HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME
The halogenated zinc phthalocyanine pigment is for use as a green pigment for color filters and capable of achieving high brightness. In the halogenated zinc phthalocyanine pigment, when a coating film containing 1.00 part by mass of the pigment, 0.95 parts by mass of a benzyl methacrylate-methacryl...
Gespeichert in:
Hauptverfasser: | , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Sakamoto, Keisuke Yamada, Takeshi Tamura, Yuji Tokuoka, Mayumi Shimada, Katsunori Oishi, Kentaro Hidaka, Yuta Yasui, Kengo Asami, Ryousuke |
description | The halogenated zinc phthalocyanine pigment is for use as a green pigment for color filters and capable of achieving high brightness. In the halogenated zinc phthalocyanine pigment, when a coating film containing 1.00 part by mass of the pigment, 0.95 parts by mass of a benzyl methacrylate-methacrylic acid copolymer, and 0.30 parts by mass of a dimethylaminoethyl methacrylate copolymer is heated at 230° C. for one hour to form an evaluation coating film having a thickness of 4 μm, an average scattering intensity at scattering angles 2θ in a range of 17° to 21° is determined from a two-dimensional scattering image obtained by GI-WAXS measurement of the evaluation coating film, and a normalized average scattering intensity is determined such that the average scattering intensity at an azimuth of 45° is 1, the normalized average scattering intensity at azimuths of 5° to 89° is 0.70 to 1.15. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2023287218A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2023287218A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2023287218A13</originalsourceid><addsrcrecordid>eNrjZHDzcPTxd3f1cwxxdVGI8vRzVgjwCAGJOUc6-nn6uSoEeLr7uvqFKDj6uSgEBPm7hDqHePr7Kfi6hnj4uyi4-QcpBDv6uvIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUkvjQYCMDI2MjC3MjQwtHQ2PiVAEAaC0tSg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME</title><source>esp@cenet</source><creator>Sakamoto, Keisuke ; Yamada, Takeshi ; Tamura, Yuji ; Tokuoka, Mayumi ; Shimada, Katsunori ; Oishi, Kentaro ; Hidaka, Yuta ; Yasui, Kengo ; Asami, Ryousuke</creator><creatorcontrib>Sakamoto, Keisuke ; Yamada, Takeshi ; Tamura, Yuji ; Tokuoka, Mayumi ; Shimada, Katsunori ; Oishi, Kentaro ; Hidaka, Yuta ; Yasui, Kengo ; Asami, Ryousuke</creatorcontrib><description>The halogenated zinc phthalocyanine pigment is for use as a green pigment for color filters and capable of achieving high brightness. In the halogenated zinc phthalocyanine pigment, when a coating film containing 1.00 part by mass of the pigment, 0.95 parts by mass of a benzyl methacrylate-methacrylic acid copolymer, and 0.30 parts by mass of a dimethylaminoethyl methacrylate copolymer is heated at 230° C. for one hour to form an evaluation coating film having a thickness of 4 μm, an average scattering intensity at scattering angles 2θ in a range of 17° to 21° is determined from a two-dimensional scattering image obtained by GI-WAXS measurement of the evaluation coating film, and a normalized average scattering intensity is determined such that the average scattering intensity at an azimuth of 45° is 1, the normalized average scattering intensity at azimuths of 5° to 89° is 0.70 to 1.15.</description><language>eng</language><subject>ADHESIVES ; CHEMISTRY ; DYES ; LAKES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; MORDANTS ; NATURAL RESINS ; ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES ; PAINTS ; POLISHES</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230914&DB=EPODOC&CC=US&NR=2023287218A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230914&DB=EPODOC&CC=US&NR=2023287218A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Sakamoto, Keisuke</creatorcontrib><creatorcontrib>Yamada, Takeshi</creatorcontrib><creatorcontrib>Tamura, Yuji</creatorcontrib><creatorcontrib>Tokuoka, Mayumi</creatorcontrib><creatorcontrib>Shimada, Katsunori</creatorcontrib><creatorcontrib>Oishi, Kentaro</creatorcontrib><creatorcontrib>Hidaka, Yuta</creatorcontrib><creatorcontrib>Yasui, Kengo</creatorcontrib><creatorcontrib>Asami, Ryousuke</creatorcontrib><title>HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME</title><description>The halogenated zinc phthalocyanine pigment is for use as a green pigment for color filters and capable of achieving high brightness. In the halogenated zinc phthalocyanine pigment, when a coating film containing 1.00 part by mass of the pigment, 0.95 parts by mass of a benzyl methacrylate-methacrylic acid copolymer, and 0.30 parts by mass of a dimethylaminoethyl methacrylate copolymer is heated at 230° C. for one hour to form an evaluation coating film having a thickness of 4 μm, an average scattering intensity at scattering angles 2θ in a range of 17° to 21° is determined from a two-dimensional scattering image obtained by GI-WAXS measurement of the evaluation coating film, and a normalized average scattering intensity is determined such that the average scattering intensity at an azimuth of 45° is 1, the normalized average scattering intensity at azimuths of 5° to 89° is 0.70 to 1.15.