ON 'REALLY' STOICHIOMETRIC LiCoO2
The 7Li NMR T1 spin-lattice relaxation time was to be a very stringent criterion for determining stoichiometry of LiCoO2. When Co3O4 containing a impurity level of paramagnetic ions such as Fe or was used as the starting material (together with a T1 value as long as 18 s was obtained, but this a rat...