METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES
Methods for preparing thermoplastic automotive appliques include applying heat from an auxiliary heater to a tool cavity of a forming tool. The auxiliary heater is activated for a period of time until a temperature of the heated tool cavity is heated to less than or equal to about a melting temperat...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | Dellock, Paul Kenneth Salter, Stuart C Walawender, Chester Stanislaus Gall, Richard Glickman, Dave Brian |
description | Methods for preparing thermoplastic automotive appliques include applying heat from an auxiliary heater to a tool cavity of a forming tool. The auxiliary heater is activated for a period of time until a temperature of the heated tool cavity is heated to less than or equal to about a melting temperature of the thermoplastic. The heated tool cavity is filled with the thermoplastic, and a cooling fluid is pulsed through the forming tool. The thermoplastic applique is then removed, and the supply of cooling fluid is turned off. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2021039294A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2021039294A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2021039294A13</originalsourceid><addsrcrecordid>eNqNyrEKwjAQgOEsDqK-w4Gz0KYuHY_0QgqtF5NLwakUiZNoob4_dvABnH74-bZq6EkcNyAMQr2nAOIIYgoWDYHD0FwoRmALaMKtaw1wAF5NAN9hlHVgEu5Z2oEAve_aa6K4V5vH9Fzy4dedOloS4055fo95mad7fuXPmKIudFlUta7PWFb_qS9PxzG0</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES</title><source>esp@cenet</source><creator>Dellock, Paul Kenneth ; Salter, Stuart C ; Walawender, Chester Stanislaus ; Gall, Richard ; Glickman, Dave Brian</creator><creatorcontrib>Dellock, Paul Kenneth ; Salter, Stuart C ; Walawender, Chester Stanislaus ; Gall, Richard ; Glickman, Dave Brian</creatorcontrib><description>Methods for preparing thermoplastic automotive appliques include applying heat from an auxiliary heater to a tool cavity of a forming tool. The auxiliary heater is activated for a period of time until a temperature of the heated tool cavity is heated to less than or equal to about a melting temperature of the thermoplastic. The heated tool cavity is filled with the thermoplastic, and a cooling fluid is pulsed through the forming tool. The thermoplastic applique is then removed, and the supply of cooling fluid is turned off.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210211&DB=EPODOC&CC=US&NR=2021039294A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20210211&DB=EPODOC&CC=US&NR=2021039294A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Dellock, Paul Kenneth</creatorcontrib><creatorcontrib>Salter, Stuart C</creatorcontrib><creatorcontrib>Walawender, Chester Stanislaus</creatorcontrib><creatorcontrib>Gall, Richard</creatorcontrib><creatorcontrib>Glickman, Dave Brian</creatorcontrib><title>METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES</title><description>Methods for preparing thermoplastic automotive appliques include applying heat from an auxiliary heater to a tool cavity of a forming tool. The auxiliary heater is activated for a period of time until a temperature of the heated tool cavity is heated to less than or equal to about a melting temperature of the thermoplastic. The heated tool cavity is filled with the thermoplastic, and a cooling fluid is pulsed through the forming tool. The thermoplastic applique is then removed, and the supply of cooling fluid is turned off.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQgOEsDqK-w4Gz0KYuHY_0QgqtF5NLwakUiZNoob4_dvABnH74-bZq6EkcNyAMQr2nAOIIYgoWDYHD0FwoRmALaMKtaw1wAF5NAN9hlHVgEu5Z2oEAve_aa6K4V5vH9Fzy4dedOloS4055fo95mad7fuXPmKIudFlUta7PWFb_qS9PxzG0</recordid><startdate>20210211</startdate><enddate>20210211</enddate><creator>Dellock, Paul Kenneth</creator><creator>Salter, Stuart C</creator><creator>Walawender, Chester Stanislaus</creator><creator>Gall, Richard</creator><creator>Glickman, Dave Brian</creator><scope>EVB</scope></search><sort><creationdate>20210211</creationdate><title>METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES</title><author>Dellock, Paul Kenneth ; Salter, Stuart C ; Walawender, Chester Stanislaus ; Gall, Richard ; Glickman, Dave Brian</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2021039294A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2021</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>Dellock, Paul Kenneth</creatorcontrib><creatorcontrib>Salter, Stuart C</creatorcontrib><creatorcontrib>Walawender, Chester Stanislaus</creatorcontrib><creatorcontrib>Gall, Richard</creatorcontrib><creatorcontrib>Glickman, Dave Brian</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Dellock, Paul Kenneth</au><au>Salter, Stuart C</au><au>Walawender, Chester Stanislaus</au><au>Gall, Richard</au><au>Glickman, Dave Brian</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES</title><date>2021-02-11</date><risdate>2021</risdate><abstract>Methods for preparing thermoplastic automotive appliques include applying heat from an auxiliary heater to a tool cavity of a forming tool. The auxiliary heater is activated for a period of time until a temperature of the heated tool cavity is heated to less than or equal to about a melting temperature of the thermoplastic. The heated tool cavity is filled with the thermoplastic, and a cooling fluid is pulsed through the forming tool. The thermoplastic applique is then removed, and the supply of cooling fluid is turned off.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_US2021039294A1 |
source | esp@cenet |
subjects | AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING PERFORMING OPERATIONS SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR SHAPING OR JOINING OF PLASTICS TRANSPORTING WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | METHOD TO TEMPER THE SURFACE HARDNESS OF ACRYLIC OR OTHER PLASTIC AUTOMOTIVE APPLIQUES |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-21T18%3A16%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Dellock,%20Paul%20Kenneth&rft.date=2021-02-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2021039294A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |