Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature
Inconel 718 flat rough surfaces were tested under fretting conditions at room and high temperature (600°C). Analysis were focused on friction coefficient, damage and fretting regime. Several coatings were tested, and showed significant differences depending on the test temperature. The bonded coatin...
Gespeichert in:
Veröffentlicht in: | Tribology international 2016-08, Vol.100, p.430-440 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 440 |
---|---|
container_issue | |
container_start_page | 430 |
container_title | Tribology international |
container_volume | 100 |
creator | Fortes Da Cruz, J. Da Silva Botelho, T. Lemaire-Caron, I. Durand, A-M. Messager, D. |
description | Inconel 718 flat rough surfaces were tested under fretting conditions at room and high temperature (600°C). Analysis were focused on friction coefficient, damage and fretting regime. Several coatings were tested, and showed significant differences depending on the test temperature. The bonded coating offers good protection against fretting wear at ambient temperature but loses its properties at 600°C where the CrC shows excellent durability and lower friction thanks to the formation of a few micrometers thin glaze layer. WS2 solid lubricant layers also show a similar protective behaviour at high temperature but under lighter normal loads and for a lower lifespan.
•We studied combined ambient and high temperature fretting response.•High roughness flat Inconel 718 surfaces were involved.•WS2 and CrC showed low friction and improved durability at 600°C.•CrC forms protective glaze layer at high temperature.•Temperature dependent friction and damage behavior is reversible. |
doi_str_mv | 10.1016/j.triboint.2016.05.037 |
format | Article |
fullrecord | <record><control><sourceid>elsevier_hal_p</sourceid><recordid>TN_cdi_hal_primary_oai_HAL_hal_01426088v1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><els_id>S0301679X16301293</els_id><sourcerecordid>S0301679X16301293</sourcerecordid><originalsourceid>FETCH-LOGICAL-c346t-4d410c09790eb225ad3e2dd13aae49e724011943988101d8c5b4650e7e38a4bf3</originalsourceid><addsrcrecordid>eNqFkNFr2zAQxsVoYWm7f2HotWx2T7Zs2W8LYW0CgcHasr0JWTonCo4VJCXQ_35y0-61L3fcd_d9cD9CvjLIGbD6bpdHbztnx5gXac6hyqEUn8iMNaLNCl7zCzKDElhWi_bvZ3IVwg4ABG_FjJx-uwGp6-mfx-L7VL4t_IKq0dDOjQYN1U5FO24CdSM1aq82-LrtvdXRJi1ZV6N2Iw5UsIb2g4rUu-NmS8PR90pjoEnZ2iRE3B_Qq3j0eEMuezUE_PLWr8nz_c-nxTJb_3pYLebrTJe8jhk3nIGGVrSAXVFUypRYGMNKpZC3KAoOjLW8bJsmoTCNrjpeV4ACy0bxri-vye05d6sGefB2r_yLdMrK5XwtJw0YL2pomhNLt_X5VnsXgsf-v4GBnEjLnXwnLSfSEiqZSCfjj7MR0ycni14GbXHUaKxHHaVx9qOIfxOgiT0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature</title><source>Elsevier ScienceDirect Journals</source><creator>Fortes Da Cruz, J. ; Da Silva Botelho, T. ; Lemaire-Caron, I. ; Durand, A-M. ; Messager, D.</creator><creatorcontrib>Fortes Da Cruz, J. ; Da Silva Botelho, T. ; Lemaire-Caron, I. ; Durand, A-M. ; Messager, D.</creatorcontrib><description>Inconel 718 flat rough surfaces were tested under fretting conditions at room and high temperature (600°C). Analysis were focused on friction coefficient, damage and fretting regime. Several coatings were tested, and showed significant differences depending on the test temperature. The bonded coating offers good protection against fretting wear at ambient temperature but loses its properties at 600°C where the CrC shows excellent durability and lower friction thanks to the formation of a few micrometers thin glaze layer. WS2 solid lubricant layers also show a similar protective behaviour at high temperature but under lighter normal loads and for a lower lifespan.
•We studied combined ambient and high temperature fretting response.•High roughness flat Inconel 718 surfaces were involved.•WS2 and CrC showed low friction and improved durability at 600°C.•CrC forms protective glaze layer at high temperature.•Temperature dependent friction and damage behavior is reversible.</description><identifier>ISSN: 0301-679X</identifier><identifier>EISSN: 1879-2464</identifier><identifier>DOI: 10.1016/j.triboint.2016.05.037</identifier><language>eng</language><publisher>Elsevier Ltd</publisher><subject>Engineering Sciences ; Fretting ; Glaze layers ; High temperature ; Mechanics ; Mechanics of materials ; Surface coatings</subject><ispartof>Tribology international, 2016-08, Vol.100, p.430-440</ispartof><rights>2016 Elsevier Ltd</rights><rights>Distributed under a Creative Commons Attribution 4.0 International License</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c346t-4d410c09790eb225ad3e2dd13aae49e724011943988101d8c5b4650e7e38a4bf3</citedby><cites>FETCH-LOGICAL-c346t-4d410c09790eb225ad3e2dd13aae49e724011943988101d8c5b4650e7e38a4bf3</cites><orcidid>0000-0002-6360-7868 ; 0000-0002-0218-4654 ; 0000-0001-5183-0715</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://dx.doi.org/10.1016/j.triboint.2016.05.037$$EHTML$$P50$$Gelsevier$$H</linktohtml><link.rule.ids>230,314,777,781,882,3537,27905,27906,45976</link.rule.ids><backlink>$$Uhttps://hal.science/hal-01426088$$DView record in HAL$$Hfree_for_read</backlink></links><search><creatorcontrib>Fortes Da Cruz, J.</creatorcontrib><creatorcontrib>Da Silva Botelho, T.</creatorcontrib><creatorcontrib>Lemaire-Caron, I.</creatorcontrib><creatorcontrib>Durand, A-M.</creatorcontrib><creatorcontrib>Messager, D.</creatorcontrib><title>Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature</title><title>Tribology international</title><description>Inconel 718 flat rough surfaces were tested under fretting conditions at room and high temperature (600°C). Analysis were focused on friction coefficient, damage and fretting regime. Several coatings were tested, and showed significant differences depending on the test temperature. The bonded coating offers good protection against fretting wear at ambient temperature but loses its properties at 600°C where the CrC shows excellent durability and lower friction thanks to the formation of a few micrometers thin glaze layer. WS2 solid lubricant layers also show a similar protective behaviour at high temperature but under lighter normal loads and for a lower lifespan.
•We studied combined ambient and high temperature fretting response.•High roughness flat Inconel 718 surfaces were involved.•WS2 and CrC showed low friction and improved durability at 600°C.•CrC forms protective glaze layer at high temperature.•Temperature dependent friction and damage behavior is reversible.</description><subject>Engineering Sciences</subject><subject>Fretting</subject><subject>Glaze layers</subject><subject>High temperature</subject><subject>Mechanics</subject><subject>Mechanics of materials</subject><subject>Surface coatings</subject><issn>0301-679X</issn><issn>1879-2464</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2016</creationdate><recordtype>article</recordtype><recordid>eNqFkNFr2zAQxsVoYWm7f2HotWx2T7Zs2W8LYW0CgcHasr0JWTonCo4VJCXQ_35y0-61L3fcd_d9cD9CvjLIGbD6bpdHbztnx5gXac6hyqEUn8iMNaLNCl7zCzKDElhWi_bvZ3IVwg4ABG_FjJx-uwGp6-mfx-L7VL4t_IKq0dDOjQYN1U5FO24CdSM1aq82-LrtvdXRJi1ZV6N2Iw5UsIb2g4rUu-NmS8PR90pjoEnZ2iRE3B_Qq3j0eEMuezUE_PLWr8nz_c-nxTJb_3pYLebrTJe8jhk3nIGGVrSAXVFUypRYGMNKpZC3KAoOjLW8bJsmoTCNrjpeV4ACy0bxri-vye05d6sGefB2r_yLdMrK5XwtJw0YL2pomhNLt_X5VnsXgsf-v4GBnEjLnXwnLSfSEiqZSCfjj7MR0ycni14GbXHUaKxHHaVx9qOIfxOgiT0</recordid><startdate>20160801</startdate><enddate>20160801</enddate><creator>Fortes Da Cruz, J.</creator><creator>Da Silva Botelho, T.</creator><creator>Lemaire-Caron, I.</creator><creator>Durand, A-M.</creator><creator>Messager, D.</creator><general>Elsevier Ltd</general><general>Elsevier</general><scope>AAYXX</scope><scope>CITATION</scope><scope>1XC</scope><orcidid>https://orcid.org/0000-0002-6360-7868</orcidid><orcidid>https://orcid.org/0000-0002-0218-4654</orcidid><orcidid>https://orcid.org/0000-0001-5183-0715</orcidid></search><sort><creationdate>20160801</creationdate><title>Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature</title><author>Fortes Da Cruz, J. ; Da Silva Botelho, T. ; Lemaire-Caron, I. ; Durand, A-M. ; Messager, D.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c346t-4d410c09790eb225ad3e2dd13aae49e724011943988101d8c5b4650e7e38a4bf3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2016</creationdate><topic>Engineering Sciences</topic><topic>Fretting</topic><topic>Glaze layers</topic><topic>High temperature</topic><topic>Mechanics</topic><topic>Mechanics of materials</topic><topic>Surface coatings</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Fortes Da Cruz, J.</creatorcontrib><creatorcontrib>Da Silva Botelho, T.</creatorcontrib><creatorcontrib>Lemaire-Caron, I.</creatorcontrib><creatorcontrib>Durand, A-M.</creatorcontrib><creatorcontrib>Messager, D.</creatorcontrib><collection>CrossRef</collection><collection>Hyper Article en Ligne (HAL)</collection><jtitle>Tribology international</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Fortes Da Cruz, J.</au><au>Da Silva Botelho, T.</au><au>Lemaire-Caron, I.</au><au>Durand, A-M.</au><au>Messager, D.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature</atitle><jtitle>Tribology international</jtitle><date>2016-08-01</date><risdate>2016</risdate><volume>100</volume><spage>430</spage><epage>440</epage><pages>430-440</pages><issn>0301-679X</issn><eissn>1879-2464</eissn><abstract>Inconel 718 flat rough surfaces were tested under fretting conditions at room and high temperature (600°C). Analysis were focused on friction coefficient, damage and fretting regime. Several coatings were tested, and showed significant differences depending on the test temperature. The bonded coating offers good protection against fretting wear at ambient temperature but loses its properties at 600°C where the CrC shows excellent durability and lower friction thanks to the formation of a few micrometers thin glaze layer. WS2 solid lubricant layers also show a similar protective behaviour at high temperature but under lighter normal loads and for a lower lifespan.
•We studied combined ambient and high temperature fretting response.•High roughness flat Inconel 718 surfaces were involved.•WS2 and CrC showed low friction and improved durability at 600°C.•CrC forms protective glaze layer at high temperature.•Temperature dependent friction and damage behavior is reversible.</abstract><pub>Elsevier Ltd</pub><doi>10.1016/j.triboint.2016.05.037</doi><tpages>11</tpages><orcidid>https://orcid.org/0000-0002-6360-7868</orcidid><orcidid>https://orcid.org/0000-0002-0218-4654</orcidid><orcidid>https://orcid.org/0000-0001-5183-0715</orcidid></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0301-679X |
ispartof | Tribology international, 2016-08, Vol.100, p.430-440 |
issn | 0301-679X 1879-2464 |
language | eng |
recordid | cdi_hal_primary_oai_HAL_hal_01426088v1 |
source | Elsevier ScienceDirect Journals |
subjects | Engineering Sciences Fretting Glaze layers High temperature Mechanics Mechanics of materials Surface coatings |
title | Role of WS2, WS2+CrC and bonded coatings on damage and friction of Inconel 718 flat rough surfaces at high temperature |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T09%3A09%3A32IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-elsevier_hal_p&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Role%20of%20WS2,%20WS2+CrC%20and%20bonded%20coatings%20on%20damage%20and%20friction%20of%20Inconel%20718%20flat%20rough%20surfaces%20at%20high%20temperature&rft.jtitle=Tribology%20international&rft.au=Fortes%20Da%20Cruz,%20J.&rft.date=2016-08-01&rft.volume=100&rft.spage=430&rft.epage=440&rft.pages=430-440&rft.issn=0301-679X&rft.eissn=1879-2464&rft_id=info:doi/10.1016/j.triboint.2016.05.037&rft_dat=%3Celsevier_hal_p%3ES0301679X16301293%3C/elsevier_hal_p%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rft_els_id=S0301679X16301293&rfr_iscdi=true |