MULTI-LAYER CATHODE BLOCK

A multi-layer cathode block (30) for an electrolytic cell (10) has at least a surface layer (32) with a surface expansion index and a second layer (34) with a second expansion index. The surface layer (32) includes a surface wetting agent in a first total amount. The second layer (34) includes a wet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BERGERON, JULES, BRISSON, PIERRE-YVES, LECLERC, SIMON, CAMIRE, JEAN
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator BERGERON, JULES
BRISSON, PIERRE-YVES
LECLERC, SIMON
CAMIRE, JEAN
description A multi-layer cathode block (30) for an electrolytic cell (10) has at least a surface layer (32) with a surface expansion index and a second layer (34) with a second expansion index. The surface layer (32) includes a surface wetting agent in a first total amount. The second layer (34) includes a wetting agent in a second total amount. The surface layer (32) is directly superposed to the second layer (34). The second wetting agent in the second layer (34) includes metal boride precursors that react together to generate a metal boride component in situ when the cathode block (30) is exposed to start-up and operation conditions of the electrolytic cell (10). The second total amount is lower than the first total amount and is selected so as to minimize the difference between the expansion indexes of the surface layer (32) and the second layer (34). L'invention concerne un bloc stratifié (30) de cathode pour cellule électrolytique (10), qui présente au moins une couche de surface (32) dotée d'un indice de dilatation de surface et une deuxième couche (34) dotée d'un deuxième indice de dilatation. La couche de surface (32) contient une première quantité totale d'agent de mouillage de surface. La deuxième couche (34) contient une deuxième quantité totale d'agent de mouillage. La couche de surface (32) est superposée directement à la deuxième couche (34). Le deuxième agent de mouillage présent dans la deuxième couche (34) contient des précurseurs de borure métallique qui réagissent entre eux pour produire in situ un composant borure métallique lorsque le bloc de cathode (30) est exposé aux conditions de démarrage et de fonctionnement de la cellule électrolytique (10). La deuxième quantité totale est inférieure à la première quantité totale et est sélectionnée de manière à minimiser la différence entre les indices de dilatation de la couche de surface (32) et de la deuxième couche (34).
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_WO2009132459A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>WO2009132459A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_WO2009132459A13</originalsourceid><addsrcrecordid>eNrjZJD0DfUJ8dT1cYx0DVJwdgzx8HdxVXDy8Xf25mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGlobGRiamlo6GxsSpAgCImSDO</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>MULTI-LAYER CATHODE BLOCK</title><source>esp@cenet</source><creator>BERGERON, JULES ; BRISSON, PIERRE-YVES ; LECLERC, SIMON ; CAMIRE, JEAN</creator><creatorcontrib>BERGERON, JULES ; BRISSON, PIERRE-YVES ; LECLERC, SIMON ; CAMIRE, JEAN</creatorcontrib><description>A multi-layer cathode block (30) for an electrolytic cell (10) has at least a surface layer (32) with a surface expansion index and a second layer (34) with a second expansion index. The surface layer (32) includes a surface wetting agent in a first total amount. The second layer (34) includes a wetting agent in a second total amount. The surface layer (32) is directly superposed to the second layer (34). The second wetting agent in the second layer (34) includes metal boride precursors that react together to generate a metal boride component in situ when the cathode block (30) is exposed to start-up and operation conditions of the electrolytic cell (10). The second total amount is lower than the first total amount and is selected so as to minimize the difference between the expansion indexes of the surface layer (32) and the second layer (34). L'invention concerne un bloc stratifié (30) de cathode pour cellule électrolytique (10), qui présente au moins une couche de surface (32) dotée d'un indice de dilatation de surface et une deuxième couche (34) dotée d'un deuxième indice de dilatation. La couche de surface (32) contient une première quantité totale d'agent de mouillage de surface. La deuxième couche (34) contient une deuxième quantité totale d'agent de mouillage. La couche de surface (32) est superposée directement à la deuxième couche (34). Le deuxième agent de mouillage présent dans la deuxième couche (34) contient des précurseurs de borure métallique qui réagissent entre eux pour produire in situ un composant borure métallique lorsque le bloc de cathode (30) est exposé aux conditions de démarrage et de fonctionnement de la cellule électrolytique (10). La deuxième quantité totale est inférieure à la première quantité totale et est sélectionnée de manière à minimiser la différence entre les indices de dilatation de la couche de surface (32) et de la deuxième couche (34).</description><language>eng ; fre</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091105&amp;DB=EPODOC&amp;CC=WO&amp;NR=2009132459A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20091105&amp;DB=EPODOC&amp;CC=WO&amp;NR=2009132459A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BERGERON, JULES</creatorcontrib><creatorcontrib>BRISSON, PIERRE-YVES</creatorcontrib><creatorcontrib>LECLERC, SIMON</creatorcontrib><creatorcontrib>CAMIRE, JEAN</creatorcontrib><title>MULTI-LAYER CATHODE BLOCK</title><description>A multi-layer cathode block (30) for an electrolytic cell (10) has at least a surface layer (32) with a surface expansion index and a second layer (34) with a second expansion index. The surface layer (32) includes a surface wetting agent in a first total amount. The second layer (34) includes a wetting agent in a second total amount. The surface layer (32) is directly superposed to the second layer (34). The second wetting agent in the second layer (34) includes metal boride precursors that react together to generate a metal boride component in situ when the cathode block (30) is exposed to start-up and operation conditions of the electrolytic cell (10). The second total amount is lower than the first total amount and is selected so as to minimize the difference between the expansion indexes of the surface layer (32) and the second layer (34). L'invention concerne un bloc stratifié (30) de cathode pour cellule électrolytique (10), qui présente au moins une couche de surface (32) dotée d'un indice de dilatation de surface et une deuxième couche (34) dotée d'un deuxième indice de dilatation. La couche de surface (32) contient une première quantité totale d'agent de mouillage de surface. La deuxième couche (34) contient une deuxième quantité totale d'agent de mouillage. La couche de surface (32) est superposée directement à la deuxième couche (34). Le deuxième agent de mouillage présent dans la deuxième couche (34) contient des précurseurs de borure métallique qui réagissent entre eux pour produire in situ un composant borure métallique lorsque le bloc de cathode (30) est exposé aux conditions de démarrage et de fonctionnement de la cellule électrolytique (10). La deuxième quantité totale est inférieure à la première quantité totale et est sélectionnée de manière à minimiser la différence entre les indices de dilatation de la couche de surface (32) et de la deuxième couche (34).</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJD0DfUJ8dT1cYx0DVJwdgzx8HdxVXDy8Xf25mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGlobGRiamlo6GxsSpAgCImSDO</recordid><startdate>20091105</startdate><enddate>20091105</enddate><creator>BERGERON, JULES</creator><creator>BRISSON, PIERRE-YVES</creator><creator>LECLERC, SIMON</creator><creator>CAMIRE, JEAN</creator><scope>EVB</scope></search><sort><creationdate>20091105</creationdate><title>MULTI-LAYER CATHODE BLOCK</title><author>BERGERON, JULES ; BRISSON, PIERRE-YVES ; LECLERC, SIMON ; CAMIRE, JEAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_WO2009132459A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>2009</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>BERGERON, JULES</creatorcontrib><creatorcontrib>BRISSON, PIERRE-YVES</creatorcontrib><creatorcontrib>LECLERC, SIMON</creatorcontrib><creatorcontrib>CAMIRE, JEAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BERGERON, JULES</au><au>BRISSON, PIERRE-YVES</au><au>LECLERC, SIMON</au><au>CAMIRE, JEAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>MULTI-LAYER CATHODE BLOCK</title><date>2009-11-05</date><risdate>2009</risdate><abstract>A multi-layer cathode block (30) for an electrolytic cell (10) has at least a surface layer (32) with a surface expansion index and a second layer (34) with a second expansion index. The surface layer (32) includes a surface wetting agent in a first total amount. The second layer (34) includes a wetting agent in a second total amount. The surface layer (32) is directly superposed to the second layer (34). The second wetting agent in the second layer (34) includes metal boride precursors that react together to generate a metal boride component in situ when the cathode block (30) is exposed to start-up and operation conditions of the electrolytic cell (10). The second total amount is lower than the first total amount and is selected so as to minimize the difference between the expansion indexes of the surface layer (32) and the second layer (34). L'invention concerne un bloc stratifié (30) de cathode pour cellule électrolytique (10), qui présente au moins une couche de surface (32) dotée d'un indice de dilatation de surface et une deuxième couche (34) dotée d'un deuxième indice de dilatation. La couche de surface (32) contient une première quantité totale d'agent de mouillage de surface. La deuxième couche (34) contient une deuxième quantité totale d'agent de mouillage. La couche de surface (32) est superposée directement à la deuxième couche (34). Le deuxième agent de mouillage présent dans la deuxième couche (34) contient des précurseurs de borure métallique qui réagissent entre eux pour produire in situ un composant borure métallique lorsque le bloc de cathode (30) est exposé aux conditions de démarrage et de fonctionnement de la cellule électrolytique (10). La deuxième quantité totale est inférieure à la première quantité totale et est sélectionnée de manière à minimiser la différence entre les indices de dilatation de la couche de surface (32) et de la deuxième couche (34).</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_WO2009132459A1
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS
title MULTI-LAYER CATHODE BLOCK
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T20%3A36%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BERGERON,%20JULES&rft.date=2009-11-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EWO2009132459A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true