TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION

A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Sahni, Vasav, Munson, Daniel C, Kobe, James J, Deodhar, Sarang V, Opatz, Meredith A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Sahni, Vasav
Munson, Daniel C
Kobe, James J
Deodhar, Sarang V
Opatz, Meredith A
description A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed on the primed surface of the backing layer, wherein the pressure sensitive adhesive layer has a thickness of at least 7.6 micrometers (and preferably up to 25 micrometers); wherein, when disposed on an aluminum substrate, the tape displays a peel adhesion of less than 20 oz/in (219 N/m) according to a Peel Adhesion Strength Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to a Chromic Acid Anodization-Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2019352790A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2019352790A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2019352790A13</originalsourceid><addsrcrecordid>eNqNjLsKwkAQAK-xEPUfFqyFPBBJudzDW_Ru5R5NmhDkrEQD8f8xhR9gNc3MrEVIeNMR0CtwOllWEdhAjhoMB3AYL-TPgNfsyGcHMQeDcgnIg7SBHUlASWoZsKIeE7HfitVjfM5l9-NG7I1O0h7K9B7KPI338iqfIcemqrv22Jy6Cuv2P-sLX40wQQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION</title><source>esp@cenet</source><creator>Sahni, Vasav ; Munson, Daniel C ; Kobe, James J ; Deodhar, Sarang V ; Opatz, Meredith A</creator><creatorcontrib>Sahni, Vasav ; Munson, Daniel C ; Kobe, James J ; Deodhar, Sarang V ; Opatz, Meredith A</creatorcontrib><description>A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed on the primed surface of the backing layer, wherein the pressure sensitive adhesive layer has a thickness of at least 7.6 micrometers (and preferably up to 25 micrometers); wherein, when disposed on an aluminum substrate, the tape displays a peel adhesion of less than 20 oz/in (219 N/m) according to a Peel Adhesion Strength Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to a Chromic Acid Anodization-Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.</description><language>eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; APPARATUS THEREFOR ; CHEMISTRY ; DYES ; ELECTROFORMING ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; PAINTS ; POLISHES ; PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191121&amp;DB=EPODOC&amp;CC=US&amp;NR=2019352790A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191121&amp;DB=EPODOC&amp;CC=US&amp;NR=2019352790A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Sahni, Vasav</creatorcontrib><creatorcontrib>Munson, Daniel C</creatorcontrib><creatorcontrib>Kobe, James J</creatorcontrib><creatorcontrib>Deodhar, Sarang V</creatorcontrib><creatorcontrib>Opatz, Meredith A</creatorcontrib><title>TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION</title><description>A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed on the primed surface of the backing layer, wherein the pressure sensitive adhesive layer has a thickness of at least 7.6 micrometers (and preferably up to 25 micrometers); wherein, when disposed on an aluminum substrate, the tape displays a peel adhesion of less than 20 oz/in (219 N/m) according to a Peel Adhesion Strength Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to a Chromic Acid Anodization-Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>ELECTROFORMING</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLsKwkAQAK-xEPUfFqyFPBBJudzDW_Ru5R5NmhDkrEQD8f8xhR9gNc3MrEVIeNMR0CtwOllWEdhAjhoMB3AYL-TPgNfsyGcHMQeDcgnIg7SBHUlASWoZsKIeE7HfitVjfM5l9-NG7I1O0h7K9B7KPI338iqfIcemqrv22Jy6Cuv2P-sLX40wQQ</recordid><startdate>20191121</startdate><enddate>20191121</enddate><creator>Sahni, Vasav</creator><creator>Munson, Daniel C</creator><creator>Kobe, James J</creator><creator>Deodhar, Sarang V</creator><creator>Opatz, Meredith A</creator><scope>EVB</scope></search><sort><creationdate>20191121</creationdate><title>TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION</title><author>Sahni, Vasav ; Munson, Daniel C ; Kobe, James J ; Deodhar, Sarang V ; Opatz, Meredith A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2019352790A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2019</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>ELECTROFORMING</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>Sahni, Vasav</creatorcontrib><creatorcontrib>Munson, Daniel C</creatorcontrib><creatorcontrib>Kobe, James J</creatorcontrib><creatorcontrib>Deodhar, Sarang V</creatorcontrib><creatorcontrib>Opatz, Meredith A</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Sahni, Vasav</au><au>Munson, Daniel C</au><au>Kobe, James J</au><au>Deodhar, Sarang V</au><au>Opatz, Meredith A</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION</title><date>2019-11-21</date><risdate>2019</risdate><abstract>A tape includes: a flexible backing layer having two major surfaces, wherein the backing layer has a thickness of greater than 64 micrometers and up to 200 micrometers, and one major surface of the backing layer includes a primed surface; and a rubber-based pressure sensitive adhesive layer disposed on the primed surface of the backing layer, wherein the pressure sensitive adhesive layer has a thickness of at least 7.6 micrometers (and preferably up to 25 micrometers); wherein, when disposed on an aluminum substrate, the tape displays a peel adhesion of less than 20 oz/in (219 N/m) according to a Peel Adhesion Strength Test described in the Examples Section, and a leakage distance of less than 762 micrometers according to a Chromic Acid Anodization-Leakage Distance Test described in the Examples Section. A method of anodizing an aluminum surface includes: providing a substrate having an aluminum surface; applying a tape as described herein to mask the aluminum surface and form a masked substrate; and exposing the masked substrate to an electrolyte solution including chromic acid under conditions effective to form aluminum oxide.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2019352790A1
source esp@cenet
subjects ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE
ADHESIVES
APPARATUS THEREFOR
CHEMISTRY
DYES
ELECTROFORMING
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL
PAINTS
POLISHES
PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTIONOF COATINGS
USE OF MATERIALS AS ADHESIVES
title TAPES AND METHODS OF USE FOR MASKING ALUMINUM SURFACES IN CHROMIC ACID ANODIZATION
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T22%3A26%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Sahni,%20Vasav&rft.date=2019-11-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2019352790A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true