ADHESIVE AND DAMPING FILM

Adhesives including a polyester at 20 to 50 weight percent, a first tackifier at 30 to 60 weight percent, and a first olefin-styrene block copolymer at 5 to 30 weight percent are described. The polyester has a glass transition temperature between -40 °C and -10 °C, and the adhesive has a heat activa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BENDING, Benjamin J, LIU, Richard Y, LEHN, Nathaniel I, GRISLE, Roger A
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Adhesives including a polyester at 20 to 50 weight percent, a first tackifier at 30 to 60 weight percent, and a first olefin-styrene block copolymer at 5 to 30 weight percent are described. The polyester has a glass transition temperature between -40 °C and -10 °C, and the adhesive has a heat activation temperature between 20 °C and 100 °C. Damping films including at least one layer of the adhesive and including a foamed layer are described. The foamed layer includes a second olefin-styrene block copolymer at 30 to 80 weight percent and a second tackifier at 15 to 60 weight percent. L'invention concerne des adhésifs comprenant un polyester à raison de 20 à 50 pour cent en poids, un premier agent poisseux à raison de 30 à 60 pour cent en poids et un premier copolymère séquencé d'oléfine-styrène à raison de 5 à 30 pour cent en poids. Le polyester présente une température de transition vitreuse entre -40°C et -10°C et l'adhésif présente une température d'activation thermique entre 20°C et 100°C. Des films d'amortissement comprenant au moins une couche de l'adhésif et comprenant une couche moussée sont décrits. La couche moussée comprend un deuxième copolymère séquencé d'oléfine-styrène à raison de 30 à 80 pour cent en poids et un deuxième agent poisseux à raison de 15 à 60 pour cent en poids.