METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES
A method for enriching and recovering chromium resources by means of the synergistic utilization of chromium-containing sludge and chromium-containing waste residue: the chromium-containing sludge and the chromium-containing waste residue are finely ground and mixed to prepare a mixture, the mixture...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | PEI, Dejian WANG, Daya LI, Gang LI, Shuqin LI, Xiangmei HUA, Shaoguang |
description | A method for enriching and recovering chromium resources by means of the synergistic utilization of chromium-containing sludge and chromium-containing waste residue: the chromium-containing sludge and the chromium-containing waste residue are finely ground and mixed to prepare a mixture, the mixture alkalinity ((CaO%+MgO%)/(SiO2%+Al2O3%)) is within the range of 0.6 to 1.5, and FeOx content is greater than or equal to 15.0%. The mixture is subject to reduction roasting, and the roasting temperature is controlled to be within the range of 1100 to 1500°C. After grinding the roasted product, iron-chromium spinel is separated by using a strong magnetic separation process to obtain a chromium concentrate which has a Cr2O3 content that is greater than or equal to 20.0% and a Cr2O3 recovery rate that is greater than or equal to 85.0%. Two chromium-containing hazardous waste resources, i.e. the chromium-containing sludge and the chromium-containing waste residue are combined, and the chromium in the two resources is enriched at the same time, so that an obtained chromium-containing enriched phase has a high chromium grade, and by utilizing subsequent separation, has the characteristics of high efficiency, low pollution and a wide application range, which is suitable for application in the technical field of chromium enrichment and separation in chromium-containing resources. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_ZA202204726B</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>ZA202204726B</sourcerecordid><originalsourceid>FETCH-epo_espacenet_ZA202204726B3</originalsourceid><addsrcrecordid>eNqNjL0KwjAUhbs4iPoO8QEKJYrO6c1teyFNID9IupQicRIt6KP4wFpxcHBwOpxzPr559mjRN0ayyliG2hI0pGsmtGQWIYKaGjTWtBTa1-RMsICOlZG5qNHW5DyBUCqy4ElR983nYLQXpKfNqSBrfIt_3QfhPE5-kgHdMpudhvMtrT65yNYVemjyNF77dBuHY7qke98JXnBebPd8V27-YZ7S90KJ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES</title><source>esp@cenet</source><creator>PEI, Dejian ; WANG, Daya ; LI, Gang ; LI, Shuqin ; LI, Xiangmei ; HUA, Shaoguang</creator><creatorcontrib>PEI, Dejian ; WANG, Daya ; LI, Gang ; LI, Shuqin ; LI, Xiangmei ; HUA, Shaoguang</creatorcontrib><description>A method for enriching and recovering chromium resources by means of the synergistic utilization of chromium-containing sludge and chromium-containing waste residue: the chromium-containing sludge and the chromium-containing waste residue are finely ground and mixed to prepare a mixture, the mixture alkalinity ((CaO%+MgO%)/(SiO2%+Al2O3%)) is within the range of 0.6 to 1.5, and FeOx content is greater than or equal to 15.0%. The mixture is subject to reduction roasting, and the roasting temperature is controlled to be within the range of 1100 to 1500°C. After grinding the roasted product, iron-chromium spinel is separated by using a strong magnetic separation process to obtain a chromium concentrate which has a Cr2O3 content that is greater than or equal to 20.0% and a Cr2O3 recovery rate that is greater than or equal to 85.0%. Two chromium-containing hazardous waste resources, i.e. the chromium-containing sludge and the chromium-containing waste residue are combined, and the chromium in the two resources is enriched at the same time, so that an obtained chromium-containing enriched phase has a high chromium grade, and by utilizing subsequent separation, has the characteristics of high efficiency, low pollution and a wide application range, which is suitable for application in the technical field of chromium enrichment and separation in chromium-containing resources.</description><language>eng</language><creationdate>2022</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220629&DB=EPODOC&CC=ZA&NR=202204726B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20220629&DB=EPODOC&CC=ZA&NR=202204726B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PEI, Dejian</creatorcontrib><creatorcontrib>WANG, Daya</creatorcontrib><creatorcontrib>LI, Gang</creatorcontrib><creatorcontrib>LI, Shuqin</creatorcontrib><creatorcontrib>LI, Xiangmei</creatorcontrib><creatorcontrib>HUA, Shaoguang</creatorcontrib><title>METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES</title><description>A method for enriching and recovering chromium resources by means of the synergistic utilization of chromium-containing sludge and chromium-containing waste residue: the chromium-containing sludge and the chromium-containing waste residue are finely ground and mixed to prepare a mixture, the mixture alkalinity ((CaO%+MgO%)/(SiO2%+Al2O3%)) is within the range of 0.6 to 1.5, and FeOx content is greater than or equal to 15.0%. The mixture is subject to reduction roasting, and the roasting temperature is controlled to be within the range of 1100 to 1500°C. After grinding the roasted product, iron-chromium spinel is separated by using a strong magnetic separation process to obtain a chromium concentrate which has a Cr2O3 content that is greater than or equal to 20.0% and a Cr2O3 recovery rate that is greater than or equal to 85.0%. Two chromium-containing hazardous waste resources, i.e. the chromium-containing sludge and the chromium-containing waste residue are combined, and the chromium in the two resources is enriched at the same time, so that an obtained chromium-containing enriched phase has a high chromium grade, and by utilizing subsequent separation, has the characteristics of high efficiency, low pollution and a wide application range, which is suitable for application in the technical field of chromium enrichment and separation in chromium-containing resources.</description><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2022</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjL0KwjAUhbs4iPoO8QEKJYrO6c1teyFNID9IupQicRIt6KP4wFpxcHBwOpxzPr559mjRN0ayyliG2hI0pGsmtGQWIYKaGjTWtBTa1-RMsICOlZG5qNHW5DyBUCqy4ElR983nYLQXpKfNqSBrfIt_3QfhPE5-kgHdMpudhvMtrT65yNYVemjyNF77dBuHY7qke98JXnBebPd8V27-YZ7S90KJ</recordid><startdate>20220629</startdate><enddate>20220629</enddate><creator>PEI, Dejian</creator><creator>WANG, Daya</creator><creator>LI, Gang</creator><creator>LI, Shuqin</creator><creator>LI, Xiangmei</creator><creator>HUA, Shaoguang</creator><scope>EVB</scope></search><sort><creationdate>20220629</creationdate><title>METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES</title><author>PEI, Dejian ; WANG, Daya ; LI, Gang ; LI, Shuqin ; LI, Xiangmei ; HUA, Shaoguang</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_ZA202204726B3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2022</creationdate><toplevel>online_resources</toplevel><creatorcontrib>PEI, Dejian</creatorcontrib><creatorcontrib>WANG, Daya</creatorcontrib><creatorcontrib>LI, Gang</creatorcontrib><creatorcontrib>LI, Shuqin</creatorcontrib><creatorcontrib>LI, Xiangmei</creatorcontrib><creatorcontrib>HUA, Shaoguang</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PEI, Dejian</au><au>WANG, Daya</au><au>LI, Gang</au><au>LI, Shuqin</au><au>LI, Xiangmei</au><au>HUA, Shaoguang</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES</title><date>2022-06-29</date><risdate>2022</risdate><abstract>A method for enriching and recovering chromium resources by means of the synergistic utilization of chromium-containing sludge and chromium-containing waste residue: the chromium-containing sludge and the chromium-containing waste residue are finely ground and mixed to prepare a mixture, the mixture alkalinity ((CaO%+MgO%)/(SiO2%+Al2O3%)) is within the range of 0.6 to 1.5, and FeOx content is greater than or equal to 15.0%. The mixture is subject to reduction roasting, and the roasting temperature is controlled to be within the range of 1100 to 1500°C. After grinding the roasted product, iron-chromium spinel is separated by using a strong magnetic separation process to obtain a chromium concentrate which has a Cr2O3 content that is greater than or equal to 20.0% and a Cr2O3 recovery rate that is greater than or equal to 85.0%. Two chromium-containing hazardous waste resources, i.e. the chromium-containing sludge and the chromium-containing waste residue are combined, and the chromium in the two resources is enriched at the same time, so that an obtained chromium-containing enriched phase has a high chromium grade, and by utilizing subsequent separation, has the characteristics of high efficiency, low pollution and a wide application range, which is suitable for application in the technical field of chromium enrichment and separation in chromium-containing resources.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_ZA202204726B |
source | esp@cenet |
title | METHOD FOR ENRICHING AND RECYCLING CHROMIUM RESOURCES BY SYNERGISTICALLY UTILIZING CHROMIUM-CONTAINING SLUDGE AND CHROMIUM-CONTAINING WASTE RESIDUES |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T13%3A24%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PEI,%20Dejian&rft.date=2022-06-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EZA202204726B%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |