Self-fluxing pellets for blast furnace and method for manufacturing the same

Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO2 mass ratio C/S is 0.8 or more and a MgO/SiO2 mass ratio M/S is 0.4 or more; when an iron content (mass %) in the entire pellet is represented by % TFe, % TFe is 65% or less; and a temperature Ts (unit: ° C.) at w...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YASUDA EISAKU, HASEGAWA NOBUHIRO, KITAYAMA SHUJI, MATSUI YOSHIYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YASUDA EISAKU
HASEGAWA NOBUHIRO
KITAYAMA SHUJI
MATSUI YOSHIYUKI
description Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO2 mass ratio C/S is 0.8 or more and a MgO/SiO2 mass ratio M/S is 0.4 or more; when an iron content (mass %) in the entire pellet is represented by % TFe, % TFe is 65% or less; and a temperature Ts (unit: ° C.) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test and which is calculated by the equation below is 1290° C. or higher: Ts=110×C/S+100×M/S+25×% TFe−480.  Equation:
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US8211204B2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US8211204B2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US8211204B23</originalsourceid><addsrcrecordid>eNrjZPAJTs1J003LKa3IzEtXKEjNyUktKVZIyy9SSMpJLC5RSCstyktMTlVIzEtRyE0tychPAUvmJuaVpiUml5QWgbSVZKQqFCfmpvIwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTiAqBBeakl8aHBFkaGhkYGJk5GxkQoAQAtkzVt</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Self-fluxing pellets for blast furnace and method for manufacturing the same</title><source>esp@cenet</source><creator>YASUDA EISAKU ; HASEGAWA NOBUHIRO ; KITAYAMA SHUJI ; MATSUI YOSHIYUKI</creator><creatorcontrib>YASUDA EISAKU ; HASEGAWA NOBUHIRO ; KITAYAMA SHUJI ; MATSUI YOSHIYUKI</creatorcontrib><description>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO2 mass ratio C/S is 0.8 or more and a MgO/SiO2 mass ratio M/S is 0.4 or more; when an iron content (mass %) in the entire pellet is represented by % TFe, % TFe is 65% or less; and a temperature Ts (unit: ° C.) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test and which is calculated by the equation below is 1290° C. or higher: Ts=110×C/S+100×M/S+25×% TFe−480.  Equation:</description><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120703&amp;DB=EPODOC&amp;CC=US&amp;NR=8211204B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120703&amp;DB=EPODOC&amp;CC=US&amp;NR=8211204B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YASUDA EISAKU</creatorcontrib><creatorcontrib>HASEGAWA NOBUHIRO</creatorcontrib><creatorcontrib>KITAYAMA SHUJI</creatorcontrib><creatorcontrib>MATSUI YOSHIYUKI</creatorcontrib><title>Self-fluxing pellets for blast furnace and method for manufacturing the same</title><description>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO2 mass ratio C/S is 0.8 or more and a MgO/SiO2 mass ratio M/S is 0.4 or more; when an iron content (mass %) in the entire pellet is represented by % TFe, % TFe is 65% or less; and a temperature Ts (unit: ° C.) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test and which is calculated by the equation below is 1290° C. or higher: Ts=110×C/S+100×M/S+25×% TFe−480.  Equation:</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPAJTs1J003LKa3IzEtXKEjNyUktKVZIyy9SSMpJLC5RSCstyktMTlVIzEtRyE0tychPAUvmJuaVpiUml5QWgbSVZKQqFCfmpvIwsKYl5hSn8kJpbgYFN9cQZw_d1IL8-NTiAqBBeakl8aHBFkaGhkYGJk5GxkQoAQAtkzVt</recordid><startdate>20120703</startdate><enddate>20120703</enddate><creator>YASUDA EISAKU</creator><creator>HASEGAWA NOBUHIRO</creator><creator>KITAYAMA SHUJI</creator><creator>MATSUI YOSHIYUKI</creator><scope>EVB</scope></search><sort><creationdate>20120703</creationdate><title>Self-fluxing pellets for blast furnace and method for manufacturing the same</title><author>YASUDA EISAKU ; HASEGAWA NOBUHIRO ; KITAYAMA SHUJI ; MATSUI YOSHIYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US8211204B23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>YASUDA EISAKU</creatorcontrib><creatorcontrib>HASEGAWA NOBUHIRO</creatorcontrib><creatorcontrib>KITAYAMA SHUJI</creatorcontrib><creatorcontrib>MATSUI YOSHIYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YASUDA EISAKU</au><au>HASEGAWA NOBUHIRO</au><au>KITAYAMA SHUJI</au><au>MATSUI YOSHIYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Self-fluxing pellets for blast furnace and method for manufacturing the same</title><date>2012-07-03</date><risdate>2012</risdate><abstract>Provided are self-fluxing pellets for a blast furnace, characterized in that a CaO/SiO2 mass ratio C/S is 0.8 or more and a MgO/SiO2 mass ratio M/S is 0.4 or more; when an iron content (mass %) in the entire pellet is represented by % TFe, % TFe is 65% or less; and a temperature Ts (unit: ° C.) at which the pressure loss starts to increase sharply in a loaded high-temperature reduction test and which is calculated by the equation below is 1290° C. or higher: Ts=110×C/S+100×M/S+25×% TFe−480.  Equation:</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US8211204B2
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Self-fluxing pellets for blast furnace and method for manufacturing the same
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-26T14%3A31%3A35IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YASUDA%20EISAKU&rft.date=2012-07-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS8211204B2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true