Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge
Disclosed is a method of smelting ferronickel that comprises the steps of adjusting the depth of the slag bath, the depth of immersion of the electrodes thereinto and the specific power at the electrode surfaces wetted with the slag. According to this method, the depth of the slag bath is maintained...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | BUROCHKIN ALEXANDR E KADYKOV VLADIMIR A MIKSHIN VIKTOR P ERMAKOV GENNADY P MITTSEV SERGEI G LINEV VALERY D TIMOFEEV GENNADY A KELLER VIKTOR R ONISCHIN BORIS P KHRISTOFOROV VIKTOR P GRODINSKY GRIGORY I |
description | Disclosed is a method of smelting ferronickel that comprises the steps of adjusting the depth of the slag bath, the depth of immersion of the electrodes thereinto and the specific power at the electrode surfaces wetted with the slag. According to this method, the depth of the slag bath is maintained within the range of from 0.6 to 1.1 of the electrodes diameter, while the depth of immersion of the electrodes and the specific power at the electrode surfaces wetted with the slag are kept at such levels as to provide a mode approaching to the arc mode, but at the same time to that of the ferronickel bath temperature should be adequately high for the free ferronickel tapping. The depth of immersion of the electrodes into the slag bath of 0.1 to 0.25 of the electrode diameter and the specific power at the electrode surfaces wetted with the slag of 5.0 to 6.5 MW/m2 are optimal for the hereinabove mentioned mode. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4412857A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4412857A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4412857A3</originalsourceid><addsrcrecordid>eNqFjDEOwjAQBNNQIOAN3AdSAEGkRQhEQwUUVNHJWScWhx2dnYLf4wLRUk2xszMtHhekPrQULMUXJDnfkYVq8M48IeQ8BUX52yAwSZ1hITuqZwMafQslJuF3Zg6ZnrXDvJhYlojFl7NieTreDucSQ2gQh3z1SM39WlWrdb3d7Tf_jQ_11jnZ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge</title><source>esp@cenet</source><creator>BUROCHKIN; ALEXANDR E ; KADYKOV; VLADIMIR A ; MIKSHIN; VIKTOR P ; ERMAKOV; GENNADY P ; MITTSEV; SERGEI G ; LINEV; VALERY D ; TIMOFEEV; GENNADY A ; KELLER; VIKTOR R ; ONISCHIN; BORIS P ; KHRISTOFOROV; VIKTOR P ; GRODINSKY; GRIGORY I</creator><creatorcontrib>BUROCHKIN; ALEXANDR E ; KADYKOV; VLADIMIR A ; MIKSHIN; VIKTOR P ; ERMAKOV; GENNADY P ; MITTSEV; SERGEI G ; LINEV; VALERY D ; TIMOFEEV; GENNADY A ; KELLER; VIKTOR R ; ONISCHIN; BORIS P ; KHRISTOFOROV; VIKTOR P ; GRODINSKY; GRIGORY I</creatorcontrib><description>Disclosed is a method of smelting ferronickel that comprises the steps of adjusting the depth of the slag bath, the depth of immersion of the electrodes thereinto and the specific power at the electrode surfaces wetted with the slag. According to this method, the depth of the slag bath is maintained within the range of from 0.6 to 1.1 of the electrodes diameter, while the depth of immersion of the electrodes and the specific power at the electrode surfaces wetted with the slag are kept at such levels as to provide a mode approaching to the arc mode, but at the same time to that of the ferronickel bath temperature should be adequately high for the free ferronickel tapping. The depth of immersion of the electrodes into the slag bath of 0.1 to 0.25 of the electrode diameter and the specific power at the electrode surfaces wetted with the slag of 5.0 to 6.5 MW/m2 are optimal for the hereinabove mentioned mode.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1983</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19831101&DB=EPODOC&CC=US&NR=4412857A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19831101&DB=EPODOC&CC=US&NR=4412857A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BUROCHKIN; ALEXANDR E</creatorcontrib><creatorcontrib>KADYKOV; VLADIMIR A</creatorcontrib><creatorcontrib>MIKSHIN; VIKTOR P</creatorcontrib><creatorcontrib>ERMAKOV; GENNADY P</creatorcontrib><creatorcontrib>MITTSEV; SERGEI G</creatorcontrib><creatorcontrib>LINEV; VALERY D</creatorcontrib><creatorcontrib>TIMOFEEV; GENNADY A</creatorcontrib><creatorcontrib>KELLER; VIKTOR R</creatorcontrib><creatorcontrib>ONISCHIN; BORIS P</creatorcontrib><creatorcontrib>KHRISTOFOROV; VIKTOR P</creatorcontrib><creatorcontrib>GRODINSKY; GRIGORY I</creatorcontrib><title>Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge</title><description>Disclosed is a method of smelting ferronickel that comprises the steps of adjusting the depth of the slag bath, the depth of immersion of the electrodes thereinto and the specific power at the electrode surfaces wetted with the slag. According to this method, the depth of the slag bath is maintained within the range of from 0.6 to 1.1 of the electrodes diameter, while the depth of immersion of the electrodes and the specific power at the electrode surfaces wetted with the slag are kept at such levels as to provide a mode approaching to the arc mode, but at the same time to that of the ferronickel bath temperature should be adequately high for the free ferronickel tapping. The depth of immersion of the electrodes into the slag bath of 0.1 to 0.25 of the electrode diameter and the specific power at the electrode surfaces wetted with the slag of 5.0 to 6.5 MW/m2 are optimal for the hereinabove mentioned mode.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1983</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFjDEOwjAQBNNQIOAN3AdSAEGkRQhEQwUUVNHJWScWhx2dnYLf4wLRUk2xszMtHhekPrQULMUXJDnfkYVq8M48IeQ8BUX52yAwSZ1hITuqZwMafQslJuF3Zg6ZnrXDvJhYlojFl7NieTreDucSQ2gQh3z1SM39WlWrdb3d7Tf_jQ_11jnZ</recordid><startdate>19831101</startdate><enddate>19831101</enddate><creator>BUROCHKIN; ALEXANDR E</creator><creator>KADYKOV; VLADIMIR A</creator><creator>MIKSHIN; VIKTOR P</creator><creator>ERMAKOV; GENNADY P</creator><creator>MITTSEV; SERGEI G</creator><creator>LINEV; VALERY D</creator><creator>TIMOFEEV; GENNADY A</creator><creator>KELLER; VIKTOR R</creator><creator>ONISCHIN; BORIS P</creator><creator>KHRISTOFOROV; VIKTOR P</creator><creator>GRODINSKY; GRIGORY I</creator><scope>EVB</scope></search><sort><creationdate>19831101</creationdate><title>Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge</title><author>BUROCHKIN; ALEXANDR E ; KADYKOV; VLADIMIR A ; MIKSHIN; VIKTOR P ; ERMAKOV; GENNADY P ; MITTSEV; SERGEI G ; LINEV; VALERY D ; TIMOFEEV; GENNADY A ; KELLER; VIKTOR R ; ONISCHIN; BORIS P ; KHRISTOFOROV; VIKTOR P ; GRODINSKY; GRIGORY I</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4412857A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1983</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>BUROCHKIN; ALEXANDR E</creatorcontrib><creatorcontrib>KADYKOV; VLADIMIR A</creatorcontrib><creatorcontrib>MIKSHIN; VIKTOR P</creatorcontrib><creatorcontrib>ERMAKOV; GENNADY P</creatorcontrib><creatorcontrib>MITTSEV; SERGEI G</creatorcontrib><creatorcontrib>LINEV; VALERY D</creatorcontrib><creatorcontrib>TIMOFEEV; GENNADY A</creatorcontrib><creatorcontrib>KELLER; VIKTOR R</creatorcontrib><creatorcontrib>ONISCHIN; BORIS P</creatorcontrib><creatorcontrib>KHRISTOFOROV; VIKTOR P</creatorcontrib><creatorcontrib>GRODINSKY; GRIGORY I</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BUROCHKIN; ALEXANDR E</au><au>KADYKOV; VLADIMIR A</au><au>MIKSHIN; VIKTOR P</au><au>ERMAKOV; GENNADY P</au><au>MITTSEV; SERGEI G</au><au>LINEV; VALERY D</au><au>TIMOFEEV; GENNADY A</au><au>KELLER; VIKTOR R</au><au>ONISCHIN; BORIS P</au><au>KHRISTOFOROV; VIKTOR P</au><au>GRODINSKY; GRIGORY I</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge</title><date>1983-11-01</date><risdate>1983</risdate><abstract>Disclosed is a method of smelting ferronickel that comprises the steps of adjusting the depth of the slag bath, the depth of immersion of the electrodes thereinto and the specific power at the electrode surfaces wetted with the slag. According to this method, the depth of the slag bath is maintained within the range of from 0.6 to 1.1 of the electrodes diameter, while the depth of immersion of the electrodes and the specific power at the electrode surfaces wetted with the slag are kept at such levels as to provide a mode approaching to the arc mode, but at the same time to that of the ferronickel bath temperature should be adequately high for the free ferronickel tapping. The depth of immersion of the electrodes into the slag bath of 0.1 to 0.25 of the electrode diameter and the specific power at the electrode surfaces wetted with the slag of 5.0 to 6.5 MW/m2 are optimal for the hereinabove mentioned mode.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US4412857A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Method of smelting ferronickel in ore-smelting electrical furnace under a layer of charge |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-21T13%3A38%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BUROCHKIN;%20ALEXANDR%20E&rft.date=1983-11-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4412857A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |