Process for the preparation of substantially amorphous poly-alpha-olefins

The present invention provides a process for preparing a substantially amorphous poly-alpha-olefin, which includes:a) preforming a solid catalyst and, optionally, a first amount of a trialkylaluminum cocatalyst, by contacting the catalyst and optionally the cocatalyst with at least one selected from...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SCHLUETER NORBERT, WEY HANS GUENTHER
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SCHLUETER NORBERT
WEY HANS GUENTHER
description The present invention provides a process for preparing a substantially amorphous poly-alpha-olefin, which includes:a) preforming a solid catalyst and, optionally, a first amount of a trialkylaluminum cocatalyst, by contacting the catalyst and optionally the cocatalyst with at least one selected from the group including oxygen and a compound which includes active oxygen, to form a preformed catalyst,wherein the solid catalyst includes magnesium, aluminum and titanium, andwherein said trialkylaluminum cocatalyst includes 1 to 9 carbon atoms in each alkyl group;b) contacting the preformed catalyst with a second amount of the cocatalyst, wherein a molar ratio of trialkylaluminum to the titanium ranges from 40:1 to 700:1, to form a catalyst mixture;c) polymerizing, in the liquid phase, with the catalyst mixture, an olefin or an olefin mixture at a temperature between 30 and 160° C., to produce the poly-alpha-olefin. The invention also provides a preformed catalyst for preparing a substantially amorphous poly-alpha-olefin, which is prepared the above process step (a). By the present invention, it is possible to avoid the disadvantages associated with conventional methods and prepare a substantially amorphous poly-alpha-olefin with a substantially improved space-time yield in a wide temperature range and with a more uniform course of reaction.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US6586543B1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US6586543B1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US6586543B13</originalsourceid><addsrcrecordid>eNqNyjEOwjAMAMAsDKjwB38gQ1VaMVOBYEMC5spUjhLJxFacDv09Cw9guuW27nYvMpMZBClQI4EWUixYk2SQALa8rWKuCZlXwI8UjbIYqPDqkTWiF6aQsu3cJiAb7X82Di7n53j1pDKRKc6UqU6vx9Afh_7Qndruj_IF2wU1TA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for the preparation of substantially amorphous poly-alpha-olefins</title><source>esp@cenet</source><creator>SCHLUETER NORBERT ; WEY HANS GUENTHER</creator><creatorcontrib>SCHLUETER NORBERT ; WEY HANS GUENTHER</creatorcontrib><description>The present invention provides a process for preparing a substantially amorphous poly-alpha-olefin, which includes:a) preforming a solid catalyst and, optionally, a first amount of a trialkylaluminum cocatalyst, by contacting the catalyst and optionally the cocatalyst with at least one selected from the group including oxygen and a compound which includes active oxygen, to form a preformed catalyst,wherein the solid catalyst includes magnesium, aluminum and titanium, andwherein said trialkylaluminum cocatalyst includes 1 to 9 carbon atoms in each alkyl group;b) contacting the preformed catalyst with a second amount of the cocatalyst, wherein a molar ratio of trialkylaluminum to the titanium ranges from 40:1 to 700:1, to form a catalyst mixture;c) polymerizing, in the liquid phase, with the catalyst mixture, an olefin or an olefin mixture at a temperature between 30 and 160° C., to produce the poly-alpha-olefin. The invention also provides a preformed catalyst for preparing a substantially amorphous poly-alpha-olefin, which is prepared the above process step (a). By the present invention, it is possible to avoid the disadvantages associated with conventional methods and prepare a substantially amorphous poly-alpha-olefin with a substantially improved space-time yield in a wide temperature range and with a more uniform course of reaction.</description><edition>7</edition><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2003</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030701&amp;DB=EPODOC&amp;CC=US&amp;NR=6586543B1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20030701&amp;DB=EPODOC&amp;CC=US&amp;NR=6586543B1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SCHLUETER NORBERT</creatorcontrib><creatorcontrib>WEY HANS GUENTHER</creatorcontrib><title>Process for the preparation of substantially amorphous poly-alpha-olefins</title><description>The present invention provides a process for preparing a substantially amorphous poly-alpha-olefin, which includes:a) preforming a solid catalyst and, optionally, a first amount of a trialkylaluminum cocatalyst, by contacting the catalyst and optionally the cocatalyst with at least one selected from the group including oxygen and a compound which includes active oxygen, to form a preformed catalyst,wherein the solid catalyst includes magnesium, aluminum and titanium, andwherein said trialkylaluminum cocatalyst includes 1 to 9 carbon atoms in each alkyl group;b) contacting the preformed catalyst with a second amount of the cocatalyst, wherein a molar ratio of trialkylaluminum to the titanium ranges from 40:1 to 700:1, to form a catalyst mixture;c) polymerizing, in the liquid phase, with the catalyst mixture, an olefin or an olefin mixture at a temperature between 30 and 160° C., to produce the poly-alpha-olefin. The invention also provides a preformed catalyst for preparing a substantially amorphous poly-alpha-olefin, which is prepared the above process step (a). By the present invention, it is possible to avoid the disadvantages associated with conventional methods and prepare a substantially amorphous poly-alpha-olefin with a substantially improved space-time yield in a wide temperature range and with a more uniform course of reaction.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2003</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOwjAMAMAsDKjwB38gQ1VaMVOBYEMC5spUjhLJxFacDv09Cw9guuW27nYvMpMZBClQI4EWUixYk2SQALa8rWKuCZlXwI8UjbIYqPDqkTWiF6aQsu3cJiAb7X82Di7n53j1pDKRKc6UqU6vx9Afh_7Qndruj_IF2wU1TA</recordid><startdate>20030701</startdate><enddate>20030701</enddate><creator>SCHLUETER NORBERT</creator><creator>WEY HANS GUENTHER</creator><scope>EVB</scope></search><sort><creationdate>20030701</creationdate><title>Process for the preparation of substantially amorphous poly-alpha-olefins</title><author>SCHLUETER NORBERT ; WEY HANS GUENTHER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US6586543B13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2003</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>SCHLUETER NORBERT</creatorcontrib><creatorcontrib>WEY HANS GUENTHER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SCHLUETER NORBERT</au><au>WEY HANS GUENTHER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for the preparation of substantially amorphous poly-alpha-olefins</title><date>2003-07-01</date><risdate>2003</risdate><abstract>The present invention provides a process for preparing a substantially amorphous poly-alpha-olefin, which includes:a) preforming a solid catalyst and, optionally, a first amount of a trialkylaluminum cocatalyst, by contacting the catalyst and optionally the cocatalyst with at least one selected from the group including oxygen and a compound which includes active oxygen, to form a preformed catalyst,wherein the solid catalyst includes magnesium, aluminum and titanium, andwherein said trialkylaluminum cocatalyst includes 1 to 9 carbon atoms in each alkyl group;b) contacting the preformed catalyst with a second amount of the cocatalyst, wherein a molar ratio of trialkylaluminum to the titanium ranges from 40:1 to 700:1, to form a catalyst mixture;c) polymerizing, in the liquid phase, with the catalyst mixture, an olefin or an olefin mixture at a temperature between 30 and 160° C., to produce the poly-alpha-olefin. The invention also provides a preformed catalyst for preparing a substantially amorphous poly-alpha-olefin, which is prepared the above process step (a). By the present invention, it is possible to avoid the disadvantages associated with conventional methods and prepare a substantially amorphous poly-alpha-olefin with a substantially improved space-time yield in a wide temperature range and with a more uniform course of reaction.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US6586543B1
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Process for the preparation of substantially amorphous poly-alpha-olefins
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T14%3A21%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SCHLUETER%20NORBERT&rft.date=2003-07-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS6586543B1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true