METHOD FOR MANUFACTURING MOLDED BODY

A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHINOHARA, Takashi, WAKABAYASHI, Shigemi, SAGO, Takumi, NAKAZAWA, Masahiko
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHINOHARA, Takashi
WAKABAYASHI, Shigemi
SAGO, Takumi
NAKAZAWA, Masahiko
description A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied. In the method described above, the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA). The measurement is performed such that (1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute; (2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes; (3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and (4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2024003090A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2024003090A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2024003090A13</originalsourceid><addsrcrecordid>eNrjZFDxdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8PX3cXF1UXDyd4nkYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBkYmBgbGBpYGjobGxKkCAABdI8Y</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING MOLDED BODY</title><source>esp@cenet</source><creator>SHINOHARA, Takashi ; WAKABAYASHI, Shigemi ; SAGO, Takumi ; NAKAZAWA, Masahiko</creator><creatorcontrib>SHINOHARA, Takashi ; WAKABAYASHI, Shigemi ; SAGO, Takumi ; NAKAZAWA, Masahiko</creatorcontrib><description>A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied. In the method described above, the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA). The measurement is performed such that (1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute; (2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes; (3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and (4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.</description><language>eng</language><subject>IMPREGNATING OR COATING OF PAPER ; MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNERANALOGOUS TO PAPER ; MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN AMANNER ANALOGOUS TO PAPER, NOT PROVIDED FOR IN SUBCLASSESB31B OR B31C ; METHODS OF PRODUCING PAPER THEREON ; PAPER NOT OTHERWISE PROVIDED FOR ; PAPER-MAKING ; PAPER-MAKING MACHINES ; PERFORMING OPERATIONS ; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D ; PRODUCTION OF CELLULOSE ; PULP COMPOSITIONS ; TEXTILES ; TRANSPORTING ; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G ; WORKING PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUSTO PAPER</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240104&amp;DB=EPODOC&amp;CC=US&amp;NR=2024003090A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240104&amp;DB=EPODOC&amp;CC=US&amp;NR=2024003090A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHINOHARA, Takashi</creatorcontrib><creatorcontrib>WAKABAYASHI, Shigemi</creatorcontrib><creatorcontrib>SAGO, Takumi</creatorcontrib><creatorcontrib>NAKAZAWA, Masahiko</creatorcontrib><title>METHOD FOR MANUFACTURING MOLDED BODY</title><description>A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied. In the method described above, the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA). The measurement is performed such that (1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute; (2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes; (3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and (4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.</description><subject>IMPREGNATING OR COATING OF PAPER</subject><subject>MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNERANALOGOUS TO PAPER</subject><subject>MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN AMANNER ANALOGOUS TO PAPER, NOT PROVIDED FOR IN SUBCLASSESB31B OR B31C</subject><subject>METHODS OF PRODUCING PAPER THEREON</subject><subject>PAPER NOT OTHERWISE PROVIDED FOR</subject><subject>PAPER-MAKING</subject><subject>PAPER-MAKING MACHINES</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D</subject><subject>PRODUCTION OF CELLULOSE</subject><subject>PULP COMPOSITIONS</subject><subject>TEXTILES</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G</subject><subject>WORKING PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUSTO PAPER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFDxdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8PX3cXF1UXDyd4nkYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBkYmBgbGBpYGjobGxKkCAABdI8Y</recordid><startdate>20240104</startdate><enddate>20240104</enddate><creator>SHINOHARA, Takashi</creator><creator>WAKABAYASHI, Shigemi</creator><creator>SAGO, Takumi</creator><creator>NAKAZAWA, Masahiko</creator><scope>EVB</scope></search><sort><creationdate>20240104</creationdate><title>METHOD FOR MANUFACTURING MOLDED BODY</title><author>SHINOHARA, Takashi ; WAKABAYASHI, Shigemi ; SAGO, Takumi ; NAKAZAWA, Masahiko</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2024003090A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2024</creationdate><topic>IMPREGNATING OR COATING OF PAPER</topic><topic>MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNERANALOGOUS TO PAPER</topic><topic>MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN AMANNER ANALOGOUS TO PAPER, NOT PROVIDED FOR IN SUBCLASSESB31B OR B31C</topic><topic>METHODS OF PRODUCING PAPER THEREON</topic><topic>PAPER NOT OTHERWISE PROVIDED FOR</topic><topic>PAPER-MAKING</topic><topic>PAPER-MAKING MACHINES</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D</topic><topic>PRODUCTION OF CELLULOSE</topic><topic>PULP COMPOSITIONS</topic><topic>TEXTILES</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G</topic><topic>WORKING PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUSTO PAPER</topic><toplevel>online_resources</toplevel><creatorcontrib>SHINOHARA, Takashi</creatorcontrib><creatorcontrib>WAKABAYASHI, Shigemi</creatorcontrib><creatorcontrib>SAGO, Takumi</creatorcontrib><creatorcontrib>NAKAZAWA, Masahiko</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHINOHARA, Takashi</au><au>WAKABAYASHI, Shigemi</au><au>SAGO, Takumi</au><au>NAKAZAWA, Masahiko</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING MOLDED BODY</title><date>2024-01-04</date><risdate>2024</risdate><abstract>A method for manufacturing a molded body, includes a deposition step of depositing a mixture containing fibers and a starch in air; a moisturizing step of applying water to the mixture; and a molding step of forming a molded body by heating and pressurizing the mixture to which the water is applied. In the method described above, the starch has a setback viscosity (η50-η93) of 40 to 200 mPa·s, the setback viscosity (η50-η93) being obtained by measurement performed in accordance with the following measurement methods (1) to (4) using a rapid visco analyzer (RVA). The measurement is performed such that (1) after a water suspension containing the starch at 25 percent by mass is charged in the RVA as a measurement sample, the temperature thereof is increased to 50° C. and then maintained for one minute; (2) the temperature of the measurement sample is increased from 50° C. to 93° C. over 4 minutes and then maintained at 93° C. for 7 minutes; (3) the temperature of the measurement sample is decreased from 93° C. to 50° C. over 4 minutes and then maintained at 50° C. for 3 minutes; and (4) in the above (2) and (3), a rotational speed of a measurement paddle of the RVA is set to 960 rpm for 10 seconds after the start of the viscosity measurement and is then set to 160 rpm 10 seconds thereafter.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2024003090A1
source esp@cenet
subjects IMPREGNATING OR COATING OF PAPER
MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNERANALOGOUS TO PAPER
MAKING ARTICLES OF PAPER, CARDBOARD OR MATERIAL WORKED IN AMANNER ANALOGOUS TO PAPER, NOT PROVIDED FOR IN SUBCLASSESB31B OR B31C
METHODS OF PRODUCING PAPER THEREON
PAPER NOT OTHERWISE PROVIDED FOR
PAPER-MAKING
PAPER-MAKING MACHINES
PERFORMING OPERATIONS
PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D
PRODUCTION OF CELLULOSE
PULP COMPOSITIONS
TEXTILES
TRANSPORTING
TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G
WORKING PAPER, CARDBOARD OR MATERIAL WORKED IN A MANNER ANALOGOUSTO PAPER
title METHOD FOR MANUFACTURING MOLDED BODY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T22%3A25%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHINOHARA,%20Takashi&rft.date=2024-01-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2024003090A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true