From core–shell BaTiO3@MgO to nanostructured low dielectric loss ceramics by spark plasma sintering

We report a quite general way to design materials with tailored properties by combining thermolysis and fast sintering approaches. Submicrometric-sized BaTiO3 particles have been directly coated in a continuous nanocrystalline MgO shell through a thermal decomposition process. The electron microscop...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials chemistry. C, Materials for optical and electronic devices Materials for optical and electronic devices, 2014-01, Vol.2 (4), p.683-690
Hauptverfasser: Berthelot, Romain, Basly, Brice, Buffiere, Sonia, Majimel, Jérôme, Chevallier, Geoffroy, Weibel, Alicia, Veillère, Amélie, Étienne, Laetitia, Chung, U-Chan, Goglio, Graziella, Maglione, Mario, Estournès, Claude, Mornet, Stéphane, Elissalde, Catherine
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We report a quite general way to design materials with tailored properties by combining thermolysis and fast sintering approaches. Submicrometric-sized BaTiO3 particles have been directly coated in a continuous nanocrystalline MgO shell through a thermal decomposition process. The electron microscopy study has evidenced a shell composed of randomly oriented MgO nanocrystallites. The final nanostructured composite, made of sub-micrometric MgO and BaTiO3 grains uniformly distributed, is obtained in situ during the SPS process. Such a rearrangement can be explained by the initial core–shell architecture, the weak cohesion of the MgO nanocrystallites and their soft plastic behavior under SPS conditions. The composite effect leads to significant modifications in both the dielectric properties and Curie–Weiss parameters compared to uncoated BaTiO3, especially a decrease and thermal stabilization of both the permittivity and the dielectric losses. We ascribe such changes to the stress generated during SPS through the extended interfaces between the two components.
ISSN:2050-7526
2050-7534
DOI:10.1039/c3tc31990c