in crude glycerol.•Organic sulphur and fatty acid derivatives are the most problematic contaminants. The activity of four different noble metals (Ag, Au, Pd and Pt) in the liquid phase oxidation of pure glycerol was confronted with the results obtained with a crude glycerol fraction, received from a large-scale biodiesel production plant. The catalysts were characterized by numerous techniques, giving insight into actual metal loading (elemental analysis by ICP and XRF), surface morphology (nitrogen absorption methods—BET and porosity), chemical state of both the support and the metal (XRD and XPS), and, finally, the metal particle size distribution (TEM microscopy). A good dispersion of totally reduced noble metal particles of a nanometric size (an average metal diameters were equal 3.5nm, 4.2nm, 4.7nm and 21.2nm for respectively Pd, Pt, Au and Ag) was accompanied with a comparable values of total metal loadings on the alumina support (from 0.95 and 0.96wt.% for Pt and Pd, up to 0.98 and 1.13wt.% for Au and Ag supported catalysts, respectively). In terms of initial reaction rate, the most active sample was the Au/Al2O3 catalyst, both using pure (12976molh−1molAu−1) or crude glycerol (1230molh−1molAu−1). However, comparison of the selectivities and conversions after 1–2h shows that the most robust and resistant catalyst – toward the impurities present in crude glycerol – is Pd/Al2O3, with a loss of conversion less than 50% (in respect to analogous reaction using pure glycerol) and almost unchanged high selectivity to glyceric acid (close to 80–90%). Ag/Al2O3 also showed a relatively high resistance to impurities in terms of glycerol conversion, but with a drastic modification of its selectivity. The activity of the two other catalysts was dramatically affected with a conversion divided by ca. 4 and even 10 for the Pt and the Au catalysts, respectively, when using crude glycerol instead of pure glycerol. Finally, the effect of each main impurity (MONG-NM, i.e., matter organic non-glycerol and non-methanol; ash; methanol; sulphur compounds) was independently studied. In any case, the sulphur compounds and MONG-NM were the impurities the most detrimental for the performances of catalysts. Thus, they should be removed in priority from crude glycerol fractions before reaction, while ashes and methanol should not be considered as completely undesirable.</description><subject>Ashes</subject><subject>Catalysis</subject><subject>Catalysts</subject><subject>Chemical Sciences</subject><subject>Crude glycerol oxidation</subject><subject>Glycerols</subject><subject>Gold</subject><subject>Impurities</subject><subject>Methyl alcohol</subject><subject>Noble metals</subject><subject>Palladium</subject><subject>Platinum</subject><subject>Silver</subject><subject>Sulfur compounds</subject><subject>Supported noble metal catalysts</subject><issn>0926-860X</issn><issn>1873-3875</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2015</creationdate><recordtype>article</recordtype><recordid>eNp9kE9r3DAQxUVoINsk3yAHHduD3ZH_Sb4UwtImhYVcWsghIGR5lNXitVxJXrLfvjIuOeYyjxne-8E8Qu4Y5AxY8-2Qq0mrqPICWJ1DlQOIC7JhgpdZKXj9iWygLZpMNPB8RT6HcACAomrrDXnZptxwjlbTDvfqZN3sqTPULNpbY9DjGGmYp8n5iD0dXTcgPWJKBWpHGvdItZ97pK_DWaN3A3VvtlfRuvGGXJpkw9v_ek3-_Pzxe_uY7Z4efm3vd5muGMRM1b0SSldNGrzkRafTCiVnihes0bwDNG1juGJQsA6aFhXXAurOILJS1OU1-bpy92qQk7dH5c_SKSsf73dyuQHjvKia-sSS98vqnbz7O2OI8miDxmFQI7o5SMZLgLYW7YKtVqv2LgSP5p3NQC7Fy4Nci5dL8RIqmYpPse9rDNPLJ4teBm1x1NhbjzrK3tmPAf8AyXOOoA</recordid><startdate>20150625</startdate><enddate>20150625</enddate><creator>Skrzyńska, Elżbieta</creator><creator>Zaid, Soraya</creator><creator>Girardon, Jean-Sébastien</creator><creator>Capron, Mickaël</creator><creator>Dumeignil, Franck</creator><general>Elsevier B.V</general><general>Elsevier</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SR</scope><scope>7U5</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope><scope>L7M</scope><scope>1XC</scope><orcidid>https://orcid.org/0000-0002-4941-4680</orcidid><orcidid>https://orcid.org/0000-0001-9727-8196</orcidid></search><sort><creationdate>20150625</creationdate><title>Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation</title><author>Skrzyńska, Elżbieta ; Zaid, Soraya ; Girardon, Jean-Sébastien ; Capron, Mickaël ; Dumeignil, Franck</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c410t-a5da8ac468ac7372bca8a0371a7216c7b0ef96f7a1021b069ea7c805bfee13853</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2015</creationdate><topic>Ashes</topic><topic>Catalysis</topic><topic>Catalysts</topic><topic>Chemical Sciences</topic><topic>Crude glycerol oxidation</topic><topic>Glycerols</topic><topic>Gold</topic><topic>Impurities</topic><topic>Methyl alcohol</topic><topic>Noble metals</topic><topic>Palladium</topic><topic>Platinum</topic><topic>Silver</topic><topic>Sulfur compounds</topic><topic>Supported noble metal