Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition

To provide a polyolefin polymer having a polar group represented by Formula (i) produced by modifying, with a high modification ratio, a double bond in a polymer having the double bond at one terminal, both terminals, or at the inside of a polymer chain thereof that is obtained by a known method; a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUZUKI MAKOTO, NAGAI NAOSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SUZUKI MAKOTO
NAGAI NAOSHI
description To provide a polyolefin polymer having a polar group represented by Formula (i) produced by modifying, with a high modification ratio, a double bond in a polymer having the double bond at one terminal, both terminals, or at the inside of a polymer chain thereof that is obtained by a known method; a method for producing the polyolefin polymer; and a water dispersion material and a mold release agent composition each containing the polyolefin polymer, wherein, PO, A, B, D, E, d, e, M, i, j, and n are defined as in the application.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US8513362B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US8513362B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US8513362B23</originalsourceid><addsrcrecordid>eNqNTEsKwjAQ7caFqHeYA9SFLYrriuJSUNdlaCZtIMmESap4Ac9tIx7A1fu_efG-sH2xJW08hIk6EhjwYXyfJQr0wmMowVEaWIFmgSCsxi4Z9pAGEmJdAnoFT0zTWJkYSGJOXTYM2m_q2CoQsoSRAHvyCTp2gaPJT8tiptFGWv1wUcDpeDuc1xS4pRiwI0-pvV_3201d76qmqv-ofAAOHUwE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition</title><source>esp@cenet</source><creator>SUZUKI MAKOTO ; NAGAI NAOSHI</creator><creatorcontrib>SUZUKI MAKOTO ; NAGAI NAOSHI</creatorcontrib><description>To provide a polyolefin polymer having a polar group represented by Formula (i) produced by modifying, with a high modification ratio, a double bond in a polymer having the double bond at one terminal, both terminals, or at the inside of a polymer chain thereof that is obtained by a known method; a method for producing the polyolefin polymer; and a water dispersion material and a mold release agent composition each containing the polyolefin polymer, wherein, PO, A, B, D, E, d, e, M, i, j, and n are defined as in the application.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130820&amp;DB=EPODOC&amp;CC=US&amp;NR=8513362B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20130820&amp;DB=EPODOC&amp;CC=US&amp;NR=8513362B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SUZUKI MAKOTO</creatorcontrib><creatorcontrib>NAGAI NAOSHI</creatorcontrib><title>Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition</title><description>To provide a polyolefin polymer having a polar group represented by Formula (i) produced by modifying, with a high modification ratio, a double bond in a polymer having the double bond at one terminal, both terminals, or at the inside of a polymer chain thereof that is obtained by a known method; a method for producing the polyolefin polymer; and a water dispersion material and a mold release agent composition each containing the polyolefin polymer, wherein, PO, A, B, D, E, d, e, M, i, j, and n are defined as in the application.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNTEsKwjAQ7caFqHeYA9SFLYrriuJSUNdlaCZtIMmESap4Ac9tIx7A1fu_efG-sH2xJW08hIk6EhjwYXyfJQr0wmMowVEaWIFmgSCsxi4Z9pAGEmJdAnoFT0zTWJkYSGJOXTYM2m_q2CoQsoSRAHvyCTp2gaPJT8tiptFGWv1wUcDpeDuc1xS4pRiwI0-pvV_3201d76qmqv-ofAAOHUwE</recordid><startdate>20130820</startdate><enddate>20130820</enddate><creator>SUZUKI MAKOTO</creator><creator>NAGAI NAOSHI</creator><scope>EVB</scope></search><sort><creationdate>20130820</creationdate><title>Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition</title><author>SUZUKI MAKOTO ; NAGAI NAOSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US8513362B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>SUZUKI MAKOTO</creatorcontrib><creatorcontrib>NAGAI NAOSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SUZUKI MAKOTO</au><au>NAGAI NAOSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition</title><date>2013-08-20</date><risdate>2013</risdate><abstract>To provide a polyolefin polymer having a polar group represented by Formula (i) produced by modifying, with a high modification ratio, a double bond in a polymer having the double bond at one terminal, both terminals, or at the inside of a polymer chain thereof that is obtained by a known method; a method for producing the polyolefin polymer; and a water dispersion material and a mold release agent composition each containing the polyolefin polymer, wherein, PO, A, B, D, E, d, e, M, i, j, and n are defined as in the application.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US8513362B2
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Polyolefin polymer having polar group, method for production thereof, and water dispersion material and mold release agent composition
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T06%3A42%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SUZUKI%20MAKOTO&rft.date=2013-08-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS8513362B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true