SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF

A chemically toughenable or toughened sheet-like glass article is provided. The article has a glass with a composition comprising Al2O3, SiO2, Li2O, and Na2O, wherein (Al2O3)−(Li2O+Na2O), in mol %, is less than 0; a thickness between 0.3 mm and 4 mm; a light transmittance of at least 0.001% to at mo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Leukel, Sebastian, Engelmann, Jacqueline
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Leukel, Sebastian
Engelmann, Jacqueline
description A chemically toughenable or toughened sheet-like glass article is provided. The article has a glass with a composition comprising Al2O3, SiO2, Li2O, and Na2O, wherein (Al2O3)−(Li2O+Na2O), in mol %, is less than 0; a thickness between 0.3 mm and 4 mm; a light transmittance of at least 0.001% to at most 60% at 450 nm, of at least 0.001% to at most 30% at 540 nm, and of at least 0.001% to at most 30% at 630 nm; and an IR transmittance of at least 10% to not more than 99% at any wavelength in a wavelength range from 900 nm to 1100 nm. The light and IR transmittances are determined for a thickness of the article of 1 mm.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2023159383A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2023159383A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2023159383A13</originalsourceid><addsrcrecordid>eNrjZHAJ9nB1DdH18fR2VXD3cQwOVnAMCvF09nHVUfB1DfHwd1Fw8w9SCAjydwl19vRzVwh29AVKOfq5KIQGuyqEeLgGufq78TCwpiXmFKfyQmluBmU31xBnD93Ugvz41OKCxOTUvNSS-NBgIwMjY0NTS2MLY0dDY-JUAQDFhSwu</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF</title><source>esp@cenet</source><creator>Leukel, Sebastian ; Engelmann, Jacqueline</creator><creatorcontrib>Leukel, Sebastian ; Engelmann, Jacqueline</creatorcontrib><description>A chemically toughenable or toughened sheet-like glass article is provided. The article has a glass with a composition comprising Al2O3, SiO2, Li2O, and Na2O, wherein (Al2O3)−(Li2O+Na2O), in mol %, is less than 0; a thickness between 0.3 mm and 4 mm; a light transmittance of at least 0.001% to at most 60% at 450 nm, of at least 0.001% to at most 30% at 540 nm, and of at least 0.001% to at most 30% at 630 nm; and an IR transmittance of at least 10% to not more than 99% at any wavelength in a wavelength range from 900 nm to 1100 nm. The light and IR transmittances are determined for a thickness of the article of 1 mm.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230525&amp;DB=EPODOC&amp;CC=US&amp;NR=2023159383A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230525&amp;DB=EPODOC&amp;CC=US&amp;NR=2023159383A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Leukel, Sebastian</creatorcontrib><creatorcontrib>Engelmann, Jacqueline</creatorcontrib><title>SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF</title><description>A chemically toughenable or toughened sheet-like glass article is provided. The article has a glass with a composition comprising Al2O3, SiO2, Li2O, and Na2O, wherein (Al2O3)−(Li2O+Na2O), in mol %, is less than 0; a thickness between 0.3 mm and 4 mm; a light transmittance of at least 0.001% to at most 60% at 450 nm, of at least 0.001% to at most 30% at 540 nm, and of at least 0.001% to at most 30% at 630 nm; and an IR transmittance of at least 10% to not more than 99% at any wavelength in a wavelength range from 900 nm to 1100 nm. The light and IR transmittances are determined for a thickness of the article of 1 mm.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAJ9nB1DdH18fR2VXD3cQwOVnAMCvF09nHVUfB1DfHwd1Fw8w9SCAjydwl19vRzVwh29AVKOfq5KIQGuyqEeLgGufq78TCwpiXmFKfyQmluBmU31xBnD93Ugvz41OKCxOTUvNSS-NBgIwMjY0NTS2MLY0dDY-JUAQDFhSwu</recordid><startdate>20230525</startdate><enddate>20230525</enddate><creator>Leukel, Sebastian</creator><creator>Engelmann, Jacqueline</creator><scope>EVB</scope></search><sort><creationdate>20230525</creationdate><title>SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF</title><author>Leukel, Sebastian ; Engelmann, Jacqueline</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2023159383A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2023</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>Leukel, Sebastian</creatorcontrib><creatorcontrib>Engelmann, Jacqueline</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Leukel, Sebastian</au><au>Engelmann, Jacqueline</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF</title><date>2023-05-25</date><risdate>2023</risdate><abstract>A chemically toughenable or toughened sheet-like glass article is provided. The article has a glass with a composition comprising Al2O3, SiO2, Li2O, and Na2O, wherein (Al2O3)−(Li2O+Na2O), in mol %, is less than 0; a thickness between 0.3 mm and 4 mm; a light transmittance of at least 0.001% to at most 60% at 450 nm, of at least 0.001% to at most 30% at 540 nm, and of at least 0.001% to at most 30% at 630 nm; and an IR transmittance of at least 10% to not more than 99% at any wavelength in a wavelength range from 900 nm to 1100 nm. The light and IR transmittances are determined for a thickness of the article of 1 mm.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2023159383A1
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title SHEET-LIKE GLASS ARTICLE, METHOD FOR PRODUCING SAME, AND USE THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T23%3A33%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Leukel,%20Sebastian&rft.date=2023-05-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2023159383A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true