Dyed wrinkle-resistant and durable-press cotton fabrics

A cellulosic fabric is treated with a crosslinking agent selected from the group consisting of: an adduct from an amide and glyoxal, an acetal derived from a dialdehyde and an aldehyde other than formaldehyde and an acidic catalyst. The catalyst and crosslinking agent is of sufficient amount and con...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: FRICK, JR., JOHN G, WATSON, MICHAEL D, STONE, ROBBIE L, JONES, BRIAN W
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A cellulosic fabric is treated with a crosslinking agent selected from the group consisting of: an adduct from an amide and glyoxal, an acetal derived from a dialdehyde and an aldehyde other than formaldehyde and an acidic catalyst. The catalyst and crosslinking agent is of sufficient amount and concentration to impregnate the fabric and produce wrinkle-resistance and smooth-drying finishes when dried from about 3-10 minutes at from about 60 DEG -100 DEG C. and then cured from about 1-5 minutes at from about 120 DEG -180 DEG C. The resultant fabric is then dyed.