ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR

Provided is an anode active material, including: an amorphous carbon material in which the ratio of moieties having a distance d002 of 3.77 Å or more between crystal planes is 4% to 15% based on the entire crystal plane distance distribution. When the anode active material is used, the lifespan char...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEE, Soojeong, SHIN, Changsu
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LEE, Soojeong
SHIN, Changsu
description Provided is an anode active material, including: an amorphous carbon material in which the ratio of moieties having a distance d002 of 3.77 Å or more between crystal planes is 4% to 15% based on the entire crystal plane distance distribution. When the anode active material is used, the lifespan characteristics of a lithium battery may be improved while exhibiting high capacity.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2019341613A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2019341613A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2019341613A13</originalsourceid><addsrcrecordid>eNrjZDB19PN3cVVwdA7xDHNV8HUMcQ3ydPRRcPRzUQgIcg1wDHIM8fT3U_B1DfHwd1EI8XANcnXzD-JhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfGhwUYGhpbGJoZmhsaOhsbEqQIAehsodg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR</title><source>esp@cenet</source><creator>LEE, Soojeong ; SHIN, Changsu</creator><creatorcontrib>LEE, Soojeong ; SHIN, Changsu</creatorcontrib><description>Provided is an anode active material, including: an amorphous carbon material in which the ratio of moieties having a distance d002 of 3.77 Å or more between crystal planes is 4% to 15% based on the entire crystal plane distance distribution. When the anode active material is used, the lifespan characteristics of a lithium battery may be improved while exhibiting high capacity.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191107&amp;DB=EPODOC&amp;CC=US&amp;NR=2019341613A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20191107&amp;DB=EPODOC&amp;CC=US&amp;NR=2019341613A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LEE, Soojeong</creatorcontrib><creatorcontrib>SHIN, Changsu</creatorcontrib><title>ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR</title><description>Provided is an anode active material, including: an amorphous carbon material in which the ratio of moieties having a distance d002 of 3.77 Å or more between crystal planes is 4% to 15% based on the entire crystal plane distance distribution. When the anode active material is used, the lifespan characteristics of a lithium battery may be improved while exhibiting high capacity.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB19PN3cVVwdA7xDHNV8HUMcQ3ydPRRcPRzUQgIcg1wDHIM8fT3U_B1DfHwd1EI8XANcnXzD-JhYE1LzClO5YXS3AzKbq4hzh66qQX58anFBYnJqXmpJfGhwUYGhpbGJoZmhsaOhsbEqQIAehsodg</recordid><startdate>20191107</startdate><enddate>20191107</enddate><creator>LEE, Soojeong</creator><creator>SHIN, Changsu</creator><scope>EVB</scope></search><sort><creationdate>20191107</creationdate><title>ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR</title><author>LEE, Soojeong ; SHIN, Changsu</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2019341613A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2019</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>LEE, Soojeong</creatorcontrib><creatorcontrib>SHIN, Changsu</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LEE, Soojeong</au><au>SHIN, Changsu</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR</title><date>2019-11-07</date><risdate>2019</risdate><abstract>Provided is an anode active material, including: an amorphous carbon material in which the ratio of moieties having a distance d002 of 3.77 Å or more between crystal planes is 4% to 15% based on the entire crystal plane distance distribution. When the anode active material is used, the lifespan characteristics of a lithium battery may be improved while exhibiting high capacity.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2019341613A1
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title ANODE ACTIVE MATERIAL AND PREPARATION METHOD THEREFOR
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T21%3A00%3A33IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LEE,%20Soojeong&rft.date=2019-11-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2019341613A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true