Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby

A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400 DEG C. to about 1800 DEG C. in an inert atmosphere or vacuum. Silicon carbide powde...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MORELOCK, CHARLES R, LASKOW, WILLIAM
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MORELOCK
CHARLES R
LASKOW
WILLIAM
description A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400 DEG C. to about 1800 DEG C. in an inert atmosphere or vacuum. Silicon carbide powder can also be incorporated in the preform structure.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4294788A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4294788A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4294788A3</originalsourceid><addsrcrecordid>eNqFir0KwkAQBtNYiPoM7guk0YCxFFFsrNROCJu7L7nF--PuCn17LbS2GoaZaXU_o5igKQzk-CF-JKZsOEJTFisqeFKcetGof-64JHmSCi6GLAXEXhOnIsoif6oGFYOE_jWvJgPbjMWXs2p5PFz3pxoxdMiRFTxKd7s0q22zadvd-v_xBqO1Oxk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby</title><source>esp@cenet</source><creator>MORELOCK; CHARLES R ; LASKOW; WILLIAM</creator><creatorcontrib>MORELOCK; CHARLES R ; LASKOW; WILLIAM</creatorcontrib><description>A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400 DEG C. to about 1800 DEG C. in an inert atmosphere or vacuum. Silicon carbide powder can also be incorporated in the preform structure.</description><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1981</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19811013&amp;DB=EPODOC&amp;CC=US&amp;NR=4294788A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19811013&amp;DB=EPODOC&amp;CC=US&amp;NR=4294788A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MORELOCK; CHARLES R</creatorcontrib><creatorcontrib>LASKOW; WILLIAM</creatorcontrib><title>Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby</title><description>A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400 DEG C. to about 1800 DEG C. in an inert atmosphere or vacuum. Silicon carbide powder can also be incorporated in the preform structure.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1981</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFir0KwkAQBtNYiPoM7guk0YCxFFFsrNROCJu7L7nF--PuCn17LbS2GoaZaXU_o5igKQzk-CF-JKZsOEJTFisqeFKcetGof-64JHmSCi6GLAXEXhOnIsoif6oGFYOE_jWvJgPbjMWXs2p5PFz3pxoxdMiRFTxKd7s0q22zadvd-v_xBqO1Oxk</recordid><startdate>19811013</startdate><enddate>19811013</enddate><creator>MORELOCK; CHARLES R</creator><creator>LASKOW; WILLIAM</creator><scope>EVB</scope></search><sort><creationdate>19811013</creationdate><title>Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby</title><author>MORELOCK; CHARLES R ; LASKOW; WILLIAM</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4294788A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1981</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>MORELOCK; CHARLES R</creatorcontrib><creatorcontrib>LASKOW; WILLIAM</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MORELOCK; CHARLES R</au><au>LASKOW; WILLIAM</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby</title><date>1981-10-13</date><risdate>1981</risdate><abstract>A method is described for making a shaped silicon carbide-silicon matrix composite. A confined carbon fiber preform is infiltrated with sufficient molten silicon metal at a temperature in the range of from about 1400 DEG C. to about 1800 DEG C. in an inert atmosphere or vacuum. Silicon carbide powder can also be incorporated in the preform structure.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US4294788A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Method of making a shaped silicon carbide-silicon matrix composite and articles made thereby
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-02T10%3A50%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MORELOCK;%20CHARLES%20R&rft.date=1981-10-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4294788A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true