METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET

A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body at a temperature of 1,000° C. or higher and 1,100° C. or lower, and then performing (a) temperature dropping to 500° C. at 10° C./min or less,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUNIYOSHI, Futoshi, ISHII, Rintaro, SATOH, Teppei
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUNIYOSHI, Futoshi
ISHII, Rintaro
SATOH, Teppei
description A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body at a temperature of 1,000° C. or higher and 1,100° C. or lower, and then performing (a) temperature dropping to 500° C. at 10° C./min or less, or (b) temperature dropping to 500° C. at 10° C./min or less after performing a first heat treatment of holding at a first heat treatment temperature of 800° C. or higher and 950° C. or lower, the R-T-B based sintered magnet material satisfying compositional requirements; and 2) a heat treatment step of performing a second heat treatment by heating the R-T-B based sintered magnet material to a second heat treatment temperature of 650° C. or higher and 750° C. or lower, and then cooling the R-T-B based sintered magnet material to 400° C. at 5° C./min or more.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_US2018130580A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>US2018130580A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_US2018130580A13</originalsourceid><addsrcrecordid>eNrjZDDxdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCNIN0XVScHIMdnVRCPb0C3ENAjJ8Hd39XEN4GFjTEnOKU3mhNDeDsptriLOHbmpBfnxqcUFicmpeakl8aLCRgaGFobGBqYWBo6ExcaoAQwQn_g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET</title><source>esp@cenet</source><creator>KUNIYOSHI, Futoshi ; ISHII, Rintaro ; SATOH, Teppei</creator><creatorcontrib>KUNIYOSHI, Futoshi ; ISHII, Rintaro ; SATOH, Teppei</creatorcontrib><description>A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body at a temperature of 1,000° C. or higher and 1,100° C. or lower, and then performing (a) temperature dropping to 500° C. at 10° C./min or less, or (b) temperature dropping to 500° C. at 10° C./min or less after performing a first heat treatment of holding at a first heat treatment temperature of 800° C. or higher and 950° C. or lower, the R-T-B based sintered magnet material satisfying compositional requirements; and 2) a heat treatment step of performing a second heat treatment by heating the R-T-B based sintered magnet material to a second heat treatment temperature of 650° C. or higher and 750° C. or lower, and then cooling the R-T-B based sintered magnet material to 400° C. at 5° C./min or more.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CASTING ; CHEMISTRY ; ELECTRICITY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; INDUCTANCES ; MAGNETS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MAKING METALLIC POWDER ; MANUFACTURE OF ARTICLES FROM METALLIC POWDER ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; POWDER METALLURGY ; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES ; TRANSFORMERS ; TRANSPORTING ; WORKING METALLIC POWDER</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180510&amp;DB=EPODOC&amp;CC=US&amp;NR=2018130580A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180510&amp;DB=EPODOC&amp;CC=US&amp;NR=2018130580A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUNIYOSHI, Futoshi</creatorcontrib><creatorcontrib>ISHII, Rintaro</creatorcontrib><creatorcontrib>SATOH, Teppei</creatorcontrib><title>METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET</title><description>A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body at a temperature of 1,000° C. or higher and 1,100° C. or lower, and then performing (a) temperature dropping to 500° C. at 10° C./min or less, or (b) temperature dropping to 500° C. at 10° C./min or less after performing a first heat treatment of holding at a first heat treatment temperature of 800° C. or higher and 950° C. or lower, the R-T-B based sintered magnet material satisfying compositional requirements; and 2) a heat treatment step of performing a second heat treatment by heating the R-T-B based sintered magnet material to a second heat treatment temperature of 650° C. or higher and 750° C. or lower, and then cooling the R-T-B based sintered magnet material to 400° C. at 5° C./min or more.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CASTING</subject><subject>CHEMISTRY</subject><subject>ELECTRICITY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>INDUCTANCES</subject><subject>MAGNETS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MAKING METALLIC POWDER</subject><subject>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</subject><subject>TRANSFORMERS</subject><subject>TRANSPORTING</subject><subject>WORKING METALLIC POWDER</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDDxdQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXCNIN0XVScHIMdnVRCPb0C3ENAjJ8Hd39XEN4GFjTEnOKU3mhNDeDsptriLOHbmpBfnxqcUFicmpeakl8aLCRgaGFobGBqYWBo6ExcaoAQwQn_g</recordid><startdate>20180510</startdate><enddate>20180510</enddate><creator>KUNIYOSHI, Futoshi</creator><creator>ISHII, Rintaro</creator><creator>SATOH, Teppei</creator><scope>EVB</scope></search><sort><creationdate>20180510</creationdate><title>METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET</title><author>KUNIYOSHI, Futoshi ; ISHII, Rintaro ; SATOH, Teppei</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_US2018130580A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2018</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CASTING</topic><topic>CHEMISTRY</topic><topic>ELECTRICITY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>INDUCTANCES</topic><topic>MAGNETS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MAKING METALLIC POWDER</topic><topic>MANUFACTURE OF ARTICLES FROM METALLIC POWDER</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES</topic><topic>TRANSFORMERS</topic><topic>TRANSPORTING</topic><topic>WORKING METALLIC POWDER</topic><toplevel>online_resources</toplevel><creatorcontrib>KUNIYOSHI, Futoshi</creatorcontrib><creatorcontrib>ISHII, Rintaro</creatorcontrib><creatorcontrib>SATOH, Teppei</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUNIYOSHI, Futoshi</au><au>ISHII, Rintaro</au><au>SATOH, Teppei</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET</title><date>2018-05-10</date><risdate>2018</risdate><abstract>A method for manufacturing an R-T-B based sintered magnet includes: 1) a step of preparing an R-T-B based sintered magnet material by sintering a molded body at a temperature of 1,000° C. or higher and 1,100° C. or lower, and then performing (a) temperature dropping to 500° C. at 10° C./min or less, or (b) temperature dropping to 500° C. at 10° C./min or less after performing a first heat treatment of holding at a first heat treatment temperature of 800° C. or higher and 950° C. or lower, the R-T-B based sintered magnet material satisfying compositional requirements; and 2) a heat treatment step of performing a second heat treatment by heating the R-T-B based sintered magnet material to a second heat treatment temperature of 650° C. or higher and 750° C. or lower, and then cooling the R-T-B based sintered magnet material to 400° C. at 5° C./min or more.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_US2018130580A1
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CASTING
CHEMISTRY
ELECTRICITY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
INDUCTANCES
MAGNETS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MAKING METALLIC POWDER
MANUFACTURE OF ARTICLES FROM METALLIC POWDER
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
POWDER METALLURGY
SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
TRANSFORMERS
TRANSPORTING
WORKING METALLIC POWDER
title METHOD FOR MANUFACTURING R-T-B BASED SINTERED MAGNET
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T16%3A59%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUNIYOSHI,%20Futoshi&rft.date=2018-05-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EUS2018130580A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true