Welding electrodes for producing low carbon bainitic ferrite weld deposits

Welding electrodes useful for gas metal-arc welding of low carbon steels such as HSLA and HY steels are provided. Those welding electrodes have a carbon content of up to about 0.05 weight percent, and form weld deposits with a low carbon bainitic ferrite microstructure and yield strength in excess o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FIORE, SUSAN R, COLDREN, A. PHILLIP, SMITH, RONALD B
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator FIORE
SUSAN R
COLDREN
A. PHILLIP
SMITH
RONALD B
description Welding electrodes useful for gas metal-arc welding of low carbon steels such as HSLA and HY steels are provided. Those welding electrodes have a carbon content of up to about 0.05 weight percent, and form weld deposits with a low carbon bainitic ferrite microstructure and yield strength in excess of 80 ksi. More particularly, the welding electrodes have the following elemental composition ranges: 0.01 to 0.05 wt. % carbon, 0.7 to 1.8 wt. % manganese, 0.2 to 0.4 wt. % silicon, 1.0 to 9.0 wt. % nickel, up to 0.8 wt. % chromium, 0.4 to 1.5 wt. % molybdenum, up to 1.0 wt. % copper, up to 0.03 wt. % titanium, and up to 0.035 wt. % aluminum. The weld deposits resulting from those welding electrodes resist hydrogen induced cracking and may be used for welding naval hull materials without substantial preheating.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US5523540A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US5523540A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US5523540A3</originalsourceid><addsrcrecordid>eNrjZPAKT81JycxLV0jNSU0uKcpPSS1WSMsvUigAMkuTQRI5-eUKyYlFSfl5CkmJmXmZJZnJCmmpRUWZJakK5UDNCimpBfnFmSXFPAysaYk5xam8UJqbQd7NNcTZQxcoH59aXJCYnJqXWhIfGmxqamRsamLgaExYBQCAQjTD</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Welding electrodes for producing low carbon bainitic ferrite weld deposits</title><source>esp@cenet</source><creator>FIORE; SUSAN R ; COLDREN; A. PHILLIP ; SMITH; RONALD B</creator><creatorcontrib>FIORE; SUSAN R ; COLDREN; A. PHILLIP ; SMITH; RONALD B</creatorcontrib><description>Welding electrodes useful for gas metal-arc welding of low carbon steels such as HSLA and HY steels are provided. Those welding electrodes have a carbon content of up to about 0.05 weight percent, and form weld deposits with a low carbon bainitic ferrite microstructure and yield strength in excess of 80 ksi. More particularly, the welding electrodes have the following elemental composition ranges: 0.01 to 0.05 wt. % carbon, 0.7 to 1.8 wt. % manganese, 0.2 to 0.4 wt. % silicon, 1.0 to 9.0 wt. % nickel, up to 0.8 wt. % chromium, 0.4 to 1.5 wt. % molybdenum, up to 1.0 wt. % copper, up to 0.03 wt. % titanium, and up to 0.035 wt. % aluminum. The weld deposits resulting from those welding electrodes resist hydrogen induced cracking and may be used for welding naval hull materials without substantial preheating.</description><edition>6</edition><language>eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>1996</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960604&amp;DB=EPODOC&amp;CC=US&amp;NR=5523540A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19960604&amp;DB=EPODOC&amp;CC=US&amp;NR=5523540A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FIORE; SUSAN R</creatorcontrib><creatorcontrib>COLDREN; A. PHILLIP</creatorcontrib><creatorcontrib>SMITH; RONALD B</creatorcontrib><title>Welding electrodes for producing low carbon bainitic ferrite weld deposits</title><description>Welding electrodes useful for gas metal-arc welding of low carbon steels such as HSLA and HY steels are provided. Those welding electrodes have a carbon content of up to about 0.05 weight percent, and form weld deposits with a low carbon bainitic ferrite microstructure and yield strength in excess of 80 ksi. More particularly, the welding electrodes have the following elemental composition ranges: 0.01 to 0.05 wt. % carbon, 0.7 to 1.8 wt. % manganese, 0.2 to 0.4 wt. % silicon, 1.0 to 9.0 wt. % nickel, up to 0.8 wt. % chromium, 0.4 to 1.5 wt. % molybdenum, up to 1.0 wt. % copper, up to 0.03 wt. % titanium, and up to 0.035 wt. % aluminum. The weld deposits resulting from those welding electrodes resist hydrogen induced cracking and may be used for welding naval hull materials without substantial preheating.</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1996</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPAKT81JycxLV0jNSU0uKcpPSS1WSMsvUigAMkuTQRI5-eUKyYlFSfl5CkmJmXmZJZnJCmmpRUWZJakK5UDNCimpBfnFmSXFPAysaYk5xam8UJqbQd7NNcTZQxcoH59aXJCYnJqXWhIfGmxqamRsamLgaExYBQCAQjTD</recordid><startdate>19960604</startdate><enddate>19960604</enddate><creator>FIORE; SUSAN R</creator><creator>COLDREN; A. PHILLIP</creator><creator>SMITH; RONALD B</creator><scope>EVB</scope></search><sort><creationdate>19960604</creationdate><title>Welding electrodes for producing low carbon bainitic ferrite weld deposits</title><author>FIORE; SUSAN R ; COLDREN; A. PHILLIP ; SMITH; RONALD B</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US5523540A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1996</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>FIORE; SUSAN R</creatorcontrib><creatorcontrib>COLDREN; A. PHILLIP</creatorcontrib><creatorcontrib>SMITH; RONALD B</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FIORE; SUSAN R</au><au>COLDREN; A. PHILLIP</au><au>SMITH; RONALD B</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Welding electrodes for producing low carbon bainitic ferrite weld deposits</title><date>1996-06-04</date><risdate>1996</risdate><abstract>Welding electrodes useful for gas metal-arc welding of low carbon steels such as HSLA and HY steels are provided. Those welding electrodes have a carbon content of up to about 0.05 weight percent, and form weld deposits with a low carbon bainitic ferrite microstructure and yield strength in excess of 80 ksi. More particularly, the welding electrodes have the following elemental composition ranges: 0.01 to 0.05 wt. % carbon, 0.7 to 1.8 wt. % manganese, 0.2 to 0.4 wt. % silicon, 1.0 to 9.0 wt. % nickel, up to 0.8 wt. % chromium, 0.4 to 1.5 wt. % molybdenum, up to 1.0 wt. % copper, up to 0.03 wt. % titanium, and up to 0.035 wt. % aluminum. The weld deposits resulting from those welding electrodes resist hydrogen induced cracking and may be used for welding naval hull materials without substantial preheating.</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US5523540A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Welding electrodes for producing low carbon bainitic ferrite weld deposits
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T04%3A22%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FIORE;%20SUSAN%20R&rft.date=1996-06-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS5523540A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true