Process for preparing a moulded polyurethane material
Process for preparing a moulded elastomeric polyurethane material having an overall density of 200-1000 kg/m3, preferably of 200-500 kg/m3, and a compression load at 40% deflection of at least 25 kPa by reacting in a closed mould an isocyanate terminated prepolymer, having an NCO-value of 5-15% by w...