COPPER-NICKEL-SILICON ALLOYS

A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUHN, HANS, ACHIM, TYLER, DEREK, E, HOFMANN, UWE, MUTSCHLER, RALPH, A, ROBINSON, PETER, WILLIAM, KAUFLER, ANDREA
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUHN, HANS, ACHIM
TYLER, DEREK, E
HOFMANN, UWE
MUTSCHLER, RALPH, A
ROBINSON, PETER, WILLIAM
KAUFLER, ANDREA
description A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight percent Mg, up to about 1.0 weight percent Cr, up to about 1.0 weight percent Sn, and up to about 1.0 weight percent Mn, the balance being copper and impurities, the alloy processed to have a yield strength of at least about 137ksi, and an electrical conductivity of at least about 25% IACS. L'invention concerne un alliage à base de cuivre ayant une combinaison améliorée de la limite d'élasticité et de la conductivité électrique consistant sensiblement en entre environ 1,0 et environ 6,0 pour cent en poids de Ni, jusqu'à environ 3,0 pour cent en poids de Co, entre environ 0,5 et environ 2,0 pour cent en poids de Si, entre environ 0,01 et environ 0,5 pour cent en poids de Mg, jusqu'à environ 1,0 pour cent en poids de Cr, jusqu'à environ 1,0 pour cent en poids de Sn et jusqu'à environ 1,0 pour cent en poids de Mn, le reste étant du cuivre et des impuretés, l'alliage étant traité pour avoir une limite d'élasticité d'au moins environ 137 ksi et une conductivité électrique d'au moins environ 25 % IACS.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_WO2009082695A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>WO2009082695A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_WO2009082695A13</originalsourceid><addsrcrecordid>eNrjZJBx9g8IcA3S9fN09nb10Q329PF09vdTcPTx8Y8M5mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGlgYWRmaWpo6GxsSpAgAApyHj</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COPPER-NICKEL-SILICON ALLOYS</title><source>esp@cenet</source><creator>KUHN, HANS, ACHIM ; TYLER, DEREK, E ; HOFMANN, UWE ; MUTSCHLER, RALPH, A ; ROBINSON, PETER, WILLIAM ; KAUFLER, ANDREA</creator><creatorcontrib>KUHN, HANS, ACHIM ; TYLER, DEREK, E ; HOFMANN, UWE ; MUTSCHLER, RALPH, A ; ROBINSON, PETER, WILLIAM ; KAUFLER, ANDREA</creatorcontrib><description>A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight percent Mg, up to about 1.0 weight percent Cr, up to about 1.0 weight percent Sn, and up to about 1.0 weight percent Mn, the balance being copper and impurities, the alloy processed to have a yield strength of at least about 137ksi, and an electrical conductivity of at least about 25% IACS. L'invention concerne un alliage à base de cuivre ayant une combinaison améliorée de la limite d'élasticité et de la conductivité électrique consistant sensiblement en entre environ 1,0 et environ 6,0 pour cent en poids de Ni, jusqu'à environ 3,0 pour cent en poids de Co, entre environ 0,5 et environ 2,0 pour cent en poids de Si, entre environ 0,01 et environ 0,5 pour cent en poids de Mg, jusqu'à environ 1,0 pour cent en poids de Cr, jusqu'à environ 1,0 pour cent en poids de Sn et jusqu'à environ 1,0 pour cent en poids de Mn, le reste étant du cuivre et des impuretés, l'alliage étant traité pour avoir une limite d'élasticité d'au moins environ 137 ksi et une conductivité électrique d'au moins environ 25 % IACS.</description><language>eng ; fre</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090702&amp;DB=EPODOC&amp;CC=WO&amp;NR=2009082695A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090702&amp;DB=EPODOC&amp;CC=WO&amp;NR=2009082695A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUHN, HANS, ACHIM</creatorcontrib><creatorcontrib>TYLER, DEREK, E</creatorcontrib><creatorcontrib>HOFMANN, UWE</creatorcontrib><creatorcontrib>MUTSCHLER, RALPH, A</creatorcontrib><creatorcontrib>ROBINSON, PETER, WILLIAM</creatorcontrib><creatorcontrib>KAUFLER, ANDREA</creatorcontrib><title>COPPER-NICKEL-SILICON ALLOYS</title><description>A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight percent Mg, up to about 1.0 weight percent Cr, up to about 1.0 weight percent Sn, and up to about 1.0 weight percent Mn, the balance being copper and impurities, the alloy processed to have a yield strength of at least about 137ksi, and an electrical conductivity of at least about 25% IACS. L'invention concerne un alliage à base de cuivre ayant une combinaison améliorée de la limite d'élasticité et de la conductivité électrique consistant sensiblement en entre environ 1,0 et environ 6,0 pour cent en poids de Ni, jusqu'à environ 3,0 pour cent en poids de Co, entre environ 0,5 et environ 2,0 pour cent en poids de Si, entre environ 0,01 et environ 0,5 pour cent en poids de Mg, jusqu'à environ 1,0 pour cent en poids de Cr, jusqu'à environ 1,0 pour cent en poids de Sn et jusqu'à environ 1,0 pour cent en poids de Mn, le reste étant du cuivre et des impuretés, l'alliage étant traité pour avoir une limite d'élasticité d'au moins environ 137 ksi et une conductivité électrique d'au moins environ 25 % IACS.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJBx9g8IcA3S9fN09nb10Q329PF09vdTcPTx8Y8M5mFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGlgYWRmaWpo6GxsSpAgAApyHj</recordid><startdate>20090702</startdate><enddate>20090702</enddate><creator>KUHN, HANS, ACHIM</creator><creator>TYLER, DEREK, E</creator><creator>HOFMANN, UWE</creator><creator>MUTSCHLER, RALPH, A</creator><creator>ROBINSON, PETER, WILLIAM</creator><creator>KAUFLER, ANDREA</creator><scope>EVB</scope></search><sort><creationdate>20090702</creationdate><title>COPPER-NICKEL-SILICON ALLOYS</title><author>KUHN, HANS, ACHIM ; TYLER, DEREK, E ; HOFMANN, UWE ; MUTSCHLER, RALPH, A ; ROBINSON, PETER, WILLIAM ; KAUFLER, ANDREA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_WO2009082695A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>2009</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KUHN, HANS, ACHIM</creatorcontrib><creatorcontrib>TYLER, DEREK, E</creatorcontrib><creatorcontrib>HOFMANN, UWE</creatorcontrib><creatorcontrib>MUTSCHLER, RALPH, A</creatorcontrib><creatorcontrib>ROBINSON, PETER, WILLIAM</creatorcontrib><creatorcontrib>KAUFLER, ANDREA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUHN, HANS, ACHIM</au><au>TYLER, DEREK, E</au><au>HOFMANN, UWE</au><au>MUTSCHLER, RALPH, A</au><au>ROBINSON, PETER, WILLIAM</au><au>KAUFLER, ANDREA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COPPER-NICKEL-SILICON ALLOYS</title><date>2009-07-02</date><risdate>2009</risdate><abstract>A copper base alloy having an improved combination of yield strength and electrical conductivity consisting essentially of between about 1.0 and about 6.0 weight percent Ni, up to about 3.0 weight percent Co, between about 0.5 and about 2.0 weight percent Si, between about 0.01 and about 0.5 weight percent Mg, up to about 1.0 weight percent Cr, up to about 1.0 weight percent Sn, and up to about 1.0 weight percent Mn, the balance being copper and impurities, the alloy processed to have a yield strength of at least about 137ksi, and an electrical conductivity of at least about 25% IACS. L'invention concerne un alliage à base de cuivre ayant une combinaison améliorée de la limite d'élasticité et de la conductivité électrique consistant sensiblement en entre environ 1,0 et environ 6,0 pour cent en poids de Ni, jusqu'à environ 3,0 pour cent en poids de Co, entre environ 0,5 et environ 2,0 pour cent en poids de Si, entre environ 0,01 et environ 0,5 pour cent en poids de Mg, jusqu'à environ 1,0 pour cent en poids de Cr, jusqu'à environ 1,0 pour cent en poids de Sn et jusqu'à environ 1,0 pour cent en poids de Mn, le reste étant du cuivre et des impuretés, l'alliage étant traité pour avoir une limite d'élasticité d'au moins environ 137 ksi et une conductivité électrique d'au moins environ 25 % IACS.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_WO2009082695A1
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title COPPER-NICKEL-SILICON ALLOYS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T06%3A12%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUHN,%20HANS,%20ACHIM&rft.date=2009-07-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EWO2009082695A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true