PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY

1277592 Germanium dioxide DEUTSCHE GOLDUND SILBER-SCHEIDEANSTALT 4 Sept 1969 [20 Sept 1968] 43879/69 Heading C1A Amorphous highly dispersed germanium dioxide is prepared by reacting a volatile tetravalent germanium compound or a sprayable solution thereof under hydrolysing or oxidizing conditions in...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DUESING G,DT, HECKEL E,DT, RENNGARDT F,DT, MEYER SIMON E,DT
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DUESING G,DT
HECKEL E,DT
RENNGARDT F,DT
MEYER SIMON E,DT
description 1277592 Germanium dioxide DEUTSCHE GOLDUND SILBER-SCHEIDEANSTALT 4 Sept 1969 [20 Sept 1968] 43879/69 Heading C1A Amorphous highly dispersed germanium dioxide is prepared by reacting a volatile tetravalent germanium compound or a sprayable solution thereof under hydrolysing or oxidizing conditions in the gas phase or as an aerosol at a temperature above 1300‹ C., allowing the germanium dioxide formed to coagulate at a temperature of from 200‹ to 1000‹ C., and separating the gaseous reaction products. The germanium compound is preferably a halide or a volatile organo-germanium compound. The reaction is preferably carried out at a temperature of from 1400‹ to 1700‹ C. using a fuel gas of high calorific value with a free oxygen containing gas or pure oxygen, the mixture being reacted after passage through a nozzle. The germanium dioxide formed is preferably coagulated and separated at a temperature of from 400‹ to 700‹ C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US3793442A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US3793442A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US3793442A3</originalsourceid><addsrcrecordid>eNqFjLsKwjAUQLM4iPoN3h9wMQVxTJPbJGge5AEtDqVInEQL9f8xg7vTgcPhrMnNB8cxRnAdGHbRVgIzLnjlcgSlpboOIHT0GCIKkBgMszqb6lyvBQKzAupCZJ7AtYlpW7OkMGA7bMnqMT2XsvtxQ_YdJq4OZX6PZZmne3mVz5gjPZ1p0xwZ_V98AdrxMZU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY</title><source>esp@cenet</source><creator>DUESING G,DT ; HECKEL E,DT ; RENNGARDT F,DT ; MEYER SIMON E,DT</creator><creatorcontrib>DUESING G,DT ; HECKEL E,DT ; RENNGARDT F,DT ; MEYER SIMON E,DT</creatorcontrib><description>1277592 Germanium dioxide DEUTSCHE GOLDUND SILBER-SCHEIDEANSTALT 4 Sept 1969 [20 Sept 1968] 43879/69 Heading C1A Amorphous highly dispersed germanium dioxide is prepared by reacting a volatile tetravalent germanium compound or a sprayable solution thereof under hydrolysing or oxidizing conditions in the gas phase or as an aerosol at a temperature above 1300‹ C., allowing the germanium dioxide formed to coagulate at a temperature of from 200‹ to 1000‹ C., and separating the gaseous reaction products. The germanium compound is preferably a halide or a volatile organo-germanium compound. The reaction is preferably carried out at a temperature of from 1400‹ to 1700‹ C. using a fuel gas of high calorific value with a free oxygen containing gas or pure oxygen, the mixture being reacted after passage through a nozzle. The germanium dioxide formed is preferably coagulated and separated at a temperature of from 400‹ to 700‹ C.</description><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; INORGANIC CHEMISTRY ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1974</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19740219&amp;DB=EPODOC&amp;CC=US&amp;NR=3793442A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19740219&amp;DB=EPODOC&amp;CC=US&amp;NR=3793442A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DUESING G,DT</creatorcontrib><creatorcontrib>HECKEL E,DT</creatorcontrib><creatorcontrib>RENNGARDT F,DT</creatorcontrib><creatorcontrib>MEYER SIMON E,DT</creatorcontrib><title>PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY</title><description>1277592 Germanium dioxide DEUTSCHE GOLDUND SILBER-SCHEIDEANSTALT 4 Sept 1969 [20 Sept 1968] 43879/69 Heading C1A Amorphous highly dispersed germanium dioxide is prepared by reacting a volatile tetravalent germanium compound or a sprayable solution thereof under hydrolysing or oxidizing conditions in the gas phase or as an aerosol at a temperature above 1300‹ C., allowing the germanium dioxide formed to coagulate at a temperature of from 200‹ to 1000‹ C., and separating the gaseous reaction products. The germanium compound is preferably a halide or a volatile organo-germanium compound. The reaction is preferably carried out at a temperature of from 1400‹ to 1700‹ C. using a fuel gas of high calorific value with a free oxygen containing gas or pure oxygen, the mixture being reacted after passage through a nozzle. The germanium dioxide formed is preferably coagulated and separated at a temperature of from 400‹ to 700‹ C.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>INORGANIC CHEMISTRY</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1974</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqFjLsKwjAUQLM4iPoN3h9wMQVxTJPbJGge5AEtDqVInEQL9f8xg7vTgcPhrMnNB8cxRnAdGHbRVgIzLnjlcgSlpboOIHT0GCIKkBgMszqb6lyvBQKzAupCZJ7AtYlpW7OkMGA7bMnqMT2XsvtxQ_YdJq4OZX6PZZmne3mVz5gjPZ1p0xwZ_V98AdrxMZU</recordid><startdate>19740219</startdate><enddate>19740219</enddate><creator>DUESING G,DT</creator><creator>HECKEL E,DT</creator><creator>RENNGARDT F,DT</creator><creator>MEYER SIMON E,DT</creator><scope>EVB</scope></search><sort><creationdate>19740219</creationdate><title>PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY</title><author>DUESING G,DT ; HECKEL E,DT ; RENNGARDT F,DT ; MEYER SIMON E,DT</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US3793442A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1974</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>INORGANIC CHEMISTRY</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>DUESING G,DT</creatorcontrib><creatorcontrib>HECKEL E,DT</creatorcontrib><creatorcontrib>RENNGARDT F,DT</creatorcontrib><creatorcontrib>MEYER SIMON E,DT</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DUESING G,DT</au><au>HECKEL E,DT</au><au>RENNGARDT F,DT</au><au>MEYER SIMON E,DT</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY</title><date>1974-02-19</date><risdate>1974</risdate><abstract>1277592 Germanium dioxide DEUTSCHE GOLDUND SILBER-SCHEIDEANSTALT 4 Sept 1969 [20 Sept 1968] 43879/69 Heading C1A Amorphous highly dispersed germanium dioxide is prepared by reacting a volatile tetravalent germanium compound or a sprayable solution thereof under hydrolysing or oxidizing conditions in the gas phase or as an aerosol at a temperature above 1300‹ C., allowing the germanium dioxide formed to coagulate at a temperature of from 200‹ to 1000‹ C., and separating the gaseous reaction products. The germanium compound is preferably a halide or a volatile organo-germanium compound. The reaction is preferably carried out at a temperature of from 1400‹ to 1700‹ C. using a fuel gas of high calorific value with a free oxygen containing gas or pure oxygen, the mixture being reacted after passage through a nozzle. The germanium dioxide formed is preferably coagulated and separated at a temperature of from 400‹ to 700‹ C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US3793442A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
INORGANIC CHEMISTRY
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title PROCESS OF MAKING AMORPHOUS HIGHLY DISPERSED GERMANIUM DIOXIDE AND PRODUCT OBTAINED THEREBY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-14T12%3A26%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DUESING%20G,DT&rft.date=1974-02-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS3793442A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true