Polybutadiene

The present invention provides a polybutadiene having improved workability and abrasion resistance. A polybutadiene according to the present invention has: (A) a Mooney viscosity (ML1+4,100° C.) being 43 or more; (B) a ratio (Tcp/ML1+4,100° C.) of 5 wt % toluene solution viscosity (Tcp) to Mooney vi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Ambe Mitsuharu, Shoda Takeshi, Kanou Yuuto
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Ambe Mitsuharu
Shoda Takeshi
Kanou Yuuto
description The present invention provides a polybutadiene having improved workability and abrasion resistance. A polybutadiene according to the present invention has: (A) a Mooney viscosity (ML1+4,100° C.) being 43 or more; (B) a ratio (Tcp/ML1+4,100° C.) of 5 wt % toluene solution viscosity (Tcp) to Mooney viscosity (ML1+4,100° C.) being 0.9 to 2.3; (C) a stress relaxation time (T80) being 10.0 to 40.0 seconds, which is a time until a torque is attenuated by 80% when the torque at the end of ML1+4,100° C.measurement is 100%; and (D) a molecular weight distribution (Mw/Mn) being 2.50 to 4.00.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US9676881B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US9676881B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US9676881B23</originalsourceid><addsrcrecordid>eNrjZOANyM-pTCotSUzJTM1L5WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFiclARSXxocGWZuZmFhaGTkbGRCgBABauHjU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polybutadiene</title><source>esp@cenet</source><creator>Ambe Mitsuharu ; Shoda Takeshi ; Kanou Yuuto</creator><creatorcontrib>Ambe Mitsuharu ; Shoda Takeshi ; Kanou Yuuto</creatorcontrib><description>The present invention provides a polybutadiene having improved workability and abrasion resistance. A polybutadiene according to the present invention has: (A) a Mooney viscosity (ML1+4,100° C.) being 43 or more; (B) a ratio (Tcp/ML1+4,100° C.) of 5 wt % toluene solution viscosity (Tcp) to Mooney viscosity (ML1+4,100° C.) being 0.9 to 2.3; (C) a stress relaxation time (T80) being 10.0 to 40.0 seconds, which is a time until a torque is attenuated by 80% when the torque at the end of ML1+4,100° C.measurement is 100%; and (D) a molecular weight distribution (Mw/Mn) being 2.50 to 4.00.</description><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170613&amp;DB=EPODOC&amp;CC=US&amp;NR=9676881B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170613&amp;DB=EPODOC&amp;CC=US&amp;NR=9676881B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Ambe Mitsuharu</creatorcontrib><creatorcontrib>Shoda Takeshi</creatorcontrib><creatorcontrib>Kanou Yuuto</creatorcontrib><title>Polybutadiene</title><description>The present invention provides a polybutadiene having improved workability and abrasion resistance. A polybutadiene according to the present invention has: (A) a Mooney viscosity (ML1+4,100° C.) being 43 or more; (B) a ratio (Tcp/ML1+4,100° C.) of 5 wt % toluene solution viscosity (Tcp) to Mooney viscosity (ML1+4,100° C.) being 0.9 to 2.3; (C) a stress relaxation time (T80) being 10.0 to 40.0 seconds, which is a time until a torque is attenuated by 80% when the torque at the end of ML1+4,100° C.measurement is 100%; and (D) a molecular weight distribution (Mw/Mn) being 2.50 to 4.00.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOANyM-pTCotSUzJTM1L5WFgTUvMKU7lhdLcDApuriHOHrqpBfnxqcUFiclARSXxocGWZuZmFhaGTkbGRCgBABauHjU</recordid><startdate>20170613</startdate><enddate>20170613</enddate><creator>Ambe Mitsuharu</creator><creator>Shoda Takeshi</creator><creator>Kanou Yuuto</creator><scope>EVB</scope></search><sort><creationdate>20170613</creationdate><title>Polybutadiene</title><author>Ambe Mitsuharu ; Shoda Takeshi ; Kanou Yuuto</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US9676881B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2017</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>Ambe Mitsuharu</creatorcontrib><creatorcontrib>Shoda Takeshi</creatorcontrib><creatorcontrib>Kanou Yuuto</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Ambe Mitsuharu</au><au>Shoda Takeshi</au><au>Kanou Yuuto</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polybutadiene</title><date>2017-06-13</date><risdate>2017</risdate><abstract>The present invention provides a polybutadiene having improved workability and abrasion resistance. A polybutadiene according to the present invention has: (A) a Mooney viscosity (ML1+4,100° C.) being 43 or more; (B) a ratio (Tcp/ML1+4,100° C.) of 5 wt % toluene solution viscosity (Tcp) to Mooney viscosity (ML1+4,100° C.) being 0.9 to 2.3; (C) a stress relaxation time (T80) being 10.0 to 40.0 seconds, which is a time until a torque is attenuated by 80% when the torque at the end of ML1+4,100° C.measurement is 100%; and (D) a molecular weight distribution (Mw/Mn) being 2.50 to 4.00.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US9676881B2
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Polybutadiene
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T09%3A03%3A53IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Ambe%20Mitsuharu&rft.date=2017-06-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS9676881B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true