Low foaming, high weaving efficiency polyvinyl alcohol size composition
An aqueous size composition for cotton-containing textile yarn comprising in an aqueous solution (a) 100 parts polyvinyl alcohol (b) 2-15 parts hydrophobic waxy material (c) 0.2-5 parts ethylene oxide-propylene oxide surfactant which has a surface tension between about 37 and 48 dynes/cm as a 0.1% a...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | FAMILI AMIR MARTEN FINN L |
description | An aqueous size composition for cotton-containing textile yarn comprising in an aqueous solution (a) 100 parts polyvinyl alcohol (b) 2-15 parts hydrophobic waxy material (c) 0.2-5 parts ethylene oxide-propylene oxide surfactant which has a surface tension between about 37 and 48 dynes/cm as a 0.1% aqueous solution at 25 DEG C., and a foaming number less than about 20 (ml foam/g solution) DEG F. as a 7% aqueous polyvinyl alcohol solution containing 11.4 parts hydrogenated tallow wax and 2 parts surfactant per 100 parts polyvinyl alcohol. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4797127A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4797127A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4797127A3</originalsourceid><addsrcrecordid>eNrjZHD3yS9XSMtPzM3MS9dRyMhMz1AoT00sA_IUUtPSMpMzU_OSKxUK8nMqgWKVOQqJOcn5Gfk5CsWZVakKyfm5BfnFmSWZ-Xk8DKxpiTnFqbxQmptB3s01xNlDN7UgPz61uCAxOTUvtSQ-NNjE3NLc0Mjc0ZiwCgDEKjPO</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low foaming, high weaving efficiency polyvinyl alcohol size composition</title><source>esp@cenet</source><creator>FAMILI; AMIR ; MARTEN; FINN L</creator><creatorcontrib>FAMILI; AMIR ; MARTEN; FINN L</creatorcontrib><description>An aqueous size composition for cotton-containing textile yarn comprising in an aqueous solution (a) 100 parts polyvinyl alcohol (b) 2-15 parts hydrophobic waxy material (c) 0.2-5 parts ethylene oxide-propylene oxide surfactant which has a surface tension between about 37 and 48 dynes/cm as a 0.1% aqueous solution at 25 DEG C., and a foaming number less than about 20 (ml foam/g solution) DEG F. as a 7% aqueous polyvinyl alcohol solution containing 11.4 parts hydrogenated tallow wax and 2 parts surfactant per 100 parts polyvinyl alcohol.</description><edition>4</edition><language>eng</language><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC ; GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS ; LAUNDERING ; TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION ; TECHNICAL SUBJECTS COVERED BY FORMER USPC ; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><creationdate>1989</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19890110&DB=EPODOC&CC=US&NR=4797127A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19890110&DB=EPODOC&CC=US&NR=4797127A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FAMILI; AMIR</creatorcontrib><creatorcontrib>MARTEN; FINN L</creatorcontrib><title>Low foaming, high weaving efficiency polyvinyl alcohol size composition</title><description>An aqueous size composition for cotton-containing textile yarn comprising in an aqueous solution (a) 100 parts polyvinyl alcohol (b) 2-15 parts hydrophobic waxy material (c) 0.2-5 parts ethylene oxide-propylene oxide surfactant which has a surface tension between about 37 and 48 dynes/cm as a 0.1% aqueous solution at 25 DEG C., and a foaming number less than about 20 (ml foam/g solution) DEG F. as a 7% aqueous polyvinyl alcohol solution containing 11.4 parts hydrogenated tallow wax and 2 parts surfactant per 100 parts polyvinyl alcohol.</description><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</subject><subject>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</subject><subject>LAUNDERING</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC</subject><subject>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1989</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHD3yS9XSMtPzM3MS9dRyMhMz1AoT00sA_IUUtPSMpMzU_OSKxUK8nMqgWKVOQqJOcn5Gfk5CsWZVakKyfm5BfnFmSWZ-Xk8DKxpiTnFqbxQmptB3s01xNlDN7UgPz61uCAxOTUvtSQ-NNjE3NLc0Mjc0ZiwCgDEKjPO</recordid><startdate>19890110</startdate><enddate>19890110</enddate><creator>FAMILI; AMIR</creator><creator>MARTEN; FINN L</creator><scope>EVB</scope></search><sort><creationdate>19890110</creationdate><title>Low foaming, high weaving efficiency polyvinyl alcohol size composition</title><author>FAMILI; AMIR ; MARTEN; FINN L</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4797127A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1989</creationdate><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC</topic><topic>GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS</topic><topic>LAUNDERING</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC</topic><topic>TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><toplevel>online_resources</toplevel><creatorcontrib>FAMILI; AMIR</creatorcontrib><creatorcontrib>MARTEN; FINN L</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FAMILI; AMIR</au><au>MARTEN; FINN L</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low foaming, high weaving efficiency polyvinyl alcohol size composition</title><date>1989-01-10</date><risdate>1989</risdate><abstract>An aqueous size composition for cotton-containing textile yarn comprising in an aqueous solution (a) 100 parts polyvinyl alcohol (b) 2-15 parts hydrophobic waxy material (c) 0.2-5 parts ethylene oxide-propylene oxide surfactant which has a surface tension between about 37 and 48 dynes/cm as a 0.1% aqueous solution at 25 DEG C., and a foaming number less than about 20 (ml foam/g solution) DEG F. as a 7% aqueous polyvinyl alcohol solution containing 11.4 parts hydrogenated tallow wax and 2 parts surfactant per 100 parts polyvinyl alcohol.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US4797127A |
source | esp@cenet |
subjects | FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS LAUNDERING TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION TECHNICAL SUBJECTS COVERED BY FORMER USPC TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS TEXTILES TREATMENT OF TEXTILES OR THE LIKE TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS |
title | Low foaming, high weaving efficiency polyvinyl alcohol size composition |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-20T09%3A51%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FAMILI;%20AMIR&rft.date=1989-01-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4797127A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |