Epoxy resins having improved physical properties when cured
Epoxy resins having improved properties are prepared by reacting an epoxy resin with a dihydric phenol in the presence of a sufficient quantity of a phosphonium catalyst such that the product resulting from reacting a mixture of the catalyst, epoxy resin and dihydric phenol has a % epoxide differenc...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | DOORAKIAN GEORGE A GIST ADOLPHUS V WHITESIDE, JR. ROSS C |
description | Epoxy resins having improved properties are prepared by reacting an epoxy resin with a dihydric phenol in the presence of a sufficient quantity of a phosphonium catalyst such that the product resulting from reacting a mixture of the catalyst, epoxy resin and dihydric phenol has a % epoxide difference from the theoretical percent epoxide of from about 0.5 to about 4.0. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4370465A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4370465A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4370465A3</originalsourceid><addsrcrecordid>eNrjZLB2LcivqFQoSi3OzCtWyEgsy8xLV8jMLSjKL0tNUSjIqCzOTE7MUQDyC1KLSjJTixXKM1LzFJJLi1JTeBhY0xJzilN5oTQ3g7yba4izh25qQX58anFBYnJqXmpJfGiwibG5gYmZqaMxYRUAQIQvYQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Epoxy resins having improved physical properties when cured</title><source>esp@cenet</source><creator>DOORAKIAN; GEORGE A ; GIST; ADOLPHUS V ; WHITESIDE, JR.; ROSS C</creator><creatorcontrib>DOORAKIAN; GEORGE A ; GIST; ADOLPHUS V ; WHITESIDE, JR.; ROSS C</creatorcontrib><description>Epoxy resins having improved properties are prepared by reacting an epoxy resin with a dihydric phenol in the presence of a sufficient quantity of a phosphonium catalyst such that the product resulting from reacting a mixture of the catalyst, epoxy resin and dihydric phenol has a % epoxide difference from the theoretical percent epoxide of from about 0.5 to about 4.0.</description><language>eng</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>1983</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19830125&DB=EPODOC&CC=US&NR=4370465A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19830125&DB=EPODOC&CC=US&NR=4370465A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DOORAKIAN; GEORGE A</creatorcontrib><creatorcontrib>GIST; ADOLPHUS V</creatorcontrib><creatorcontrib>WHITESIDE, JR.; ROSS C</creatorcontrib><title>Epoxy resins having improved physical properties when cured</title><description>Epoxy resins having improved properties are prepared by reacting an epoxy resin with a dihydric phenol in the presence of a sufficient quantity of a phosphonium catalyst such that the product resulting from reacting a mixture of the catalyst, epoxy resin and dihydric phenol has a % epoxide difference from the theoretical percent epoxide of from about 0.5 to about 4.0.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1983</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLB2LcivqFQoSi3OzCtWyEgsy8xLV8jMLSjKL0tNUSjIqCzOTE7MUQDyC1KLSjJTixXKM1LzFJJLi1JTeBhY0xJzilN5oTQ3g7yba4izh25qQX58anFBYnJqXmpJfGiwibG5gYmZqaMxYRUAQIQvYQ</recordid><startdate>19830125</startdate><enddate>19830125</enddate><creator>DOORAKIAN; GEORGE A</creator><creator>GIST; ADOLPHUS V</creator><creator>WHITESIDE, JR.; ROSS C</creator><scope>EVB</scope></search><sort><creationdate>19830125</creationdate><title>Epoxy resins having improved physical properties when cured</title><author>DOORAKIAN; GEORGE A ; GIST; ADOLPHUS V ; WHITESIDE, JR.; ROSS C</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4370465A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1983</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>DOORAKIAN; GEORGE A</creatorcontrib><creatorcontrib>GIST; ADOLPHUS V</creatorcontrib><creatorcontrib>WHITESIDE, JR.; ROSS C</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DOORAKIAN; GEORGE A</au><au>GIST; ADOLPHUS V</au><au>WHITESIDE, JR.; ROSS C</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Epoxy resins having improved physical properties when cured</title><date>1983-01-25</date><risdate>1983</risdate><abstract>Epoxy resins having improved properties are prepared by reacting an epoxy resin with a dihydric phenol in the presence of a sufficient quantity of a phosphonium catalyst such that the product resulting from reacting a mixture of the catalyst, epoxy resin and dihydric phenol has a % epoxide difference from the theoretical percent epoxide of from about 0.5 to about 4.0.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US4370465A |
source | esp@cenet |
subjects | AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G CHEMISTRY COMPOSITIONS BASED THEREON GENERAL PROCESSES OF COMPOUNDING MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP WORKING-UP |
title | Epoxy resins having improved physical properties when cured |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T03%3A32%3A56IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DOORAKIAN;%20GEORGE%20A&rft.date=1983-01-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4370465A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |