METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE

A method in recovering nickel and possibly cobalt through leaching from inckel-containing laterite ore. Crushed and possibly pre-ground nickel-containing laterite ore is ground in an attritor mill into a size which is suitable for leaching. Then laterite ore in an attritor mill can be leached with l...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KARPALE, KAUKO, AALTONEN, ANTTI, MALMSTROEM, ROLF
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KARPALE, KAUKO
AALTONEN, ANTTI
MALMSTROEM, ROLF
description A method in recovering nickel and possibly cobalt through leaching from inckel-containing laterite ore. Crushed and possibly pre-ground nickel-containing laterite ore is ground in an attritor mill into a size which is suitable for leaching. Then laterite ore in an attritor mill can be leached with leaching liquid , e.g. sulphuric acid, hydrochloric acid, or sulphuric acid + SO2, at relatively low temperatures. Nickel and possibly cobalt are recovered from the leaching solution. L'invention concerne un procédé permettant de récupérer du nickel et probablement du cobalt par lixiviation d'un minerai de latérite contenant du nickel. On broie, dans une broyeuse par frottement, de la latérite contenant du nickel écrasé et probablement pré-broyé à une taille appropriée à la lixiviation. Puis, on peut lixivier la latérite moulue avec un liquide de lixiviation, par exemple, un acide sulfurique, un acide chlorhydrique ou un acide sulfurique ajoutée à SO2, à des températures relativement basses, le nickel et le cobalt pouvant être récupérés à partir de la solution de lixiviation.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_WO03004709A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>WO03004709A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_WO03004709A13</originalsourceid><addsrcrecordid>eNqNzMEKgkAQgGEvHaJ6h-kBhA2D6DiuYy6tM7BMlieR2k5Rgr0_FfgAnf7Lxz9PbjVpJQWUEiCQlYaC4wOws0fygFwANcR6Qu9bsJKjV8hboIsGtOqEoQxSTz61woqOfweP-l0pgQRaJrN7_xjjauoiWZektkrj8OriOPTX-Izv7iwmM2a7M3vcZP-YD1NaNKU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE</title><source>esp@cenet</source><creator>KARPALE, KAUKO ; AALTONEN, ANTTI ; MALMSTROEM, ROLF</creator><creatorcontrib>KARPALE, KAUKO ; AALTONEN, ANTTI ; MALMSTROEM, ROLF</creatorcontrib><description>A method in recovering nickel and possibly cobalt through leaching from inckel-containing laterite ore. Crushed and possibly pre-ground nickel-containing laterite ore is ground in an attritor mill into a size which is suitable for leaching. Then laterite ore in an attritor mill can be leached with leaching liquid , e.g. sulphuric acid, hydrochloric acid, or sulphuric acid + SO2, at relatively low temperatures. Nickel and possibly cobalt are recovered from the leaching solution. L'invention concerne un procédé permettant de récupérer du nickel et probablement du cobalt par lixiviation d'un minerai de latérite contenant du nickel. On broie, dans une broyeuse par frottement, de la latérite contenant du nickel écrasé et probablement pré-broyé à une taille appropriée à la lixiviation. Puis, on peut lixivier la latérite moulue avec un liquide de lixiviation, par exemple, un acide sulfurique, un acide chlorhydrique ou un acide sulfurique ajoutée à SO2, à des températures relativement basses, le nickel et le cobalt pouvant être récupérés à partir de la solution de lixiviation.</description><edition>7</edition><language>eng ; fre</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030116&amp;DB=EPODOC&amp;CC=WO&amp;NR=03004709A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030116&amp;DB=EPODOC&amp;CC=WO&amp;NR=03004709A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KARPALE, KAUKO</creatorcontrib><creatorcontrib>AALTONEN, ANTTI</creatorcontrib><creatorcontrib>MALMSTROEM, ROLF</creatorcontrib><title>METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE</title><description>A method in recovering nickel and possibly cobalt through leaching from inckel-containing laterite ore. Crushed and possibly pre-ground nickel-containing laterite ore is ground in an attritor mill into a size which is suitable for leaching. Then laterite ore in an attritor mill can be leached with leaching liquid , e.g. sulphuric acid, hydrochloric acid, or sulphuric acid + SO2, at relatively low temperatures. Nickel and possibly cobalt are recovered from the leaching solution. L'invention concerne un procédé permettant de récupérer du nickel et probablement du cobalt par lixiviation d'un minerai de latérite contenant du nickel. On broie, dans une broyeuse par frottement, de la latérite contenant du nickel écrasé et probablement pré-broyé à une taille appropriée à la lixiviation. Puis, on peut lixivier la latérite moulue avec un liquide de lixiviation, par exemple, un acide sulfurique, un acide chlorhydrique ou un acide sulfurique ajoutée à SO2, à des températures relativement basses, le nickel et le cobalt pouvant être récupérés à partir de la solution de lixiviation.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzMEKgkAQgGEvHaJ6h-kBhA2D6DiuYy6tM7BMlieR2k5Rgr0_FfgAnf7Lxz9PbjVpJQWUEiCQlYaC4wOws0fygFwANcR6Qu9bsJKjV8hboIsGtOqEoQxSTz61woqOfweP-l0pgQRaJrN7_xjjauoiWZektkrj8OriOPTX-Izv7iwmM2a7M3vcZP-YD1NaNKU</recordid><startdate>20030116</startdate><enddate>20030116</enddate><creator>KARPALE, KAUKO</creator><creator>AALTONEN, ANTTI</creator><creator>MALMSTROEM, ROLF</creator><scope>EVB</scope></search><sort><creationdate>20030116</creationdate><title>METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE</title><author>KARPALE, KAUKO ; AALTONEN, ANTTI ; MALMSTROEM, ROLF</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_WO03004709A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>2003</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KARPALE, KAUKO</creatorcontrib><creatorcontrib>AALTONEN, ANTTI</creatorcontrib><creatorcontrib>MALMSTROEM, ROLF</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KARPALE, KAUKO</au><au>AALTONEN, ANTTI</au><au>MALMSTROEM, ROLF</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE</title><date>2003-01-16</date><risdate>2003</risdate><abstract>A method in recovering nickel and possibly cobalt through leaching from inckel-containing laterite ore. Crushed and possibly pre-ground nickel-containing laterite ore is ground in an attritor mill into a size which is suitable for leaching. Then laterite ore in an attritor mill can be leached with leaching liquid , e.g. sulphuric acid, hydrochloric acid, or sulphuric acid + SO2, at relatively low temperatures. Nickel and possibly cobalt are recovered from the leaching solution. L'invention concerne un procédé permettant de récupérer du nickel et probablement du cobalt par lixiviation d'un minerai de latérite contenant du nickel. On broie, dans une broyeuse par frottement, de la latérite contenant du nickel écrasé et probablement pré-broyé à une taille appropriée à la lixiviation. Puis, on peut lixivier la latérite moulue avec un liquide de lixiviation, par exemple, un acide sulfurique, un acide chlorhydrique ou un acide sulfurique ajoutée à SO2, à des températures relativement basses, le nickel et le cobalt pouvant être récupérés à partir de la solution de lixiviation.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_WO03004709A1
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR RECOVERING NICKEL AND EVENTUALLY COBALT BY EXTRACTION FROM NICKEL-CONTAINING LATERITE ORE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T19%3A03%3A32IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KARPALE,%20KAUKO&rft.date=2003-01-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EWO03004709A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true