Method of manufacturing a catalyst for hydration of olefins to alcohols

A method of manufacturing a catalyst for hydration of olefins to alcohols. A montmorillonite-containing clay is employed as a catalyst support for phosphoric acid, to which a fine-grained silica gel is added after a first acid treatment. The silica gel has a particle size distribution between 30 and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SOMMER, AUGUST, SCHLUETER, DIETRICH
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SOMMER
AUGUST
SCHLUETER
DIETRICH
description A method of manufacturing a catalyst for hydration of olefins to alcohols. A montmorillonite-containing clay is employed as a catalyst support for phosphoric acid, to which a fine-grained silica gel is added after a first acid treatment. The silica gel has a particle size distribution between 30 and 60 micron, a pore volume of 0.9-1.7 ml/g, and a specific surface of 200-500 sq m/g.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4808559A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4808559A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4808559A3</originalsourceid><addsrcrecordid>eNqFyrEKwjAQANAsDqJ-g_cDBUELdRSxujipcznSSxM470pyHfr3Irg7veUt3fVOFrUHDfBGmQJ6m3KSARA8GvJcDIJmiHOf0ZLKdypTSFLAFJC9RuWydouAXGjzc-W27eV5vlU0akdlRE9C1r0eh2bX1PXxtP8_PqdgM2w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of manufacturing a catalyst for hydration of olefins to alcohols</title><source>esp@cenet</source><creator>SOMMER; AUGUST ; SCHLUETER; DIETRICH</creator><creatorcontrib>SOMMER; AUGUST ; SCHLUETER; DIETRICH</creatorcontrib><description>A method of manufacturing a catalyst for hydration of olefins to alcohols. A montmorillonite-containing clay is employed as a catalyst support for phosphoric acid, to which a fine-grained silica gel is added after a first acid treatment. The silica gel has a particle size distribution between 30 and 60 micron, a pore volume of 0.9-1.7 ml/g, and a specific surface of 200-500 sq m/g.</description><edition>4</edition><language>eng</language><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS ; CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; METALLURGY ; ORGANIC CHEMISTRY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING</subject><creationdate>1989</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19890228&amp;DB=EPODOC&amp;CC=US&amp;NR=4808559A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19890228&amp;DB=EPODOC&amp;CC=US&amp;NR=4808559A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SOMMER; AUGUST</creatorcontrib><creatorcontrib>SCHLUETER; DIETRICH</creatorcontrib><title>Method of manufacturing a catalyst for hydration of olefins to alcohols</title><description>A method of manufacturing a catalyst for hydration of olefins to alcohols. A montmorillonite-containing clay is employed as a catalyst support for phosphoric acid, to which a fine-grained silica gel is added after a first acid treatment. The silica gel has a particle size distribution between 30 and 60 micron, a pore volume of 0.9-1.7 ml/g, and a specific surface of 200-500 sq m/g.</description><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS</subject><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>ORGANIC CHEMISTRY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1989</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFyrEKwjAQANAsDqJ-g_cDBUELdRSxujipcznSSxM470pyHfr3Irg7veUt3fVOFrUHDfBGmQJ6m3KSARA8GvJcDIJmiHOf0ZLKdypTSFLAFJC9RuWydouAXGjzc-W27eV5vlU0akdlRE9C1r0eh2bX1PXxtP8_PqdgM2w</recordid><startdate>19890228</startdate><enddate>19890228</enddate><creator>SOMMER; AUGUST</creator><creator>SCHLUETER; DIETRICH</creator><scope>EVB</scope></search><sort><creationdate>19890228</creationdate><title>Method of manufacturing a catalyst for hydration of olefins to alcohols</title><author>SOMMER; AUGUST ; SCHLUETER; DIETRICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4808559A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1989</creationdate><topic>ACYCLIC OR CARBOCYCLIC COMPOUNDS</topic><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>ORGANIC CHEMISTRY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>SOMMER; AUGUST</creatorcontrib><creatorcontrib>SCHLUETER; DIETRICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SOMMER; AUGUST</au><au>SCHLUETER; DIETRICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of manufacturing a catalyst for hydration of olefins to alcohols</title><date>1989-02-28</date><risdate>1989</risdate><abstract>A method of manufacturing a catalyst for hydration of olefins to alcohols. A montmorillonite-containing clay is employed as a catalyst support for phosphoric acid, to which a fine-grained silica gel is added after a first acid treatment. The silica gel has a particle size distribution between 30 and 60 micron, a pore volume of 0.9-1.7 ml/g, and a specific surface of 200-500 sq m/g.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US4808559A
source esp@cenet
subjects ACYCLIC OR CARBOCYCLIC COMPOUNDS
CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
METALLURGY
ORGANIC CHEMISTRY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
title Method of manufacturing a catalyst for hydration of olefins to alcohols
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T11%3A45%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SOMMER;%20AUGUST&rft.date=1989-02-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4808559A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true