Method to Reduce Anode Lead Wire Embrittlement in Capacitors
An improved capacitor, and method of manufacturing the improved capacitor, is provided. The method includes deoxygenating and leaching the anode wire to produce a capacitor comprising an anode having a surface area of at least 4.0 m2/g or a charge density of at least 200,000 CV/g with the anode wire...