catalysts</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Skrzyńska, Elżbieta</creatorcontrib><creatorcontrib>Zaid, Soraya</creatorcontrib><creatorcontrib>Girardon, Jean-Sébastien</creatorcontrib><creatorcontrib>Capron, Mickaël</creatorcontrib><creatorcontrib>Dumeignil, Franck</creatorcontrib><collection>CrossRef</collection><collection>Engineered Materials Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><collection>Hyper Article en Ligne (HAL)</collection><jtitle>Applied catalysis. A, General</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Skrzyńska, Elżbieta</au><au>Zaid, Soraya</au><au>Girardon, Jean-Sébastien</au><au>Capron, Mickaël</au><au>Dumeignil, Franck</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation</atitle><jtitle>Applied catalysis. A, General</jtitle><date>2015-06-25</date><risdate>2015</risdate><volume>499</volume><spage>89</spage><epage>100</epage><pages>89-100</pages><issn>0926-860X</issn><eissn>1873-3875</eissn><abstract>•Response of the catalyst depends on type of noble metal used.•Pd/Al2O3 shows the highest resistance to crude glycerol impurities.•Selectivity of silver supported catalyst alters in crude glycerol.•Organic sulphur and fatty acid derivatives are the most problematic contaminants. The activity of four different noble metals (Ag, Au, Pd and Pt) in the liquid phase oxidation of pure glycerol was confronted with the results obtained with a crude glycerol fraction, received from a large-scale biodiesel production plant. The catalysts were characterized by numerous techniques, giving insight into actual metal loading (elemental analysis by ICP and XRF), surface morphology (nitrogen absorption methods—BET and porosity), chemical state of both the support and the metal (XRD and XPS), and, finally, the metal particle size distribution (TEM microscopy). A good dispersion of totally reduced noble metal particles of a nanometric size (an average metal diameters were equal 3.5nm, 4.2nm, 4.7nm and 21.2nm for respectively Pd, Pt, Au and Ag) was accompanied with a comparable values of total metal loadings on the alumina support (from 0.95 and 0.96wt.% for Pt and Pd, up to 0.98 and 1.13wt.% for Au and Ag supported catalysts, respectively). In terms of initial reaction rate, the most active sample was the Au/Al2O3 catalyst, both using pure (12976molh−1molAu−1) or crude glycerol (1230molh−1molAu−1). However, comparison of the selectivities and conversions after 1–2h shows that the most robust and resistant catalyst – toward the impurities present in crude glycerol – is Pd/Al2O3, with a loss of conversion less than 50% (in respect to analogous reaction using pure glycerol) and almost unchanged high selectivity to glyceric acid (close to 80–90%). Ag/Al2O3 also showed a relatively high resistance to impurities in terms of glycerol conversion, but with a drastic modification of its selectivity. The activity of the two other catalysts was dramatically affected with a conversion divided by ca. 4 and even 10 for the Pt and the Au catalysts, respectively, when using crude glycerol instead of pure glycerol. Finally, the effect of each main impurity (MONG-NM, i.e., matter organic non-glycerol and non-methanol; ash; methanol; sulphur compounds) was independently studied. In any case, the sulphur compounds and MONG-NM were the impurities the most detrimental for the performances of catalysts. Thus, they should be removed in priority from crude glycerol fractions before reaction, while ashes and methanol should not be considered as completely undesirable.</abstract><pub>Elsevier B.V</pub><doi>10.1016/j.apcata.2015.04.008</doi><tpages>12</tpages><orcidid>https://orcid.org/0000-0002-4941-4680</orcidid><orcidid>https://orcid.org/0000-0001-9727-8196</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0926-860X
ispartof Applied catalysis. A, General, 2015-06, Vol.499, p.89-100
issn 0926-860X
1873-3875
language eng
recordid cdi_hal_primary_oai_HAL_hal_01772465v1
source Elsevier ScienceDirect Journals Complete
subjects Ashes
Catalysis
Catalysts
Chemical Sciences
Crude glycerol oxidation
Glycerols
Gold
Impurities
Methyl alcohol
Noble metals
Palladium
Platinum
Silver
Sulfur compounds
Supported noble metal catalysts
title Catalytic behaviour of four different supported noble metals in the crude glycerol oxidation
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T07%3A17%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_hal_p&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Catalytic%20behaviour%20of%20four%20different%20supported%20noble%20metals%20in%20the%20crude%20glycerol%20oxidation&rft.jtitle=Applied%20catalysis.%20A,%20General&rft.au=Skrzy%C5%84ska,%20El%C5%BCbieta&rft.date=2015-06-25&rft.volume=499&rft.spage=89&rft.epage=100&rft.pages=89-100&rft.issn=0926-860X&rft.eissn=1873-3875&rft_id=info:doi/10.1016/j.apcata.2015.04.008&rft_dat=%3Cproquest_hal_p%3E1730095895%3C/proquest_hal_p%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1730095895&rft_id=info:pmid/&rft_els_id=S0926860X15002410&rfr_iscdi=true