Nickel base alloy
A gamma prime strengthened nickel base alloy having a 1650 DEG F impact strength of at least 6 ft.-lbs. after 35,000 hours exposure at 1600 DEG F. The alloy consists essentially of, by weight, from 12.0 to 20.0% chromium, from 4.75 to 7.0% titanium, from 1.3 to 3.0% aluminum, from 13.0 to 19.0% coba...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | BOESCH WILLIAM J |
description | A gamma prime strengthened nickel base alloy having a 1650 DEG F impact strength of at least 6 ft.-lbs. after 35,000 hours exposure at 1600 DEG F. The alloy consists essentially of, by weight, from 12.0 to 20.0% chromium, from 4.75 to 7.0% titanium, from 1.3 to 3.0% aluminum, from 13.0 to 19.0% cobalt, from 2.0 to 3.5% molybdenum, from 0.5 to 2.5% tungsten, from 0.005 to 0.03% boron, from 0.005 to 0.045% carbon, up to 0.75% manganese, up to 0.08% zirconium, up to 0.5% iron, up to 0.2% of rare earth elements that will not lower the incipient melting temperature below the solvus temperature of the gamma prime present in the alloy, up to 0.02% of elements from the group consisting of magnesium, calcium, strontium and barium, balance essentially nickel. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US4083734A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US4083734A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US4083734A3</originalsourceid><addsrcrecordid>eNrjZBD0y0zOTs1RSEosTlVIzMnJr-RhYE1LzClO5YXS3Azybq4hzh66qQX58anFBYnJqXmpJfGhwSYGFsbmxiaOxoRVAABBkh6u</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Nickel base alloy</title><source>esp@cenet</source><creator>BOESCH; WILLIAM J</creator><creatorcontrib>BOESCH; WILLIAM J</creatorcontrib><description>A gamma prime strengthened nickel base alloy having a 1650 DEG F impact strength of at least 6 ft.-lbs. after 35,000 hours exposure at 1600 DEG F. The alloy consists essentially of, by weight, from 12.0 to 20.0% chromium, from 4.75 to 7.0% titanium, from 1.3 to 3.0% aluminum, from 13.0 to 19.0% cobalt, from 2.0 to 3.5% molybdenum, from 0.5 to 2.5% tungsten, from 0.005 to 0.03% boron, from 0.005 to 0.045% carbon, up to 0.75% manganese, up to 0.08% zirconium, up to 0.5% iron, up to 0.2% of rare earth elements that will not lower the incipient melting temperature below the solvus temperature of the gamma prime present in the alloy, up to 0.02% of elements from the group consisting of magnesium, calcium, strontium and barium, balance essentially nickel.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1978</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19780411&DB=EPODOC&CC=US&NR=4083734A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19780411&DB=EPODOC&CC=US&NR=4083734A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BOESCH; WILLIAM J</creatorcontrib><title>Nickel base alloy</title><description>A gamma prime strengthened nickel base alloy having a 1650 DEG F impact strength of at least 6 ft.-lbs. after 35,000 hours exposure at 1600 DEG F. The alloy consists essentially of, by weight, from 12.0 to 20.0% chromium, from 4.75 to 7.0% titanium, from 1.3 to 3.0% aluminum, from 13.0 to 19.0% cobalt, from 2.0 to 3.5% molybdenum, from 0.5 to 2.5% tungsten, from 0.005 to 0.03% boron, from 0.005 to 0.045% carbon, up to 0.75% manganese, up to 0.08% zirconium, up to 0.5% iron, up to 0.2% of rare earth elements that will not lower the incipient melting temperature below the solvus temperature of the gamma prime present in the alloy, up to 0.02% of elements from the group consisting of magnesium, calcium, strontium and barium, balance essentially nickel.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1978</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBD0y0zOTs1RSEosTlVIzMnJr-RhYE1LzClO5YXS3Azybq4hzh66qQX58anFBYnJqXmpJfGhwSYGFsbmxiaOxoRVAABBkh6u</recordid><startdate>19780411</startdate><enddate>19780411</enddate><creator>BOESCH; WILLIAM J</creator><scope>EVB</scope></search><sort><creationdate>19780411</creationdate><title>Nickel base alloy</title><author>BOESCH; WILLIAM J</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US4083734A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1978</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>BOESCH; WILLIAM J</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BOESCH; WILLIAM J</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Nickel base alloy</title><date>1978-04-11</date><risdate>1978</risdate><abstract>A gamma prime strengthened nickel base alloy having a 1650 DEG F impact strength of at least 6 ft.-lbs. after 35,000 hours exposure at 1600 DEG F. The alloy consists essentially of, by weight, from 12.0 to 20.0% chromium, from 4.75 to 7.0% titanium, from 1.3 to 3.0% aluminum, from 13.0 to 19.0% cobalt, from 2.0 to 3.5% molybdenum, from 0.5 to 2.5% tungsten, from 0.005 to 0.03% boron, from 0.005 to 0.045% carbon, up to 0.75% manganese, up to 0.08% zirconium, up to 0.5% iron, up to 0.2% of rare earth elements that will not lower the incipient melting temperature below the solvus temperature of the gamma prime present in the alloy, up to 0.02% of elements from the group consisting of magnesium, calcium, strontium and barium, balance essentially nickel.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US4083734A |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Nickel base alloy |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T04%3A51%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BOESCH;%20WILLIAM%20J&rft.date=1978-04-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS4083734A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |