COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY
A method of forming a component can include electrochemically depositing a metallic material onto a carrier component to a thickness of greater than 50 microns. The metallic material can include crystal grains and at least 90% of the crystal grains can include nanotwin boundaries. The metallic mater...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Jou, Herng-Jeng Huang, Weiming Smith, Jacob L |
description | A method of forming a component can include electrochemically depositing a metallic material onto a carrier component to a thickness of greater than 50 microns. The metallic material can include crystal grains and at least 90% of the crystal grains can include nanotwin boundaries. The metallic material can include a Copper-Silver alloy (Cu-Ag) with between about 0.5-2 at %-Ag. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2024279777A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2024279777A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2024279777A13</originalsourceid><addsrcrecordid>eNrjZLBy9g8IcA1ScPTx8Y9UcPP08VUI9wzxUPDwdPdQCA4JcvVzB_Ic_VwgIs7-fi6hziGeYZ4hkTwMrGmJOcWpvFCam0HZzTXE2UM3tSA_PrW4IDE5NS-1JD402MjAyMTI3NLc3NzR0Jg4VQBSGioI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY</title><source>esp@cenet</source><creator>Jou, Herng-Jeng ; Huang, Weiming ; Smith, Jacob L</creator><creatorcontrib>Jou, Herng-Jeng ; Huang, Weiming ; Smith, Jacob L</creatorcontrib><description>A method of forming a component can include electrochemically depositing a metallic material onto a carrier component to a thickness of greater than 50 microns. The metallic material can include crystal grains and at least 90% of the crystal grains can include nanotwin boundaries. The metallic material can include a Copper-Silver alloy (Cu-Ag) with between about 0.5-2 at %-Ag.</description><language>eng</language><subject>ALLOYS ; APPARATUS THEREFOR ; BASIC ELECTRIC ELEMENTS ; CHEMICAL SURFACE TREATMENT ; CHEMISTRY ; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL ; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL ; COATING MATERIAL WITH METALLIC MATERIAL ; COATING METALLIC MATERIAL ; DIFFUSION TREATMENT OF METALLIC MATERIAL ; ELECTRICITY ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; FERROUS OR NON-FERROUS ALLOYS ; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY ; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240822&DB=EPODOC&CC=US&NR=2024279777A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240822&DB=EPODOC&CC=US&NR=2024279777A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Jou, Herng-Jeng</creatorcontrib><creatorcontrib>Huang, Weiming</creatorcontrib><creatorcontrib>Smith, Jacob L</creatorcontrib><title>COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY</title><description>A method of forming a component can include electrochemically depositing a metallic material onto a carrier component to a thickness of greater than 50 microns. The metallic material can include crystal grains and at least 90% of the crystal grains can include nanotwin boundaries. The metallic material can include a Copper-Silver alloy (Cu-Ag) with between about 0.5-2 at %-Ag.</description><subject>ALLOYS</subject><subject>APPARATUS THEREFOR</subject><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMICAL SURFACE TREATMENT</subject><subject>CHEMISTRY</subject><subject>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</subject><subject>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</subject><subject>COATING MATERIAL WITH METALLIC MATERIAL</subject><subject>COATING METALLIC MATERIAL</subject><subject>DIFFUSION TREATMENT OF METALLIC MATERIAL</subject><subject>ELECTRICITY</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><subject>SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBy9g8IcA1ScPTx8Y9UcPP08VUI9wzxUPDwdPdQCA4JcvVzB_Ic_VwgIs7-fi6hziGeYZ4hkTwMrGmJOcWpvFCam0HZzTXE2UM3tSA_PrW4IDE5NS-1JD402MjAyMTI3NLc3NzR0Jg4VQBSGioI</recordid><startdate>20240822</startdate><enddate>20240822</enddate><creator>Jou, Herng-Jeng</creator><creator>Huang, Weiming</creator><creator>Smith, Jacob L</creator><scope>EVB</scope></search><sort><creationdate>20240822</creationdate><title>COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY</title><author>Jou, Herng-Jeng ; Huang, Weiming ; Smith, Jacob L</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2024279777A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2024</creationdate><topic>ALLOYS</topic><topic>APPARATUS THEREFOR</topic><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMICAL SURFACE TREATMENT</topic><topic>CHEMISTRY</topic><topic>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</topic><topic>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</topic><topic>COATING MATERIAL WITH METALLIC MATERIAL</topic><topic>COATING METALLIC MATERIAL</topic><topic>DIFFUSION TREATMENT OF METALLIC MATERIAL</topic><topic>ELECTRICITY</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><topic>SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Jou, Herng-Jeng</creatorcontrib><creatorcontrib>Huang, Weiming</creatorcontrib><creatorcontrib>Smith, Jacob L</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Jou, Herng-Jeng</au><au>Huang, Weiming</au><au>Smith, Jacob L</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY</title><date>2024-08-22</date><risdate>2024</risdate><abstract>A method of forming a component can include electrochemically depositing a metallic material onto a carrier component to a thickness of greater than 50 microns. The metallic material can include crystal grains and at least 90% of the crystal grains can include nanotwin boundaries. The metallic material can include a Copper-Silver alloy (Cu-Ag) with between about 0.5-2 at %-Ag.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US2024279777A1 |
source | esp@cenet |
subjects | ALLOYS APPARATUS THEREFOR BASIC ELECTRIC ELEMENTS CHEMICAL SURFACE TREATMENT CHEMISTRY COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY IONIMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL COATING MATERIAL WITH METALLIC MATERIAL COATING METALLIC MATERIAL DIFFUSION TREATMENT OF METALLIC MATERIAL ELECTRICITY ELECTROFORMING ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FERROUS OR NON-FERROUS ALLOYS INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL METALLURGY PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THESURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | COPPER ALLOY FILM WITH HIGH STRENGTH AND HIGH CONDUCTIVITY |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T16%3A23%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Jou,%20Herng-Jeng&rft.date=2024-08-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2024279777A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |