Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials
The present application relates to a process for the preparation of compounds of general formula (I) Lia-bM1bFe1-cM2cPd-eM3eOx (I), wherein M1, M2, M3, a, b, c, d, e and x: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8-1.9, b: 0-0.3, c: 0-0.9, d: 0.8-1.9, e: 0-0.5, x...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ROBERTS BRIAN LAMPERT JORDAN KEITH BRAMNIK KIRILL HIBST HARTMUT |
description | The present application relates to a process for the preparation of compounds of general formula (I) Lia-bM1bFe1-cM2cPd-eM3eOx (I), wherein M1, M2, M3, a, b, c, d, e and x: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8-1.9, b: 0-0.3, c: 0-0.9, d: 0.8-1.9, e: 0-0.5, x: 1.0-8, depending on the amount and oxidation state of Li, M1, Fe, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing an essentially aqueous mixture comprising at least one lithium-comprising compound, FeOOH as iron-comprising compound and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, at least one compound comprising at least one phosphorous atom and at least one reducing agent, (B) drying the mixture provided in step (A), in order to obtain a solid compound and (C) calcining the solid compound obtained from step (A) or (B) at a temperature of 300 to 950° C. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US9147877B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US9147877B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US9147877B23</originalsourceid><addsrcrecordid>eNqNyj0KAkEMQOFtLES9Qw7gFP7AaqsoloJayhLGrBOYnYRkLLy9Fh7A6uPBGzf3s0kkd-jFoCYCNVI0rCwFpIdob6-YMxeCzDXxawhzYJMSAMsDNIlrwkohyqDGzuUJw7eNMfu0GfVfaPZz0sDxcN2fAql05IqRCtXudtku1u2mbXfL1R_LB6HDPFo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials</title><source>esp@cenet</source><creator>ROBERTS BRIAN ; LAMPERT JORDAN KEITH ; BRAMNIK KIRILL ; HIBST HARTMUT</creator><creatorcontrib>ROBERTS BRIAN ; LAMPERT JORDAN KEITH ; BRAMNIK KIRILL ; HIBST HARTMUT</creatorcontrib><description>The present application relates to a process for the preparation of compounds of general formula (I) Lia-bM1bFe1-cM2cPd-eM3eOx (I), wherein M1, M2, M3, a, b, c, d, e and x: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8-1.9, b: 0-0.3, c: 0-0.9, d: 0.8-1.9, e: 0-0.5, x: 1.0-8, depending on the amount and oxidation state of Li, M1, Fe, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing an essentially aqueous mixture comprising at least one lithium-comprising compound, FeOOH as iron-comprising compound and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, at least one compound comprising at least one phosphorous atom and at least one reducing agent, (B) drying the mixture provided in step (A), in order to obtain a solid compound and (C) calcining the solid compound obtained from step (A) or (B) at a temperature of 300 to 950° C.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CABLES ; CHEMISTRY ; COMPOUNDS THEREOF ; CONDUCTORS ; ELECTRICITY ; INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS ; INORGANIC CHEMISTRY ; INSULATORS ; METALLURGY ; NON-METALLIC ELEMENTS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><creationdate>2015</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150929&DB=EPODOC&CC=US&NR=9147877B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20150929&DB=EPODOC&CC=US&NR=9147877B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ROBERTS BRIAN</creatorcontrib><creatorcontrib>LAMPERT JORDAN KEITH</creatorcontrib><creatorcontrib>BRAMNIK KIRILL</creatorcontrib><creatorcontrib>HIBST HARTMUT</creatorcontrib><title>Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials</title><description>The present application relates to a process for the preparation of compounds of general formula (I) Lia-bM1bFe1-cM2cPd-eM3eOx (I), wherein M1, M2, M3, a, b, c, d, e and x: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8-1.9, b: 0-0.3, c: 0-0.9, d: 0.8-1.9, e: 0-0.5, x: 1.0-8, depending on the amount and oxidation state of Li, M1, Fe, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing an essentially aqueous mixture comprising at least one lithium-comprising compound, FeOOH as iron-comprising compound and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, at least one compound comprising at least one phosphorous atom and at least one reducing agent, (B) drying the mixture provided in step (A), in order to obtain a solid compound and (C) calcining the solid compound obtained from step (A) or (B) at a temperature of 300 to 950° C.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CABLES</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>CONDUCTORS</subject><subject>ELECTRICITY</subject><subject>INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS</subject><subject>INORGANIC CHEMISTRY</subject><subject>INSULATORS</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2015</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyj0KAkEMQOFtLES9Qw7gFP7AaqsoloJayhLGrBOYnYRkLLy9Fh7A6uPBGzf3s0kkd-jFoCYCNVI0rCwFpIdob6-YMxeCzDXxawhzYJMSAMsDNIlrwkohyqDGzuUJw7eNMfu0GfVfaPZz0sDxcN2fAql05IqRCtXudtku1u2mbXfL1R_LB6HDPFo</recordid><startdate>20150929</startdate><enddate>20150929</enddate><creator>ROBERTS BRIAN</creator><creator>LAMPERT JORDAN KEITH</creator><creator>BRAMNIK KIRILL</creator><creator>HIBST HARTMUT</creator><scope>EVB</scope></search><sort><creationdate>20150929</creationdate><title>Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials</title><author>ROBERTS BRIAN ; LAMPERT JORDAN KEITH ; BRAMNIK KIRILL ; HIBST HARTMUT</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US9147877B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2015</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CABLES</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>CONDUCTORS</topic><topic>ELECTRICITY</topic><topic>INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS</topic><topic>INORGANIC CHEMISTRY</topic><topic>INSULATORS</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES</topic><toplevel>online_resources</toplevel><creatorcontrib>ROBERTS BRIAN</creatorcontrib><creatorcontrib>LAMPERT JORDAN KEITH</creatorcontrib><creatorcontrib>BRAMNIK KIRILL</creatorcontrib><creatorcontrib>HIBST HARTMUT</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ROBERTS BRIAN</au><au>LAMPERT JORDAN KEITH</au><au>BRAMNIK KIRILL</au><au>HIBST HARTMUT</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials</title><date>2015-09-29</date><risdate>2015</risdate><abstract>The present application relates to a process for the preparation of compounds of general formula (I) Lia-bM1bFe1-cM2cPd-eM3eOx (I), wherein M1, M2, M3, a, b, c, d, e and x: M1: Na, K, Rb and/or Cs, M2: Mn, Mg, Ca, Ti, Co, Ni, Cr, V, M3: Si, S, a: 0.8-1.9, b: 0-0.3, c: 0-0.9, d: 0.8-1.9, e: 0-0.5, x: 1.0-8, depending on the amount and oxidation state of Li, M1, Fe, M2, P, M3, wherein compounds of general formula (I) are neutrally charged, comprising the following steps (A) providing an essentially aqueous mixture comprising at least one lithium-comprising compound, FeOOH as iron-comprising compound and at least one M1-comprising compound, if present, and/or at least one M2-comprising compound, if present, and/or least one M3-comprising compound, if present, at least one compound comprising at least one phosphorous atom and at least one reducing agent, (B) drying the mixture provided in step (A), in order to obtain a solid compound and (C) calcining the solid compound obtained from step (A) or (B) at a temperature of 300 to 950° C.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US9147877B2 |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CABLES CHEMISTRY COMPOUNDS THEREOF CONDUCTORS ELECTRICITY INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS INORGANIC CHEMISTRY INSULATORS METALLURGY NON-METALLIC ELEMENTS PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING ORDIELECTRIC PROPERTIES |
title | Process for the preparation of crystalline lithium-, iron- and phosphate-comprising materials |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T03%3A55%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ROBERTS%20BRIAN&rft.date=2015-09-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS9147877B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |