FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS

Four-step thermal aging method for improving environmentally assisted cracking resistance of 7xxx series aluminium alloys. The thermal aging is carried out by treating the alloys at a temperature of 120 to 130 oC for 0.3 to 0.5 h, water quenching the alloys to a temperature of 25 to 27 oC and furthe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Ajay, Krishnan, Muralidhar, Vaidya Surendra, Raja, Vngaranahalli Srinivasan
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Ajay, Krishnan
Muralidhar, Vaidya Surendra
Raja, Vngaranahalli Srinivasan
description Four-step thermal aging method for improving environmentally assisted cracking resistance of 7xxx series aluminium alloys. The thermal aging is carried out by treating the alloys at a temperature of 120 to 130 oC for 0.3 to 0.5 h, water quenching the alloys to a temperature of 25 to 27 oC and further treating the alloys at a temperature of 80 to 95 oC for 100 to 120 h and at a temperature of 120 to 130 oC for 20 to 24 h and at a temperature of 155 to 160 oC for 1 to 5 h and air cooling the alloys to room temperature, sequentially.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2019153578A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2019153578A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2019153578A13</originalsourceid><addsrcrecordid>eNqNi80KgkAURt20iOodLrQWMpFqOYxXHZofuTMjuhKJaRUl2Ka3T6EHaPUdDudbR5_CeIqtwxpchaSYBFYKXYJCV5kcCkMgVE2mWSTqRpDRCrVjUnbArBXzNwdOjF-XgnAxTHMEU8CpbVuwSAItMOmV0MKrmaTp7DZa3YfHFHa_3UT7Ah2v4jC--jCNwy08w7v39nhILkmWZqczS9L_qi8UTTvf</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS</title><source>esp@cenet</source><creator>Ajay, Krishnan ; Muralidhar, Vaidya Surendra ; Raja, Vngaranahalli Srinivasan</creator><creatorcontrib>Ajay, Krishnan ; Muralidhar, Vaidya Surendra ; Raja, Vngaranahalli Srinivasan</creatorcontrib><description>Four-step thermal aging method for improving environmentally assisted cracking resistance of 7xxx series aluminium alloys. The thermal aging is carried out by treating the alloys at a temperature of 120 to 130 oC for 0.3 to 0.5 h, water quenching the alloys to a temperature of 25 to 27 oC and further treating the alloys at a temperature of 80 to 95 oC for 100 to 120 h and at a temperature of 120 to 130 oC for 20 to 24 h and at a temperature of 155 to 160 oC for 1 to 5 h and air cooling the alloys to room temperature, sequentially.</description><language>eng</language><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2019</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190523&amp;DB=EPODOC&amp;CC=US&amp;NR=2019153578A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20190523&amp;DB=EPODOC&amp;CC=US&amp;NR=2019153578A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Ajay, Krishnan</creatorcontrib><creatorcontrib>Muralidhar, Vaidya Surendra</creatorcontrib><creatorcontrib>Raja, Vngaranahalli Srinivasan</creatorcontrib><title>FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS</title><description>Four-step thermal aging method for improving environmentally assisted cracking resistance of 7xxx series aluminium alloys. The thermal aging is carried out by treating the alloys at a temperature of 120 to 130 oC for 0.3 to 0.5 h, water quenching the alloys to a temperature of 25 to 27 oC and further treating the alloys at a temperature of 80 to 95 oC for 100 to 120 h and at a temperature of 120 to 130 oC for 20 to 24 h and at a temperature of 155 to 160 oC for 1 to 5 h and air cooling the alloys to room temperature, sequentially.</description><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2019</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi80KgkAURt20iOodLrQWMpFqOYxXHZofuTMjuhKJaRUl2Ka3T6EHaPUdDudbR5_CeIqtwxpchaSYBFYKXYJCV5kcCkMgVE2mWSTqRpDRCrVjUnbArBXzNwdOjF-XgnAxTHMEU8CpbVuwSAItMOmV0MKrmaTp7DZa3YfHFHa_3UT7Ah2v4jC--jCNwy08w7v39nhILkmWZqczS9L_qi8UTTvf</recordid><startdate>20190523</startdate><enddate>20190523</enddate><creator>Ajay, Krishnan</creator><creator>Muralidhar, Vaidya Surendra</creator><creator>Raja, Vngaranahalli Srinivasan</creator><scope>EVB</scope></search><sort><creationdate>20190523</creationdate><title>FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS</title><author>Ajay, Krishnan ; Muralidhar, Vaidya Surendra ; Raja, Vngaranahalli Srinivasan</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2019153578A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2019</creationdate><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Ajay, Krishnan</creatorcontrib><creatorcontrib>Muralidhar, Vaidya Surendra</creatorcontrib><creatorcontrib>Raja, Vngaranahalli Srinivasan</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Ajay, Krishnan</au><au>Muralidhar, Vaidya Surendra</au><au>Raja, Vngaranahalli Srinivasan</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS</title><date>2019-05-23</date><risdate>2019</risdate><abstract>Four-step thermal aging method for improving environmentally assisted cracking resistance of 7xxx series aluminium alloys. The thermal aging is carried out by treating the alloys at a temperature of 120 to 130 oC for 0.3 to 0.5 h, water quenching the alloys to a temperature of 25 to 27 oC and further treating the alloys at a temperature of 80 to 95 oC for 100 to 120 h and at a temperature of 120 to 130 oC for 20 to 24 h and at a temperature of 155 to 160 oC for 1 to 5 h and air cooling the alloys to room temperature, sequentially.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2019153578A1
source esp@cenet
subjects CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title FOUR-STEP THERMAL AGING METHOD FOR IMPROVING ENVIRONMENTALLY ASSISTED CRACKING RESISTANCE OF 7XXX SERIES ALUMINIUM ALLOYS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T04%3A18%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Ajay,%20Krishnan&rft.date=2019-05-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2019153578A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true