TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE

A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, sili...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KIRKEGAARD STAGE, RASMUS, KARLSSON, ASGER
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KIRKEGAARD STAGE, RASMUS
KARLSSON, ASGER
description A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, silicon: 0.8-1.2 %, nickel: 8.0-10.0 %, molybdenum: 0.8-1.2 % balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 °C as compared to the known allows. La présente invention concerne un alliage de fonte stable à la température ayant une résistance à l'usure élevée à des températures comprises entre 500 et 900° C. L'alliage se caractérise par la composition suivante exprimée en pourcents pondéraux : chrome : 15,0-20,0 %, carbone : 1,0-2,0 %, manganèse: 1,5-2,0 %, silicium : 0,8-1,2 %, nickel : 8,0-10,0 %, molybdène : 0,8-1,2 %, le reste étant du fer et des impuretés métalliques et non métalliques inévitablement présentes, les impuretés non métalliques comprenant l'azote, l'oxygène, le phosphore et le soufre. On obtient ainsi un alliage de fonte ayant, par rapport aux alliages de l'état de la technique, une résistance à l'usure supérieure et une tendance réduite à la formation de phase sigma indésirable lorsqu'il est chauffé à des températures comprises entre 500 et 900 °C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_WO2008029305A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>WO2008029305A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_WO2008029305A13</originalsourceid><addsrcrecordid>eNrjZNALcfUNcA1yDAkNctUNDnF08nFVcHYMDtH1DPL3U3D08fGPVHD0c1HwDAlWCA125WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGFgZGlsYGpo6GxsSpAgB5wSaW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE</title><source>esp@cenet</source><creator>KIRKEGAARD STAGE, RASMUS ; KARLSSON, ASGER</creator><creatorcontrib>KIRKEGAARD STAGE, RASMUS ; KARLSSON, ASGER</creatorcontrib><description>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, silicon: 0.8-1.2 %, nickel: 8.0-10.0 %, molybdenum: 0.8-1.2 % balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 °C as compared to the known allows. La présente invention concerne un alliage de fonte stable à la température ayant une résistance à l'usure élevée à des températures comprises entre 500 et 900° C. L'alliage se caractérise par la composition suivante exprimée en pourcents pondéraux : chrome : 15,0-20,0 %, carbone : 1,0-2,0 %, manganèse: 1,5-2,0 %, silicium : 0,8-1,2 %, nickel : 8,0-10,0 %, molybdène : 0,8-1,2 %, le reste étant du fer et des impuretés métalliques et non métalliques inévitablement présentes, les impuretés non métalliques comprenant l'azote, l'oxygène, le phosphore et le soufre. On obtient ainsi un alliage de fonte ayant, par rapport aux alliages de l'état de la technique, une résistance à l'usure supérieure et une tendance réduite à la formation de phase sigma indésirable lorsqu'il est chauffé à des températures comprises entre 500 et 900 °C.</description><language>eng ; fre</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080313&amp;DB=EPODOC&amp;CC=WO&amp;NR=2008029305A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080313&amp;DB=EPODOC&amp;CC=WO&amp;NR=2008029305A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KIRKEGAARD STAGE, RASMUS</creatorcontrib><creatorcontrib>KARLSSON, ASGER</creatorcontrib><title>TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE</title><description>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, silicon: 0.8-1.2 %, nickel: 8.0-10.0 %, molybdenum: 0.8-1.2 % balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 °C as compared to the known allows. La présente invention concerne un alliage de fonte stable à la température ayant une résistance à l'usure élevée à des températures comprises entre 500 et 900° C. L'alliage se caractérise par la composition suivante exprimée en pourcents pondéraux : chrome : 15,0-20,0 %, carbone : 1,0-2,0 %, manganèse: 1,5-2,0 %, silicium : 0,8-1,2 %, nickel : 8,0-10,0 %, molybdène : 0,8-1,2 %, le reste étant du fer et des impuretés métalliques et non métalliques inévitablement présentes, les impuretés non métalliques comprenant l'azote, l'oxygène, le phosphore et le soufre. On obtient ainsi un alliage de fonte ayant, par rapport aux alliages de l'état de la technique, une résistance à l'usure supérieure et une tendance réduite à la formation de phase sigma indésirable lorsqu'il est chauffé à des températures comprises entre 500 et 900 °C.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNALcfUNcA1yDAkNctUNDnF08nFVcHYMDtH1DPL3U3D08fGPVHD0c1HwDAlWCA125WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8eH-RgYGFgZGlsYGpo6GxsSpAgB5wSaW</recordid><startdate>20080313</startdate><enddate>20080313</enddate><creator>KIRKEGAARD STAGE, RASMUS</creator><creator>KARLSSON, ASGER</creator><scope>EVB</scope></search><sort><creationdate>20080313</creationdate><title>TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE</title><author>KIRKEGAARD STAGE, RASMUS ; KARLSSON, ASGER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_WO2008029305A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>2008</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KIRKEGAARD STAGE, RASMUS</creatorcontrib><creatorcontrib>KARLSSON, ASGER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KIRKEGAARD STAGE, RASMUS</au><au>KARLSSON, ASGER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE</title><date>2008-03-13</date><risdate>2008</risdate><abstract>A description is given of a temperature-stable cast-iron alloy having high wear resistance at temperatures between 500 and 900° C. The alloy is characterized in that it has the following composition expressed in weight percentages: chromium: 15.0-20.0 %, carbon: 1.0-2.0 %, manganese: 1.5-2.0 %, silicon: 0.8-1.2 %, nickel: 8.0-10.0 %, molybdenum: 0.8-1.2 % balance iron and unavoidable metallic and non-metallic contaminants where the non-metallic contaminants comprise nitrogen, oxygen, phosphorous and sulphur. Hereby is obtained a cast-iron alloy which has a higher wear resistance and a reduced tendency to form the undesirable sigma phase when heated to temperatures between 500 and 900 °C as compared to the known allows. La présente invention concerne un alliage de fonte stable à la température ayant une résistance à l'usure élevée à des températures comprises entre 500 et 900° C. L'alliage se caractérise par la composition suivante exprimée en pourcents pondéraux : chrome : 15,0-20,0 %, carbone : 1,0-2,0 %, manganèse: 1,5-2,0 %, silicium : 0,8-1,2 %, nickel : 8,0-10,0 %, molybdène : 0,8-1,2 %, le reste étant du fer et des impuretés métalliques et non métalliques inévitablement présentes, les impuretés non métalliques comprenant l'azote, l'oxygène, le phosphore et le soufre. On obtient ainsi un alliage de fonte ayant, par rapport aux alliages de l'état de la technique, une résistance à l'usure supérieure et une tendance réduite à la formation de phase sigma indésirable lorsqu'il est chauffé à des températures comprises entre 500 et 900 °C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_WO2008029305A1
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title TEMPERATURE-STABLE CAST-IRON ALLOY AND ITS USE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T17%3A25%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KIRKEGAARD%20STAGE,%20RASMUS&rft.date=2008-03-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EWO2008029305A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true