Method of making spinel compounds

The invention provides a method of making a magnesium/aluminium spinel compound having the formula Mg(1+x)Al(2+y)O4 in which 0

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: VAN ZYL, ARNOLD
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator VAN ZYL
ARNOLD
description The invention provides a method of making a magnesium/aluminium spinel compound having the formula Mg(1+x)Al(2+y)O4 in which 0
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US5525561A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US5525561A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US5525561A3</originalsourceid><addsrcrecordid>eNrjZFD0TS3JyE9RyE9TyE3MzsxLVyguyMxLzVFIzs8tyC_NSynmYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXxocGmpkampmaGjsaEVQAA7wQk_A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of making spinel compounds</title><source>esp@cenet</source><creator>VAN ZYL; ARNOLD</creator><creatorcontrib>VAN ZYL; ARNOLD</creatorcontrib><description>The invention provides a method of making a magnesium/aluminium spinel compound having the formula Mg(1+x)Al(2+y)O4 in which 0&lt;/=x&lt;/=0.2 and 0&lt;/=y&lt;/=0.35. Particulate aluminium metal and a magnesium-containing component selected from magnesium oxide and precursors thereof are mixed together and heated to 800 DEG -1150 DEG C. in an oxidising environment to cause oxidation of at least part of the aluminium. Further heating then takes place to a temperature of 1150 DEG -1350 DEG C. in the oxidizing environment to cause aluminium oxide and magnesium oxide in the admixture to react together.</description><edition>6</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; CONCRETE ; INORGANIC CHEMISTRY ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960611&amp;DB=EPODOC&amp;CC=US&amp;NR=5525561A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960611&amp;DB=EPODOC&amp;CC=US&amp;NR=5525561A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>VAN ZYL; ARNOLD</creatorcontrib><title>Method of making spinel compounds</title><description>The invention provides a method of making a magnesium/aluminium spinel compound having the formula Mg(1+x)Al(2+y)O4 in which 0&lt;/=x&lt;/=0.2 and 0&lt;/=y&lt;/=0.35. Particulate aluminium metal and a magnesium-containing component selected from magnesium oxide and precursors thereof are mixed together and heated to 800 DEG -1150 DEG C. in an oxidising environment to cause oxidation of at least part of the aluminium. Further heating then takes place to a temperature of 1150 DEG -1350 DEG C. in the oxidizing environment to cause aluminium oxide and magnesium oxide in the admixture to react together.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>CONCRETE</subject><subject>INORGANIC CHEMISTRY</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD0TS3JyE9RyE9TyE3MzsxLVyguyMxLzVFIzs8tyC_NSynmYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXxocGmpkampmaGjsaEVQAA7wQk_A</recordid><startdate>19960611</startdate><enddate>19960611</enddate><creator>VAN ZYL; ARNOLD</creator><scope>EVB</scope></search><sort><creationdate>19960611</creationdate><title>Method of making spinel compounds</title><author>VAN ZYL; ARNOLD</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US5525561A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1996</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>CONCRETE</topic><topic>INORGANIC CHEMISTRY</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>VAN ZYL; ARNOLD</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>VAN ZYL; ARNOLD</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of making spinel compounds</title><date>1996-06-11</date><risdate>1996</risdate><abstract>The invention provides a method of making a magnesium/aluminium spinel compound having the formula Mg(1+x)Al(2+y)O4 in which 0&lt;/=x&lt;/=0.2 and 0&lt;/=y&lt;/=0.35. Particulate aluminium metal and a magnesium-containing component selected from magnesium oxide and precursors thereof are mixed together and heated to 800 DEG -1150 DEG C. in an oxidising environment to cause oxidation of at least part of the aluminium. Further heating then takes place to a temperature of 1150 DEG -1350 DEG C. in the oxidizing environment to cause aluminium oxide and magnesium oxide in the admixture to react together.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US5525561A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
CONCRETE
INORGANIC CHEMISTRY
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Method of making spinel compounds
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T05%3A28%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=VAN%20ZYL;%20ARNOLD&rft.date=1996-06-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS5525561A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true