Molding of stress-free polycarbonate articles

A stress-free, polycarbonate article, e.g. an extruded tube, is formed by maintaining the material during and immediately after moulding at a temperature between 70 DEG and 120 DEG C. and preferably 80 DEG to 100 DEG C. The article may subsequently be tempered at a temperature between 120 DEG and 14...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STREIB HUGO, HECHELHAMMER WILHELM
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator STREIB HUGO
HECHELHAMMER WILHELM
description A stress-free, polycarbonate article, e.g. an extruded tube, is formed by maintaining the material during and immediately after moulding at a temperature between 70 DEG and 120 DEG C. and preferably 80 DEG to 100 DEG C. The article may subsequently be tempered at a temperature between 120 DEG and 145 DEG C., e.g. 140 DEG C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US3155756A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US3155756A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US3155756A3</originalsourceid><addsrcrecordid>eNrjZND1zc9JycxLV8hPUyguKUotLtZNK0pNVSjIz6lMTixKys9LLElVSCwqyUzOSS3mYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXxocHGhqam5qZmjsaEVQAAQ_Ep2g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Molding of stress-free polycarbonate articles</title><source>esp@cenet</source><creator>STREIB HUGO ; HECHELHAMMER WILHELM</creator><creatorcontrib>STREIB HUGO ; HECHELHAMMER WILHELM</creatorcontrib><description>A stress-free, polycarbonate article, e.g. an extruded tube, is formed by maintaining the material during and immediately after moulding at a temperature between 70 DEG and 120 DEG C. and preferably 80 DEG to 100 DEG C. The article may subsequently be tempered at a temperature between 120 DEG and 145 DEG C., e.g. 140 DEG C.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>1964</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19641103&amp;DB=EPODOC&amp;CC=US&amp;NR=3155756A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19641103&amp;DB=EPODOC&amp;CC=US&amp;NR=3155756A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STREIB HUGO</creatorcontrib><creatorcontrib>HECHELHAMMER WILHELM</creatorcontrib><title>Molding of stress-free polycarbonate articles</title><description>A stress-free, polycarbonate article, e.g. an extruded tube, is formed by maintaining the material during and immediately after moulding at a temperature between 70 DEG and 120 DEG C. and preferably 80 DEG to 100 DEG C. The article may subsequently be tempered at a temperature between 120 DEG and 145 DEG C., e.g. 140 DEG C.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1964</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND1zc9JycxLV8hPUyguKUotLtZNK0pNVSjIz6lMTixKys9LLElVSCwqyUzOSS3mYWBNS8wpTuWF0twM8m6uIc4euqkF-fGpxQWJyal5qSXxocHGhqam5qZmjsaEVQAAQ_Ep2g</recordid><startdate>19641103</startdate><enddate>19641103</enddate><creator>STREIB HUGO</creator><creator>HECHELHAMMER WILHELM</creator><scope>EVB</scope></search><sort><creationdate>19641103</creationdate><title>Molding of stress-free polycarbonate articles</title><author>STREIB HUGO ; HECHELHAMMER WILHELM</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US3155756A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1964</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>STREIB HUGO</creatorcontrib><creatorcontrib>HECHELHAMMER WILHELM</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STREIB HUGO</au><au>HECHELHAMMER WILHELM</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Molding of stress-free polycarbonate articles</title><date>1964-11-03</date><risdate>1964</risdate><abstract>A stress-free, polycarbonate article, e.g. an extruded tube, is formed by maintaining the material during and immediately after moulding at a temperature between 70 DEG and 120 DEG C. and preferably 80 DEG to 100 DEG C. The article may subsequently be tempered at a temperature between 120 DEG and 145 DEG C., e.g. 140 DEG C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US3155756A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Molding of stress-free polycarbonate articles
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T02%3A13%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STREIB%20HUGO&rft.date=1964-11-03&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS3155756A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true