</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>LAKES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>MORDANTS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES</subject><subject>PAINTS</subject><subject>POLISHES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDzcPTxd3f1cwxxdVGI8vRzVgjwCAGJOUc6-nn6uSoEeLr7uvqFKDj6uSgEBPm7hDqHePr7Kfi6hnj4uyi4-QcpBDv6uvIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUkvjQYCMDI2MjC3MjQwtHQ2PiVAEAaC0tSg</recordid><startdate>20230914</startdate><enddate>20230914</enddate><creator>Sakamoto, Keisuke</creator><creator>Yamada, Takeshi</creator><creator>Tamura, Yuji</creator><creator>Tokuoka, Mayumi</creator><creator>Shimada, Katsunori</creator><creator>Oishi, Kentaro</creator><creator>Hidaka, Yuta</creator><creator>Yasui, Kengo</creator><creator>Asami, Ryousuke</creator><scope>EVB</scope></search><sort><creationdate>20230914</creationdate><title>HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME</title><author>Sakamoto, Keisuke ; Yamada, Takeshi ; Tamura, Yuji ; Tokuoka, Mayumi ; Shimada, Katsunori ; Oishi, Kentaro ; Hidaka, Yuta ; Yasui, Kengo ; Asami, Ryousuke</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2023287218A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2023</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>LAKES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>MORDANTS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES</topic><topic>PAINTS</topic><topic>POLISHES</topic><toplevel>online_resources</toplevel><creatorcontrib>Sakamoto, Keisuke</creatorcontrib><creatorcontrib>Yamada, Takeshi</creatorcontrib><creatorcontrib>Tamura, Yuji</creatorcontrib><creatorcontrib>Tokuoka, Mayumi</creatorcontrib><creatorcontrib>Shimada, Katsunori</creatorcontrib><creatorcontrib>Oishi, Kentaro</creatorcontrib><creatorcontrib>Hidaka, Yuta</creatorcontrib><creatorcontrib>Yasui, Kengo</creatorcontrib><creatorcontrib>Asami, Ryousuke</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Sakamoto, Keisuke</au><au>Yamada, Takeshi</au><au>Tamura, Yuji</au><au>Tokuoka, Mayumi</au><au>Shimada, Katsunori</au><au>Oishi, Kentaro</au><au>Hidaka, Yuta</au><au>Yasui, Kengo</au><au>Asami, Ryousuke</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME</title><date>2023-09-14</date><risdate>2023</risdate><abstract>The halogenated zinc phthalocyanine pigment is for use as a green pigment for color filters and capable of achieving high brightness. In the halogenated zinc phthalocyanine pigment, when a coating film containing 1.00 part by mass of the pigment, 0.95 parts by mass of a benzyl methacrylate-methacrylic acid copolymer, and 0.30 parts by mass of a dimethylaminoethyl methacrylate copolymer is heated at 230° C. for one hour to form an evaluation coating film having a thickness of 4 μm, an average scattering intensity at scattering angles 2θ in a range of 17° to 21° is determined from a two-dimensional scattering image obtained by GI-WAXS measurement of the evaluation coating film, and a normalized average scattering intensity is determined such that the average scattering intensity at an azimuth of 45° is 1, the normalized average scattering intensity at azimuths of 5° to 89° is 0.70 to 1.15.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US2023287218A1 |
source | esp@cenet |
subjects | ADHESIVES CHEMISTRY DYES LAKES METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS MORDANTS NATURAL RESINS ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES PAINTS POLISHES |
title | HALOGENATED ZINC PHTHALOCYANINE PIGMENT AND PRODUCTION METHOD FOR SAME |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T14%3A22%3A03IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Sakamoto,%20Keisuke&rft.date=2023-09-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2023287218A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |