FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY

The disclosure describes techniques for eliminating or reducing non-wet open (NWO) defect formation by using a low activity flux to prevent a solder paste from sticking to ball grid array (BGA) solder balls during reflow soldering. The low activity flux may be configured such that: i) it creates a b...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHOU, FENGYING, CHEN, FEN, LEE, NINGNG
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHOU, FENGYING
CHEN, FEN
LEE, NINGNG
description The disclosure describes techniques for eliminating or reducing non-wet open (NWO) defect formation by using a low activity flux to prevent a solder paste from sticking to ball grid array (BGA) solder balls during reflow soldering. The low activity flux may be configured such that: i) it creates a barrier that prevents the solder paste from sticking to the solder balls of the BGA; and ii) it does not impede the formation of solder joints during reflow. In implementations, a solid coating of the low activity flux may be formed over balls of the BGA, and the BGA may then be bonded to a PCB during reflow. In implementations, the balls of a BGA may be dipped in a low-activity creamy or liquid flux prior to reflow. In some implementations, the flux may applied on a solder paste printed on pads of the PCB, followed by placement of a BGA.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2019371752A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2019371752A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2019371752A13</originalsourceid><addsrcrecordid>eNrjZLBx8wmNcA1WcHVzc3UO8QxzVfD0UwgODQgIcg0O9vRzV_Dz99MNdw3R9Q9w9VNwDFFwcndUcAwOdvV18onkYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBoaWxuaG5qZGjobGxKkCALHwKok</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY</title><source>esp@cenet</source><creator>ZHOU, FENGYING ; CHEN, FEN ; LEE, NINGNG</creator><creatorcontrib>ZHOU, FENGYING ; CHEN, FEN ; LEE, NINGNG</creatorcontrib><description>The disclosure describes techniques for eliminating or reducing non-wet open (NWO) defect formation by using a low activity flux to prevent a solder paste from sticking to ball grid array (BGA) solder balls during reflow soldering. The low activity flux may be configured such that: i) it creates a barrier that prevents the solder paste from sticking to the solder balls of the BGA; and ii) it does not impede the formation of solder joints during reflow. In implementations, a solid coating of the low activity flux may be formed over balls of the BGA, and the BGA may then be bonded to a PCB during reflow. In implementations, the balls of a BGA may be dipped in a low-activity creamy or liquid flux prior to reflow. In some implementations, the flux may applied on a solder paste printed on pads of the PCB, followed by placement of a BGA.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS ; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ; ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS ; PRINTED CIRCUITS ; SEMICONDUCTOR DEVICES</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191205&amp;DB=EPODOC&amp;CC=US&amp;NR=2019371752A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191205&amp;DB=EPODOC&amp;CC=US&amp;NR=2019371752A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHOU, FENGYING</creatorcontrib><creatorcontrib>CHEN, FEN</creatorcontrib><creatorcontrib>LEE, NINGNG</creatorcontrib><title>FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY</title><description>The disclosure describes techniques for eliminating or reducing non-wet open (NWO) defect formation by using a low activity flux to prevent a solder paste from sticking to ball grid array (BGA) solder balls during reflow soldering. The low activity flux may be configured such that: i) it creates a barrier that prevents the solder paste from sticking to the solder balls of the BGA; and ii) it does not impede the formation of solder joints during reflow. In implementations, a solid coating of the low activity flux may be formed over balls of the BGA, and the BGA may then be bonded to a PCB during reflow. In implementations, the balls of a BGA may be dipped in a low-activity creamy or liquid flux prior to reflow. In some implementations, the flux may applied on a solder paste printed on pads of the PCB, followed by placement of a BGA.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS</subject><subject>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS</subject><subject>PRINTED CIRCUITS</subject><subject>SEMICONDUCTOR DEVICES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBx8wmNcA1WcHVzc3UO8QxzVfD0UwgODQgIcg0O9vRzV_Dz99MNdw3R9Q9w9VNwDFFwcndUcAwOdvV18onkYWBNS8wpTuWF0twMym6uIc4euqkF-fGpxQWJyal5qSXxocFGBoaWxuaG5qZGjobGxKkCALHwKok</recordid><startdate>20191205</startdate><enddate>20191205</enddate><creator>ZHOU, FENGYING</creator><creator>CHEN, FEN</creator><creator>LEE, NINGNG</creator><scope>EVB</scope></search><sort><creationdate>20191205</creationdate><title>FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY</title><author>ZHOU, FENGYING ; CHEN, FEN ; LEE, NINGNG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2019371752A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS</topic><topic>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS</topic><topic>PRINTED CIRCUITS</topic><topic>SEMICONDUCTOR DEVICES</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHOU, FENGYING</creatorcontrib><creatorcontrib>CHEN, FEN</creatorcontrib><creatorcontrib>LEE, NINGNG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHOU, FENGYING</au><au>CHEN, FEN</au><au>LEE, NINGNG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY</title><date>2019-12-05</date><risdate>2019</risdate><abstract>The disclosure describes techniques for eliminating or reducing non-wet open (NWO) defect formation by using a low activity flux to prevent a solder paste from sticking to ball grid array (BGA) solder balls during reflow soldering. The low activity flux may be configured such that: i) it creates a barrier that prevents the solder paste from sticking to the solder balls of the BGA; and ii) it does not impede the formation of solder joints during reflow. In implementations, a solid coating of the low activity flux may be formed over balls of the BGA, and the BGA may then be bonded to a PCB during reflow. In implementations, the balls of a BGA may be dipped in a low-activity creamy or liquid flux prior to reflow. In some implementations, the flux may applied on a solder paste printed on pads of the PCB, followed by placement of a BGA.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2019371752A1
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS
ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
PRINTED CIRCUITS
SEMICONDUCTOR DEVICES
title FLUXES EFFECTIVE IN SUPPRESSING NON-WET-OPEN AT BGA ASSEMBLY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T16%3A54%3A33IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHOU,%20FENGYING&rft.date=2019-12-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2019371752A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true