Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals

This study reports on experimental results on the morphology of laser-induced damage in the bulk of potassium dihydrogen phosphate (or KDP) crystals by nanosecond pulses. The resulting morphology of bulk laser damage is structured in four different zones whose characteristics depend on laser paramet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied physics. A, Materials science & processing Materials science & processing, 2015-06, Vol.119 (4), p.1317-1326
Hauptverfasser: Reyné, S., Duchateau, G., Hallo, L., Natoli, J. Y., Lamaignère, L.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 1326
container_issue 4
container_start_page 1317
container_title Applied physics. A, Materials science & processing
container_volume 119
creator Reyné, S.
Duchateau, G.
Hallo, L.
Natoli, J. Y.
Lamaignère, L.
description This study reports on experimental results on the morphology of laser-induced damage in the bulk of potassium dihydrogen phosphate (or KDP) crystals by nanosecond pulses. The resulting morphology of bulk laser damage is structured in four different zones whose characteristics depend on laser parameters such as wavelength, laser polarization, and fluence. To have a better understanding of bulk formation and structure of KDP laser damage, accessing the mechanical properties of KDP is a promising way which departs from a thermal approach which is mainly used in various models well documented in the literature. In that way, we have revisited various mechanical models of fracturation frequently used to evaluate the toughness of optical materials. Our experiments are compared to these models where the toughness is the criterion, which has been chosen to validate the modeling part of this study. We conclude that experiments are in agreement with the common values obtained by indentations tests proposed in the literature, allowing us further developments with one of these models to describe the damage formation in KDP crystals. Also, it appears that laser damage events split into two separated groups depending on the wavelength, with on one side 351-nm damage sites and on the other side 1064- and 532-nm damage sites. That suggests the existence of different physical mechanisms responsible for bulk damage initiation in KDP crystals with respect to the wavelength.
doi_str_mv 10.1007/s00339-015-9098-z
format Article
fullrecord <record><control><sourceid>proquest_hal_p</sourceid><recordid>TN_cdi_hal_primary_oai_HAL_hal_01275769v1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>1709735373</sourcerecordid><originalsourceid>FETCH-LOGICAL-c425t-b5670cd8728e07fd8ecffad76f227cb833876789cfcea048d4d0be572e5914733</originalsourceid><addsrcrecordid>eNp9kD1vFDEQhi0EEkfgB9C5hMJhbO-u7TIKH0E5BEVSUFk-e_Zug88-7N2gy6_PHhtRMs1Io-d9pHkJecvhnAOoDxVASsOAt8yA0ezhGVnxRgoGnYTnZAWmUUxL070kr2q9g3kaIVbk57cpjgP74-4xYtqOO1rHKRxp7mlyKVf0OQUaXcXChhQmj4FupviLBrd3W6T7XA67HPP2SIdErz_-oL4c6-hifU1e9PPCN0_7jNx-_nRzecXW3798vbxYM9-IdmSbtlPgg1ZCI6g-aPR974LqeiGU32gpteqUNr736KDRoQmwwVYJbA1vlJRn5P3i3bloD2XYu3K02Q326mJtTzfgQrWqM_d8Zt8t7KHk3xPW0e6H6jFGlzBP1XIFRslW_tXyBfUl11qw_-fmYE-V26XyWd_aU-X2Yc6IJVNnNm2x2Ls8lTR__5_QIx3KhM0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>1709735373</pqid></control><display><type>article</type><title>Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals</title><source>Springer Nature - Complete Springer Journals</source><creator>Reyné, S. ; Duchateau, G. ; Hallo, L. ; Natoli, J. Y. ; Lamaignère, L.</creator><creatorcontrib>Reyné, S. ; Duchateau, G. ; Hallo, L. ; Natoli, J. Y. ; Lamaignère, L.</creatorcontrib><description>This study reports on experimental results on the morphology of laser-induced damage in the bulk of potassium dihydrogen phosphate (or KDP) crystals by nanosecond pulses. The resulting morphology of bulk laser damage is structured in four different zones whose characteristics depend on laser parameters such as wavelength, laser polarization, and fluence. To have a better understanding of bulk formation and structure of KDP laser damage, accessing the mechanical properties of KDP is a promising way which departs from a thermal approach which is mainly used in various models well documented in the literature. In that way, we have revisited various mechanical models of fracturation frequently used to evaluate the toughness of optical materials. Our experiments are compared to these models where the toughness is the criterion, which has been chosen to validate the modeling part of this study. We conclude that experiments are in agreement with the common values obtained by indentations tests proposed in the literature, allowing us further developments with one of these models to describe the damage formation in KDP crystals. Also, it appears that laser damage events split into two separated groups depending on the wavelength, with on one side 351-nm damage sites and on the other side 1064- and 532-nm damage sites. That suggests the existence of different physical mechanisms responsible for bulk damage initiation in KDP crystals with respect to the wavelength.</description><identifier>ISSN: 0947-8396</identifier><identifier>EISSN: 1432-0630</identifier><identifier>DOI: 10.1007/s00339-015-9098-z</identifier><language>eng</language><publisher>Berlin/Heidelberg: Springer Berlin Heidelberg</publisher><subject>Characterization and Evaluation of Materials ; Condensed Matter Physics ; Damage ; Fracture toughness ; KDP crystals ; Laser damage ; Lasers ; Machines ; Manufacturing ; Mathematical models ; Morphology ; Nanotechnology ; Optical and Electronic Materials ; Optics ; Physics ; Physics and Astronomy ; Processes ; Surfaces and Interfaces ; Thin Films ; Wavelengths</subject><ispartof>Applied physics. A, Materials science &amp; processing, 2015-06, Vol.119 (4), p.1317-1326</ispartof><rights>Springer-Verlag Berlin Heidelberg 2015</rights><rights>Distributed under a Creative Commons Attribution 4.0 International License</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c425t-b5670cd8728e07fd8ecffad76f227cb833876789cfcea048d4d0be572e5914733</citedby><cites>FETCH-LOGICAL-c425t-b5670cd8728e07fd8ecffad76f227cb833876789cfcea048d4d0be572e5914733</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://link.springer.com/content/pdf/10.1007/s00339-015-9098-z$$EPDF$$P50$$Gspringer$$H</linktopdf><linktohtml>$$Uhttps://link.springer.com/10.1007/s00339-015-9098-z$$EHTML$$P50$$Gspringer$$H</linktohtml><link.rule.ids>230,314,776,780,881,27901,27902,41464,42533,51294</link.rule.ids><backlink>$$Uhttps://hal.science/hal-01275769$$DView record in HAL$$Hfree_for_read</backlink></links><search><creatorcontrib>Reyné, S.</creatorcontrib><creatorcontrib>Duchateau, G.</creatorcontrib><creatorcontrib>Hallo, L.</creatorcontrib><creatorcontrib>Natoli, J. Y.</creatorcontrib><creatorcontrib>Lamaignère, L.</creatorcontrib><title>Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals</title><title>Applied physics. A, Materials science &amp; processing</title><addtitle>Appl. Phys. A</addtitle><description>This study reports on experimental results on the morphology of laser-induced damage in the bulk of potassium dihydrogen phosphate (or KDP) crystals by nanosecond pulses. The resulting morphology of bulk laser damage is structured in four different zones whose characteristics depend on laser parameters such as wavelength, laser polarization, and fluence. To have a better understanding of bulk formation and structure of KDP laser damage, accessing the mechanical properties of KDP is a promising way which departs from a thermal approach which is mainly used in various models well documented in the literature. In that way, we have revisited various mechanical models of fracturation frequently used to evaluate the toughness of optical materials. Our experiments are compared to these models where the toughness is the criterion, which has been chosen to validate the modeling part of this study. We conclude that experiments are in agreement with the common values obtained by indentations tests proposed in the literature, allowing us further developments with one of these models to describe the damage formation in KDP crystals. Also, it appears that laser damage events split into two separated groups depending on the wavelength, with on one side 351-nm damage sites and on the other side 1064- and 532-nm damage sites. That suggests the existence of different physical mechanisms responsible for bulk damage initiation in KDP crystals with respect to the wavelength.</description><subject>Characterization and Evaluation of Materials</subject><subject>Condensed Matter Physics</subject><subject>Damage</subject><subject>Fracture toughness</subject><subject>KDP crystals</subject><subject>Laser damage</subject><subject>Lasers</subject><subject>Machines</subject><subject>Manufacturing</subject><subject>Mathematical models</subject><subject>Morphology</subject><subject>Nanotechnology</subject><subject>Optical and Electronic Materials</subject><subject>Optics</subject><subject>Physics</subject><subject>Physics and Astronomy</subject><subject>Processes</subject><subject>Surfaces and Interfaces</subject><subject>Thin Films</subject><subject>Wavelengths</subject><issn>0947-8396</issn><issn>1432-0630</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2015</creationdate><recordtype>article</recordtype><recordid>eNp9kD1vFDEQhi0EEkfgB9C5hMJhbO-u7TIKH0E5BEVSUFk-e_Zug88-7N2gy6_PHhtRMs1Io-d9pHkJecvhnAOoDxVASsOAt8yA0ezhGVnxRgoGnYTnZAWmUUxL070kr2q9g3kaIVbk57cpjgP74-4xYtqOO1rHKRxp7mlyKVf0OQUaXcXChhQmj4FupviLBrd3W6T7XA67HPP2SIdErz_-oL4c6-hifU1e9PPCN0_7jNx-_nRzecXW3798vbxYM9-IdmSbtlPgg1ZCI6g-aPR974LqeiGU32gpteqUNr736KDRoQmwwVYJbA1vlJRn5P3i3bloD2XYu3K02Q326mJtTzfgQrWqM_d8Zt8t7KHk3xPW0e6H6jFGlzBP1XIFRslW_tXyBfUl11qw_-fmYE-V26XyWd_aU-X2Yc6IJVNnNm2x2Ls8lTR__5_QIx3KhM0</recordid><startdate>20150601</startdate><enddate>20150601</enddate><creator>Reyné, S.</creator><creator>Duchateau, G.</creator><creator>Hallo, L.</creator><creator>Natoli, J. Y.</creator><creator>Lamaignère, L.</creator><general>Springer Berlin Heidelberg</general><general>Springer Verlag</general><scope>AAYXX</scope><scope>CITATION</scope><scope>7SP</scope><scope>7U5</scope><scope>8BQ</scope><scope>8FD</scope><scope>H8D</scope><scope>JG9</scope><scope>L7M</scope><scope>1XC</scope></search><sort><creationdate>20150601</creationdate><title>Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals</title><author>Reyné, S. ; Duchateau, G. ; Hallo, L. ; Natoli, J. Y. ; Lamaignère, L.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c425t-b5670cd8728e07fd8ecffad76f227cb833876789cfcea048d4d0be572e5914733</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2015</creationdate><topic>Characterization and Evaluation of Materials</topic><topic>Condensed Matter Physics</topic><topic>Damage</topic><topic>Fracture toughness</topic><topic>KDP crystals</topic><topic>Laser damage</topic><topic>Lasers</topic><topic>Machines</topic><topic>Manufacturing</topic><topic>Mathematical models</topic><topic>Morphology</topic><topic>Nanotechnology</topic><topic>Optical and Electronic Materials</topic><topic>Optics</topic><topic>Physics</topic><topic>Physics and Astronomy</topic><topic>Processes</topic><topic>Surfaces and Interfaces</topic><topic>Thin Films</topic><topic>Wavelengths</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Reyné, S.</creatorcontrib><creatorcontrib>Duchateau, G.</creatorcontrib><creatorcontrib>Hallo, L.</creatorcontrib><creatorcontrib>Natoli, J. Y.</creatorcontrib><creatorcontrib>Lamaignère, L.</creatorcontrib><collection>CrossRef</collection><collection>Electronics &amp; Communications Abstracts</collection><collection>Solid State and Superconductivity Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Aerospace Database</collection><collection>Materials Research Database</collection><collection>Advanced Technologies Database with Aerospace</collection><collection>Hyper Article en Ligne (HAL)</collection><jtitle>Applied physics. A, Materials science &amp; processing</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Reyné, S.</au><au>Duchateau, G.</au><au>Hallo, L.</au><au>Natoli, J. Y.</au><au>Lamaignère, L.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals</atitle><jtitle>Applied physics. A, Materials science &amp; processing</jtitle><stitle>Appl. Phys. A</stitle><date>2015-06-01</date><risdate>2015</risdate><volume>119</volume><issue>4</issue><spage>1317</spage><epage>1326</epage><pages>1317-1326</pages><issn>0947-8396</issn><eissn>1432-0630</eissn><abstract>This study reports on experimental results on the morphology of laser-induced damage in the bulk of potassium dihydrogen phosphate (or KDP) crystals by nanosecond pulses. The resulting morphology of bulk laser damage is structured in four different zones whose characteristics depend on laser parameters such as wavelength, laser polarization, and fluence. To have a better understanding of bulk formation and structure of KDP laser damage, accessing the mechanical properties of KDP is a promising way which departs from a thermal approach which is mainly used in various models well documented in the literature. In that way, we have revisited various mechanical models of fracturation frequently used to evaluate the toughness of optical materials. Our experiments are compared to these models where the toughness is the criterion, which has been chosen to validate the modeling part of this study. We conclude that experiments are in agreement with the common values obtained by indentations tests proposed in the literature, allowing us further developments with one of these models to describe the damage formation in KDP crystals. Also, it appears that laser damage events split into two separated groups depending on the wavelength, with on one side 351-nm damage sites and on the other side 1064- and 532-nm damage sites. That suggests the existence of different physical mechanisms responsible for bulk damage initiation in KDP crystals with respect to the wavelength.</abstract><cop>Berlin/Heidelberg</cop><pub>Springer Berlin Heidelberg</pub><doi>10.1007/s00339-015-9098-z</doi><tpages>10</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0947-8396
ispartof Applied physics. A, Materials science & processing, 2015-06, Vol.119 (4), p.1317-1326
issn 0947-8396
1432-0630
language eng
recordid cdi_hal_primary_oai_HAL_hal_01275769v1
source Springer Nature - Complete Springer Journals
subjects Characterization and Evaluation of Materials
Condensed Matter Physics
Damage
Fracture toughness
KDP crystals
Laser damage
Lasers
Machines
Manufacturing
Mathematical models
Morphology
Nanotechnology
Optical and Electronic Materials
Optics
Physics
Physics and Astronomy
Processes
Surfaces and Interfaces
Thin Films
Wavelengths
title Multi-wavelength study of nanosecond laser-induced bulk damage morphology in KDP crystals
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T14%3A51%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest_hal_p&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Multi-wavelength%20study%20of%20nanosecond%20laser-induced%20bulk%20damage%20morphology%20in%20KDP%20crystals&rft.jtitle=Applied%20physics.%20A,%20Materials%20science%20&%20processing&rft.au=Reyn%C3%A9,%20S.&rft.date=2015-06-01&rft.volume=119&rft.issue=4&rft.spage=1317&rft.epage=1326&rft.pages=1317-1326&rft.issn=0947-8396&rft.eissn=1432-0630&rft_id=info:doi/10.1007/s00339-015-9098-z&rft_dat=%3Cproquest_hal_p%3E1709735373%3C/proquest_hal_p%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=1709735373&rft_id=info:pmid/&rfr_iscdi=true