Method of making updoped cladding by using silicon tertrachloride as the dopant
One embodiment of the disclosure relates to a method of making an optical fiber comprising the steps of: (i) exposing a silica based preform with at least one porous glass region having soot density of to a gas mixture comprising SiCl4 having SiCl4 mole fraction ySiCl4 at a doping temperature Tdop s...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HARPER BRIAN LEE KHRAPKO ROSTISLAV RADIYEVICH RANEY SONYA MARIE MISHRA SNIGDHARAJ KUMAR TANDON PUSHKAR |
description | One embodiment of the disclosure relates to a method of making an optical fiber comprising the steps of: (i) exposing a silica based preform with at least one porous glass region having soot density of to a gas mixture comprising SiCl4 having SiCl4 mole fraction ySiCl4 at a doping temperature Tdop such that parameter X is larger than 0.03 to form the chlorine treated preform, wherein X = 1 1 + [ ( s - ) 0.209748 T dop Exp [ - 5435.33 / T dop ] y SiCl 4 3 / 4 ] and s is the density of the fully densified soot layer; and (ii) exposing the chlorine treated preform to temperatures above 1400° C. to completely sinter the preform to produce sintered optical fiber preform with a chlorine doped region; and (iii) drawing an optical fiber from the sintered optical preform. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US9290405B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US9290405B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US9290405B23</originalsourceid><addsrcrecordid>eNrjZPD3TS3JyE9RyE9TyE3MzsxLVygtSMkvSE1RSM5JTEkBCSRVKpQWgxjFmTmZyfl5CiWpRSVFickZOflFmSmpConFCiUZqQpAXYl5JTwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JD402NLI0sDEwNTJyJgIJQDfFDaf</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of making updoped cladding by using silicon tertrachloride as the dopant</title><source>esp@cenet</source><creator>HARPER BRIAN LEE ; KHRAPKO ROSTISLAV RADIYEVICH ; RANEY SONYA MARIE ; MISHRA SNIGDHARAJ KUMAR ; TANDON PUSHKAR</creator><creatorcontrib>HARPER BRIAN LEE ; KHRAPKO ROSTISLAV RADIYEVICH ; RANEY SONYA MARIE ; MISHRA SNIGDHARAJ KUMAR ; TANDON PUSHKAR</creatorcontrib><description>One embodiment of the disclosure relates to a method of making an optical fiber comprising the steps of: (i) exposing a silica based preform with at least one porous glass region having soot density of to a gas mixture comprising SiCl4 having SiCl4 mole fraction ySiCl4 at a doping temperature Tdop such that parameter X is larger than 0.03 to form the chlorine treated preform, wherein X = 1 1 + [ ( s - ) 0.209748 T dop Exp [ - 5435.33 / T dop ] y SiCl 4 3 / 4 ] and s is the density of the fully densified soot layer; and (ii) exposing the chlorine treated preform to temperatures above 1400° C. to completely sinter the preform to produce sintered optical fiber preform with a chlorine doped region; and (iii) drawing an optical fiber from the sintered optical preform.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160322&DB=EPODOC&CC=US&NR=9290405B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20160322&DB=EPODOC&CC=US&NR=9290405B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HARPER BRIAN LEE</creatorcontrib><creatorcontrib>KHRAPKO ROSTISLAV RADIYEVICH</creatorcontrib><creatorcontrib>RANEY SONYA MARIE</creatorcontrib><creatorcontrib>MISHRA SNIGDHARAJ KUMAR</creatorcontrib><creatorcontrib>TANDON PUSHKAR</creatorcontrib><title>Method of making updoped cladding by using silicon tertrachloride as the dopant</title><description>One embodiment of the disclosure relates to a method of making an optical fiber comprising the steps of: (i) exposing a silica based preform with at least one porous glass region having soot density of to a gas mixture comprising SiCl4 having SiCl4 mole fraction ySiCl4 at a doping temperature Tdop such that parameter X is larger than 0.03 to form the chlorine treated preform, wherein X = 1 1 + [ ( s - ) 0.209748 T dop Exp [ - 5435.33 / T dop ] y SiCl 4 3 / 4 ] and s is the density of the fully densified soot layer; and (ii) exposing the chlorine treated preform to temperatures above 1400° C. to completely sinter the preform to produce sintered optical fiber preform with a chlorine doped region; and (iii) drawing an optical fiber from the sintered optical preform.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPD3TS3JyE9RyE9TyE3MzsxLVygtSMkvSE1RSM5JTEkBCSRVKpQWgxjFmTmZyfl5CiWpRSVFickZOflFmSmpConFCiUZqQpAXYl5JTwMrGmJOcWpvFCam0HBzTXE2UM3tSA_PrW4IDE5NS-1JD402NLI0sDEwNTJyJgIJQDfFDaf</recordid><startdate>20160322</startdate><enddate>20160322</enddate><creator>HARPER BRIAN LEE</creator><creator>KHRAPKO ROSTISLAV RADIYEVICH</creator><creator>RANEY SONYA MARIE</creator><creator>MISHRA SNIGDHARAJ KUMAR</creator><creator>TANDON PUSHKAR</creator><scope>EVB</scope></search><sort><creationdate>20160322</creationdate><title>Method of making updoped cladding by using silicon tertrachloride as the dopant</title><author>HARPER BRIAN LEE ; KHRAPKO ROSTISLAV RADIYEVICH ; RANEY SONYA MARIE ; MISHRA SNIGDHARAJ KUMAR ; TANDON PUSHKAR</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US9290405B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2016</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>HARPER BRIAN LEE</creatorcontrib><creatorcontrib>KHRAPKO ROSTISLAV RADIYEVICH</creatorcontrib><creatorcontrib>RANEY SONYA MARIE</creatorcontrib><creatorcontrib>MISHRA SNIGDHARAJ KUMAR</creatorcontrib><creatorcontrib>TANDON PUSHKAR</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HARPER BRIAN LEE</au><au>KHRAPKO ROSTISLAV RADIYEVICH</au><au>RANEY SONYA MARIE</au><au>MISHRA SNIGDHARAJ KUMAR</au><au>TANDON PUSHKAR</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of making updoped cladding by using silicon tertrachloride as the dopant</title><date>2016-03-22</date><risdate>2016</risdate><abstract>One embodiment of the disclosure relates to a method of making an optical fiber comprising the steps of: (i) exposing a silica based preform with at least one porous glass region having soot density of to a gas mixture comprising SiCl4 having SiCl4 mole fraction ySiCl4 at a doping temperature Tdop such that parameter X is larger than 0.03 to form the chlorine treated preform, wherein X = 1 1 + [ ( s - ) 0.209748 T dop Exp [ - 5435.33 / T dop ] y SiCl 4 3 / 4 ] and s is the density of the fully densified soot layer; and (ii) exposing the chlorine treated preform to temperatures above 1400° C. to completely sinter the preform to produce sintered optical fiber preform with a chlorine doped region; and (iii) drawing an optical fiber from the sintered optical preform.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US9290405B2 |
source | esp@cenet |
subjects | CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES METALLURGY MINERAL OR SLAG WOOL SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS |
title | Method of making updoped cladding by using silicon tertrachloride as the dopant |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T20%3A18%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HARPER%20BRIAN%20LEE&rft.date=2016-03-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS9290405B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |