Process for obtaining carbon black powder with reduced sulfur content

The present disclosure relates to a process for obtaining carbon black powder with a sulfur content of less than 0.07%. The process includes step of reacting carbon black powder with a sulfur content of 1-2% with an alkali metal or salt thereof, in a fluid media, at a temperature in the range of 100...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Gupta Shobhit, Chavan Sandeep Vasant, Kini Harshad Ravindra
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Gupta Shobhit
Chavan Sandeep Vasant
Kini Harshad Ravindra
description The present disclosure relates to a process for obtaining carbon black powder with a sulfur content of less than 0.07%. The process includes step of reacting carbon black powder with a sulfur content of 1-2% with an alkali metal or salt thereof, in a fluid media, at a temperature in the range of 100° C. to 350° C. and pressure in the range of 10 to 500 psig. It is found that in accordance with the process of the present disclosure, the sulfur content was reduced substantially from that of about 1.25% to that of 0.05%, resulting in about 96% desulfurization.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US9410042B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US9410042B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US9410042B23</originalsourceid><addsrcrecordid>eNqNyjEOwjAMAMAsDAj4gz-AVEoXVlARIxIwV4nj0IjIjpxE_T4LD2C65dZmvKsglQJBFMRVGznyG9CqEwaXLH4gy-JJYYl1BiXfkDyUlkJTQOFKXLdmFWwqtPu5MXAdn5fbnrJMVLJFYqrT63EaDl039Of--Ef5AqZTMx4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for obtaining carbon black powder with reduced sulfur content</title><source>esp@cenet</source><creator>Gupta Shobhit ; Chavan Sandeep Vasant ; Kini Harshad Ravindra</creator><creatorcontrib>Gupta Shobhit ; Chavan Sandeep Vasant ; Kini Harshad Ravindra</creatorcontrib><description>The present disclosure relates to a process for obtaining carbon black powder with a sulfur content of less than 0.07%. The process includes step of reacting carbon black powder with a sulfur content of 1-2% with an alkali metal or salt thereof, in a fluid media, at a temperature in the range of 100° C. to 350° C. and pressure in the range of 10 to 500 psig. It is found that in accordance with the process of the present disclosure, the sulfur content was reduced substantially from that of about 1.25% to that of 0.05%, resulting in about 96% desulfurization.</description><language>eng</language><subject>ADHESIVES ; CHEMISTRY ; DYES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; POLISHES ; PREPARATION OF CARBON BLACK ; TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160809&amp;DB=EPODOC&amp;CC=US&amp;NR=9410042B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25547,76298</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160809&amp;DB=EPODOC&amp;CC=US&amp;NR=9410042B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Gupta Shobhit</creatorcontrib><creatorcontrib>Chavan Sandeep Vasant</creatorcontrib><creatorcontrib>Kini Harshad Ravindra</creatorcontrib><title>Process for obtaining carbon black powder with reduced sulfur content</title><description>The present disclosure relates to a process for obtaining carbon black powder with a sulfur content of less than 0.07%. The process includes step of reacting carbon black powder with a sulfur content of 1-2% with an alkali metal or salt thereof, in a fluid media, at a temperature in the range of 100° C. to 350° C. and pressure in the range of 10 to 500 psig. It is found that in accordance with the process of the present disclosure, the sulfur content was reduced substantially from that of about 1.25% to that of 0.05%, resulting in about 96% desulfurization.</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>PREPARATION OF CARBON BLACK</subject><subject>TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOwjAMAMAsDAj4gz-AVEoXVlARIxIwV4nj0IjIjpxE_T4LD2C65dZmvKsglQJBFMRVGznyG9CqEwaXLH4gy-JJYYl1BiXfkDyUlkJTQOFKXLdmFWwqtPu5MXAdn5fbnrJMVLJFYqrT63EaDl039Of--Ef5AqZTMx4</recordid><startdate>20160809</startdate><enddate>20160809</enddate><creator>Gupta Shobhit</creator><creator>Chavan Sandeep Vasant</creator><creator>Kini Harshad Ravindra</creator><scope>EVB</scope></search><sort><creationdate>20160809</creationdate><title>Process for obtaining carbon black powder with reduced sulfur content</title><author>Gupta Shobhit ; Chavan Sandeep Vasant ; Kini Harshad Ravindra</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US9410042B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2016</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>PREPARATION OF CARBON BLACK</topic><topic>TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES</topic><toplevel>online_resources</toplevel><creatorcontrib>Gupta Shobhit</creatorcontrib><creatorcontrib>Chavan Sandeep Vasant</creatorcontrib><creatorcontrib>Kini Harshad Ravindra</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Gupta Shobhit</au><au>Chavan Sandeep Vasant</au><au>Kini Harshad Ravindra</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for obtaining carbon black powder with reduced sulfur content</title><date>2016-08-09</date><risdate>2016</risdate><abstract>The present disclosure relates to a process for obtaining carbon black powder with a sulfur content of less than 0.07%. The process includes step of reacting carbon black powder with a sulfur content of 1-2% with an alkali metal or salt thereof, in a fluid media, at a temperature in the range of 100° C. to 350° C. and pressure in the range of 10 to 500 psig. It is found that in accordance with the process of the present disclosure, the sulfur content was reduced substantially from that of about 1.25% to that of 0.05%, resulting in about 96% desulfurization.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US9410042B2
source esp@cenet
subjects ADHESIVES
CHEMISTRY
DYES
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
PAINTS
POLISHES
PREPARATION OF CARBON BLACK
TREATMENT OF INORGANIC MATERIALS, OTHER THAN FIBROUS FILLERS,TO ENHANCE THEIR PIGMENTING OR FILLING PROPERTIES
title Process for obtaining carbon black powder with reduced sulfur content
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T14%3A28%3A46IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Gupta%20Shobhit&rft.date=2016-08-09&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS9410042B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true