METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS

Provided is a method of manufacturing a tempered glass, including an etching step of etching a plate-shaped or sheet-shaped chemically tempered glass having a compressive stress layer in a surface thereof. The method further includes a step of preparing, as the chemically tempered glass before the e...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ITO, Shigeyoshi, NODA, Takayuki
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ITO, Shigeyoshi
NODA, Takayuki
description Provided is a method of manufacturing a tempered glass, including an etching step of etching a plate-shaped or sheet-shaped chemically tempered glass having a compressive stress layer in a surface thereof. The method further includes a step of preparing, as the chemically tempered glass before the etching, a chemically tempered glass, which has in at least part thereof a bendable thin portion having a thickness tla, in which the thickness t1a is 150 µm or less, in which a maximum compressive stress CSa in the compressive stress layer before the etching is 1,100 MPa or less, and in which a depth DOLa of the compressive stress layer before the etching is less than 15 µm. The etching step includes etching the chemically tempered glass so that an etching amount Δt on one surface of the chemically tempered glass is 0.25 µm or more and 3 µm or less.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2023250013A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2023250013A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2023250013A13</originalsourceid><addsrcrecordid>eNrjZLD3dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCHL19AOKOru6KLj7OAYH6yg4-rlgiPIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUkvjQYCMDI2MjUwMDQ2NHQ2PiVAEAGj8rDw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS</title><source>esp@cenet</source><creator>ITO, Shigeyoshi ; NODA, Takayuki</creator><creatorcontrib>ITO, Shigeyoshi ; NODA, Takayuki</creatorcontrib><description>Provided is a method of manufacturing a tempered glass, including an etching step of etching a plate-shaped or sheet-shaped chemically tempered glass having a compressive stress layer in a surface thereof. The method further includes a step of preparing, as the chemically tempered glass before the etching, a chemically tempered glass, which has in at least part thereof a bendable thin portion having a thickness tla, in which the thickness t1a is 150 µm or less, in which a maximum compressive stress CSa in the compressive stress layer before the etching is 1,100 MPa or less, and in which a depth DOLa of the compressive stress layer before the etching is less than 15 µm. The etching step includes etching the chemically tempered glass so that an etching amount Δt on one surface of the chemically tempered glass is 0.25 µm or more and 3 µm or less.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230810&amp;DB=EPODOC&amp;CC=US&amp;NR=2023250013A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230810&amp;DB=EPODOC&amp;CC=US&amp;NR=2023250013A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ITO, Shigeyoshi</creatorcontrib><creatorcontrib>NODA, Takayuki</creatorcontrib><title>METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS</title><description>Provided is a method of manufacturing a tempered glass, including an etching step of etching a plate-shaped or sheet-shaped chemically tempered glass having a compressive stress layer in a surface thereof. The method further includes a step of preparing, as the chemically tempered glass before the etching, a chemically tempered glass, which has in at least part thereof a bendable thin portion having a thickness tla, in which the thickness t1a is 150 µm or less, in which a maximum compressive stress CSa in the compressive stress layer before the etching is 1,100 MPa or less, and in which a depth DOLa of the compressive stress layer before the etching is less than 15 µm. The etching step includes etching the chemically tempered glass so that an etching amount Δt on one surface of the chemically tempered glass is 0.25 µm or more and 3 µm or less.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD3dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCHL19AOKOru6KLj7OAYH6yg4-rlgiPIwsKYl5hSn8kJpbgZlN9cQZw_d1IL8-NTigsTk1LzUkvjQYCMDI2MjUwMDQ2NHQ2PiVAEAGj8rDw</recordid><startdate>20230810</startdate><enddate>20230810</enddate><creator>ITO, Shigeyoshi</creator><creator>NODA, Takayuki</creator><scope>EVB</scope></search><sort><creationdate>20230810</creationdate><title>METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS</title><author>ITO, Shigeyoshi ; NODA, Takayuki</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2023250013A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>ITO, Shigeyoshi</creatorcontrib><creatorcontrib>NODA, Takayuki</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ITO, Shigeyoshi</au><au>NODA, Takayuki</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS</title><date>2023-08-10</date><risdate>2023</risdate><abstract>Provided is a method of manufacturing a tempered glass, including an etching step of etching a plate-shaped or sheet-shaped chemically tempered glass having a compressive stress layer in a surface thereof. The method further includes a step of preparing, as the chemically tempered glass before the etching, a chemically tempered glass, which has in at least part thereof a bendable thin portion having a thickness tla, in which the thickness t1a is 150 µm or less, in which a maximum compressive stress CSa in the compressive stress layer before the etching is 1,100 MPa or less, and in which a depth DOLa of the compressive stress layer before the etching is less than 15 µm. The etching step includes etching the chemically tempered glass so that an etching amount Δt on one surface of the chemically tempered glass is 0.25 µm or more and 3 µm or less.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2023250013A1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR MANUFACTURING REINFORCED GLASS, AND REINFORCED GLASS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T12%3A38%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ITO,%20Shigeyoshi&rft.date=2023-08-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2023250013A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true