Method of refining ferro-alloys
A ferro-alloy, namely ferrochrome or ferromanganese, is refined by being heated to at least 100 DEG C above its melting point to form a bath whereupon oxygen is blown into the melt, below the bath surface, within a protective gas envelope. The rate of oxygen blowing is so chosen that 1% of carbon is...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | STADLER FRITZ FICHTE RUDOLF BROTZMANN KARL DUDERSTADT GUNTER BREUER FRIEDRICH |
description | A ferro-alloy, namely ferrochrome or ferromanganese, is refined by being heated to at least 100 DEG C above its melting point to form a bath whereupon oxygen is blown into the melt, below the bath surface, within a protective gas envelope. The rate of oxygen blowing is so chosen that 1% of carbon is oxidized within a period not to exceed about ten minutes, preferably not more than five minutes. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4139370A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4139370A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4139370A3</originalsourceid><addsrcrecordid>eNrjZJD3TS3JyE9RyE9TKEpNy8zLzEtXSEstKsrXTczJya8s5mFgTUvMKU7lhdLcDPJuriHOHrqpBfnxqcUFicmpeakl8aHBJobGlsbmBo7GhFUAAJPiJC0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of refining ferro-alloys</title><source>esp@cenet</source><creator>STADLER; FRITZ ; FICHTE; RUDOLF ; BROTZMANN; KARL ; DUDERSTADT; GUNTER ; BREUER; FRIEDRICH</creator><creatorcontrib>STADLER; FRITZ ; FICHTE; RUDOLF ; BROTZMANN; KARL ; DUDERSTADT; GUNTER ; BREUER; FRIEDRICH</creatorcontrib><description>A ferro-alloy, namely ferrochrome or ferromanganese, is refined by being heated to at least 100 DEG C above its melting point to form a bath whereupon oxygen is blown into the melt, below the bath surface, within a protective gas envelope. The rate of oxygen blowing is so chosen that 1% of carbon is oxidized within a period not to exceed about ten minutes, preferably not more than five minutes.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1979</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19790213&DB=EPODOC&CC=US&NR=4139370A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19790213&DB=EPODOC&CC=US&NR=4139370A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STADLER; FRITZ</creatorcontrib><creatorcontrib>FICHTE; RUDOLF</creatorcontrib><creatorcontrib>BROTZMANN; KARL</creatorcontrib><creatorcontrib>DUDERSTADT; GUNTER</creatorcontrib><creatorcontrib>BREUER; FRIEDRICH</creatorcontrib><title>Method of refining ferro-alloys</title><description>A ferro-alloy, namely ferrochrome or ferromanganese, is refined by being heated to at least 100 DEG C above its melting point to form a bath whereupon oxygen is blown into the melt, below the bath surface, within a protective gas envelope. The rate of oxygen blowing is so chosen that 1% of carbon is oxidized within a period not to exceed about ten minutes, preferably not more than five minutes.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1979</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZJD3TS3JyE9RyE9TKEpNy8zLzEtXSEstKsrXTczJya8s5mFgTUvMKU7lhdLcDPJuriHOHrqpBfnxqcUFicmpeakl8aHBJobGlsbmBo7GhFUAAJPiJC0</recordid><startdate>19790213</startdate><enddate>19790213</enddate><creator>STADLER; FRITZ</creator><creator>FICHTE; RUDOLF</creator><creator>BROTZMANN; KARL</creator><creator>DUDERSTADT; GUNTER</creator><creator>BREUER; FRIEDRICH</creator><scope>EVB</scope></search><sort><creationdate>19790213</creationdate><title>Method of refining ferro-alloys</title><author>STADLER; FRITZ ; FICHTE; RUDOLF ; BROTZMANN; KARL ; DUDERSTADT; GUNTER ; BREUER; FRIEDRICH</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4139370A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1979</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>STADLER; FRITZ</creatorcontrib><creatorcontrib>FICHTE; RUDOLF</creatorcontrib><creatorcontrib>BROTZMANN; KARL</creatorcontrib><creatorcontrib>DUDERSTADT; GUNTER</creatorcontrib><creatorcontrib>BREUER; FRIEDRICH</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STADLER; FRITZ</au><au>FICHTE; RUDOLF</au><au>BROTZMANN; KARL</au><au>DUDERSTADT; GUNTER</au><au>BREUER; FRIEDRICH</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of refining ferro-alloys</title><date>1979-02-13</date><risdate>1979</risdate><abstract>A ferro-alloy, namely ferrochrome or ferromanganese, is refined by being heated to at least 100 DEG C above its melting point to form a bath whereupon oxygen is blown into the melt, below the bath surface, within a protective gas envelope. The rate of oxygen blowing is so chosen that 1% of carbon is oxidized within a period not to exceed about ten minutes, preferably not more than five minutes.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US4139370A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY METALLURGY OF IRON PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Method of refining ferro-alloys |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T16%3A03%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STADLER;%20FRITZ&rft.date=1979-02-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4139370A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |